B29K2059/00

Laser-welded body and production method therefor

A laser-welded body includes at least three of resin members, which contain a thermoplastic resin including: a first resin member which is a laser-irradiated subject, has an absorbance a.sub.1 of 0.01 to 0.12; a second resin member which has an absorbance a.sub.2 of 0.1 to 0.9 and includes a butted part where ends of one or more resin members are brought into contact with each other; and a third resin member which has an absorbance a.sub.3 of 0.2 to 3.8, and the absorbances a.sub.2, a.sub.3 exhibited by the second resin member and the third resin member are attributed to the inclusion of nigrosine as a laser beam absorbent therein, and the resin members are overlapped in the above mentioned to form contacted parts at these interfaces, at least a part of the butted part and/or the contacted parts are laser-welded.

Laser-welded body and production method therefor

A laser-welded body includes at least three of resin members, which contain a thermoplastic resin including: a first resin member which is a laser-irradiated subject, has an absorbance a.sub.1 of 0.01 to 0.12; a second resin member which has an absorbance a.sub.2 of 0.1 to 0.9 and includes a butted part where ends of one or more resin members are brought into contact with each other; and a third resin member which has an absorbance a.sub.3 of 0.2 to 3.8, and the absorbances a.sub.2, a.sub.3 exhibited by the second resin member and the third resin member are attributed to the inclusion of nigrosine as a laser beam absorbent therein, and the resin members are overlapped in the above mentioned to form contacted parts at these interfaces, at least a part of the butted part and/or the contacted parts are laser-welded.

POLYOXYMETHYLENE MICROPARTICLES AND METHODS OF PRODUCTION AND USE THEREOF
20220380557 · 2022-12-01 · ·

Methods include dissolving a polyoxymethylene (POM) homopolymer or copolymer in one or more solvents at an elevated temperature (e.g., up to a boiling point+10° C. (T.sub.BP+10C) of the one or more solvents) to form a polymer mixture, wherein a difference in total Hansen solubility parameters (Δδ.sub.t) for the POM homopolymer or copolymer and the one or more solvents is 6 or less; cooling the polymer mixture to form a POM particle composition; and isolating the POM particle composition. Said method may be performed at ambient pressures.

METHOD OF ANCHORING A CONNECTOR ELEMENT, A MACHINE FOR CARRYING OUT THE METHOD AND A CONNECTOR ELEMENT ANCHORING KIT
20230097285 · 2023-03-30 ·

A method of anchoring a connector element (10) in a receiving object (66) comprises inserting a distal end of the connector element (10) into a mounting hole in an insertion direction along an insertion axis; inserting a sleeve (36) comprising a thermoplastic material into the mounting hole, the sleeve (36) enclosing the connector element (10); and transferring energy to liquefy at least a portion of the thermoplastic material of the sleeve (36). A machine (500) configured for carrying out the method and a connector element anchoring kit comprising a connector element (10) and a sleeve (36) comprising thermoplastic material.

METHOD OF ANCHORING A CONNECTOR ELEMENT, A MACHINE FOR CARRYING OUT THE METHOD AND A CONNECTOR ELEMENT ANCHORING KIT
20230097285 · 2023-03-30 ·

A method of anchoring a connector element (10) in a receiving object (66) comprises inserting a distal end of the connector element (10) into a mounting hole in an insertion direction along an insertion axis; inserting a sleeve (36) comprising a thermoplastic material into the mounting hole, the sleeve (36) enclosing the connector element (10); and transferring energy to liquefy at least a portion of the thermoplastic material of the sleeve (36). A machine (500) configured for carrying out the method and a connector element anchoring kit comprising a connector element (10) and a sleeve (36) comprising thermoplastic material.

METHOD FOR THE PRODUCTION OF AN ELASTIC LAMINATE AND LAMINATED ELASTIC PRODUCT

A method for the production of an elastic laminate, with the following steps in a production line: coextrudeing a first web of elastic film with at least three layers, with at least two different polymer materials, to feed contemporaneously said coextruded first elastic film web and two second nonwoven webs to a thermal, binding calender, wherein the first elastic film web is arranged between said two second nonwoven webs when entering the calender; wherein said first elastic film web, during the movement from the coextrusion step to the thermal binding step, passes from a melted state, to a solidified and cold state when entering the calender, to join, through spot welding in said calender, said second nonwoven webs with respective opposite outer layers of said first elastic film web, thus producing an intermediate web, to stretch mechanically said intermediate web according to a direction transverse to the same web.

METHOD FOR THE PRODUCTION OF AN ELASTIC LAMINATE AND LAMINATED ELASTIC PRODUCT

A method for the production of an elastic laminate, with the following steps in a production line: coextrudeing a first web of elastic film with at least three layers, with at least two different polymer materials, to feed contemporaneously said coextruded first elastic film web and two second nonwoven webs to a thermal, binding calender, wherein the first elastic film web is arranged between said two second nonwoven webs when entering the calender; wherein said first elastic film web, during the movement from the coextrusion step to the thermal binding step, passes from a melted state, to a solidified and cold state when entering the calender, to join, through spot welding in said calender, said second nonwoven webs with respective opposite outer layers of said first elastic film web, thus producing an intermediate web, to stretch mechanically said intermediate web according to a direction transverse to the same web.

Method of anchoring a first object in a second object

A method for joining two objects by anchoring an insert portion provided on a first object in an opening provided on a second object. The anchorage is achieved by liquefaction of a thermoplastic material and interpenetration of the liquefied material and a penetrable material, the two materials being arranged on opposite surfaces of the insert portion and the wall of the opening. During the step of inserting the insert portion in the opening and/or during anchorage a clamping force is applied to opposing surfaces of the second object to prevent the second object from cracking or bulging.

Method of anchoring a first object in a second object

A method for joining two objects by anchoring an insert portion provided on a first object in an opening provided on a second object. The anchorage is achieved by liquefaction of a thermoplastic material and interpenetration of the liquefied material and a penetrable material, the two materials being arranged on opposite surfaces of the insert portion and the wall of the opening. During the step of inserting the insert portion in the opening and/or during anchorage a clamping force is applied to opposing surfaces of the second object to prevent the second object from cracking or bulging.

Resin composition, pellet, composite molded article, method for manufacturing composite molded article and tank

To provide a resin composition, a pellet, a composite molded article, a method for manufacturing a composite molded article and a tank, all capable of enabling tight joining and integration of the polyacetal resin molded article and the polyethylene resin molded article, and of suppressing formaldehyde emission and occurrence of mold deposit. The resin composition contains a resin ingredient and melamine, the resin ingredient containing a polyacetal resin and a maleic anhydride-modified polyethylene resin, the polyacetal resin and the maleic anhydride-modified polyethylene resin following a mass proportion of (20 to 49):(80 to 51), and molar concentration of the maleic anhydride group capable of reacting with amino group of melamine contained in the resin composition being 5 to 25 μmol/g.