Patent classifications
C01G31/00
ANODE MATERIAL FOR RECHARGEABLE LI-ION BATTERIES
Materials, designs, methods of manufacture, and devices are provided for an anode material for a rechargeable lithium-ion battery. For example, an anode material may include Li.sub.3±xV.sub.2±yO.sub.5±z. 0≤x≤7, 0≤y≤1, and z may be based on the charge resulting from Li.sub.3±x and V.sub.2±y. Also, a cell can include a lithiated anode material. The lithiated anode material may include Li3±xV2±yO5±z. The lithiated anode material may be casted on a first substrate to form a lithiated anode, having a separator stacked on the lithiated anode. The separator may include electrolytes. A cathode can be stacked on the separator. The cathode being formed by casting a cathode material on a second substrate.
Reactor for continuous production of graphene and 2D inorganic compounds
Provided is a continuous reactor system for producing graphene or an inorganic 2-D compound, the reactor comprising: (a) a first body comprising an outer wall and a second body comprising an inner wall, wherein the inner wall defines a bore and the first body is configured within the bore and a motor is configured to rotate the first and/or second body; (b) a reaction chamber between the outer wall of the first body and the inner wall of the second body; (c) a first inlet and a second inlet disposed at first end of the reactor and in fluid communication with the reaction chamber; (d) a first outlet and a second outlet disposed downstream from the first inlet, the outlets being in fluid communication with the reaction chamber; and (e) a flow return conduit having two inlets/outlets in fluid communication with two ends of the reactor.
Preparation method and application of tetragonal NaV2O5H2O nanosheet-like powder
A preparation method of a tetragonal NaV.sub.2O.sub.5.H.sub.2O nanosheet-like powder includes steps of: (Step 1) simultaneously adding NaVO.sub.3 and Na.sub.2S.9H.sub.2O into deionized water, and then magnetically stirring, and obtaining a black turbid solution; (Step 2) sealing after putting the black turbid solution into an inner lining of a reaction kettle, fixing the sealed inner lining in an outer lining of the reaction kettle, placing the reaction kettle into a homogeneous reactor, and then performing a hydrothermal reaction; and (Step 3) after completing the hydrothermal reaction, naturally cooling the reaction kettle to the room temperature, and then alternately cleaning through water and alcohol, and then collecting a product, drying the product, and finally obtaining the tetragonal NaV.sub.2O.sub.5.H.sub.2O nanosheet-like powder with a thickness in a range of 30-60 nm and a single crystal structure grown along a (002) crystal orientation.
Preparation method and application of tetragonal NaV2O5H2O nanosheet-like powder
A preparation method of a tetragonal NaV.sub.2O.sub.5.H.sub.2O nanosheet-like powder includes steps of: (Step 1) simultaneously adding NaVO.sub.3 and Na.sub.2S.9H.sub.2O into deionized water, and then magnetically stirring, and obtaining a black turbid solution; (Step 2) sealing after putting the black turbid solution into an inner lining of a reaction kettle, fixing the sealed inner lining in an outer lining of the reaction kettle, placing the reaction kettle into a homogeneous reactor, and then performing a hydrothermal reaction; and (Step 3) after completing the hydrothermal reaction, naturally cooling the reaction kettle to the room temperature, and then alternately cleaning through water and alcohol, and then collecting a product, drying the product, and finally obtaining the tetragonal NaV.sub.2O.sub.5.H.sub.2O nanosheet-like powder with a thickness in a range of 30-60 nm and a single crystal structure grown along a (002) crystal orientation.
FABRICATION OF CoVOx COMPOSITE THIN FILM ELECTRODE VIA SINGLE STEP AACVD
A CoVO.sub.x composite electrode and method of making is described. The composite electrode comprises a substrate with an average 0.5-5 m thick layer of CoVO.sub.x having pores with average diameters of 2-200 nm. The method of making the composite electrode involves contacting the substrate with an aerosol comprising a solvent, a cobalt complex, and a vanadium complex. The CoVO.sub.x composite electrode is capable of being used in an electrochemical cell for water oxidation.
REACTOR FOR CONTINUOUS PRODUCTION OF GRAPHENE AND 2D INORGANIC COMPOUNDS
Provided is a continuous reactor system for producing graphene or an inorganic 2-D compound, the reactor comprising: (a) a rust body comprising an outer wall and a second body comprising an inner wall, wherein the inner wall defines a bore and the first body is configured within the bore and a motor is configured to rotate the first and/or second body; (b) a reaction chamber between the outer wall of the first body and the inner wall of the second body; (c) a first inlet and a second inlet disposed at first end of the reactor and in fluid communication with the reaction chamber; (d) a first outlet and a second outlet disposed downstream from the first inlet, the outlets being in fluid communication with the reaction chamber; and (e) a flow return conduit having two inlets/outlets in fluid communication with two ends of the reactor.
QUANTUM MATERIAL/VANADIUM OXIDE HETEROSTRUCTURES, METHODS OF MAKING SAME, AND USES THEREOF
The subject invention pertains to the synthesis and characterization of V.sub.2O.sub.5/CdE NW/QD heterostructures. The V.sub.2O.sub.5/CdE heterostructures are versatile new materials constructs for light harvesting, charge separation, and the photocatalytic production of solar fuels; polymorphism of V.sub.2O.sub.5 and compositional alloying of both components provides for a substantial design space for tuning of interfacial energy offsets. Also provided are a new class of type-II heterostructures composed of cadmium chalcogenide QDs (CdE where E=S, Se, or Te) and -V.sub.2O.sub.5 nanowires (NWs). The synthesis and characterization of V.sub.2O.sub.5/CdE NW/QD heterostructures, prepared via successive ionic layer adsorption and reaction (SILAR) and linker-assisted assembly (LAA), the characterization of their photoinduced charge-transfer reactivity using transient absorption spectroscopy, and their performance in the photocatalytic reduction of protons to hydrogen are also disclosed.
ELECTRODE MATERIALS FOR GROUP II CATION-BASED BATTERIES
Preparation, characterization, and an electrochemical study of Mg.sub.0.1V.sub.2O.sub.5 prepared by a novel sol-gel method with no high-temperature post-processing are disclosed. Cyclic voltammetry showed the material to be quasi-reversible, with improved kinetics in an acetonitrile-, relative to a carbonate-, based electrolyte. Galvanostatic test data under a C/10 discharge showed a delivered capacity >250 mAh/g over several cycles. Based on these results, a magnesium anode battery, as disclosed, would yield an average operating voltage 3.2 Volts with an energy density 800 mWh/g for the cathode material, making the newly synthesized material a viable cathode material for secondary magnesium batteries.
ELECTRODE MATERIALS FOR GROUP II CATION-BASED BATTERIES
Preparation, characterization, and an electrochemical study of Mg.sub.0.1V.sub.2O.sub.5 prepared by a novel sol-gel method with no high-temperature post-processing are disclosed. Cyclic voltammetry showed the material to be quasi-reversible, with improved kinetics in an acetonitrile-, relative to a carbonate-, based electrolyte. Galvanostatic test data under a C/10 discharge showed a delivered capacity >250 mAh/g over several cycles. Based on these results, a magnesium anode battery, as disclosed, would yield an average operating voltage 3.2 Volts with an energy density 800 mWh/g for the cathode material, making the newly synthesized material a viable cathode material for secondary magnesium batteries.
Preparation method and application of tetragonal NaV.SUB.2.O.SUB.5.⋅H.SUB.2.O nanosheet-like powder
A preparation method of a tetragonal NaV.sub.2O.sub.5.H.sub.2O nanosheet-like powder includes steps of: (S1) simultaneously adding NaVO.sub.3 and Na.sub.2S.9H.sub.2O into deionized water, and then magnetically stirring, and obtaining a black turbid solution; (S2) sealing after putting the black turbid solution into an inner lining of a reaction kettle, fixing the sealed inner lining in an outer lining of the reaction kettle, placing the reaction kettle into a homogeneous reactor, and then performing a hydrothermal reaction; and (S3) after completing the hydrothermal reaction, naturally cooling the reaction kettle to the room temperature, and then alternately cleaning through water and alcohol, and then collecting a product, drying the product, and finally obtaining the tetragonal NaV.sub.2O.sub.5.H.sub.2O nanosheet-like powder with a thickness in a range of 30-60 nm and a single crystal structure grown along a (002) crystal orientation.