C03B27/00
Device and method for press bending glass panes
A device for bending glass panes, includes a lower press-bending mould with a frame-shaped contact surface, an upper press-bending mould arranged opposite the contact surface, wherein the lower press-bending mould and the upper press-bending mould are suitable for reshaping a glass pane situated therebetween by pressing, wherein the side edge of the glass pane rests on the contact surface along a contact line, wherein during pressing, the contact line migrates from a first contact line all the way to a pressing line, and wherein the contact surface between the first contact line and the pressing line is convexly curved.
Device and method for press bending glass panes
A device for bending glass panes, includes a lower press-bending mould with a frame-shaped contact surface, an upper press-bending mould arranged opposite the contact surface, wherein the lower press-bending mould and the upper press-bending mould are suitable for reshaping a glass pane situated therebetween by pressing, wherein the side edge of the glass pane rests on the contact surface along a contact line, wherein during pressing, the contact line migrates from a first contact line all the way to a pressing line, and wherein the contact surface between the first contact line and the pressing line is convexly curved.
BOROSILICATE GLASS ARTICLE
A glass article is composed of a glass having a demixing factor in respect of its hydrolytic resistance in a range from 0.10 to 1.65.
BOROSILICATE GLASS ARTICLE
A glass article is composed of a glass having a demixing factor in respect of its hydrolytic resistance in a range from 0.10 to 1.65.
Antimicrobial strengthened glass and preparation process thereof
An antimicrobial strengthened glass and a preparation process thereof. The antimicrobial strengthened glass made from components including 30-50 parts of silicon dioxide, 10-20 parts of epoxy resin, 10-20 parts of titanium dioxide, 5-15 parts of nano bismuth oxide, 8-12 parts of boron oxide, 4-8 parts of chlorinated polyethylene, 2-6 parts of aluminum oxide, 1-3 parts of sodium oxide, 1-3 parts of manganese dioxide, 5-15 parts of graphite powder, 1-3 parts of barium sulfate, 2-4 parts of calcium hexaluminate, 1-3 parts of sodium fluorosilicate, 2-4 parts of borax decahydrate, 3-5 parts of sodium oxalate, 1-2 parts of sodium phosphate, 1-3 parts of sodium carbonate, 1-3 parts of potassium persulfate, 1-2 parts of potassium carbonate, 1-5 parts of ethylenediamine tetraacetic acid disodium, 1-5 parts of acrylamide, 0.01-1 part of silver nitrate and 0.01-1 parts of zinc sulfate.
Tempered glass substrate having reduced iridescence
A process for the manufacture of a heat strengthened glass substrate, includes the application of a temporary layer including a polymer on a glass substrate including a glass sheet, then the application to the glass substrate coated with the temporary layer of a treatment for the heat strengthening of the glass including heating, leading to the removal of the temporary layer, and then cooling by blowing of air through nozzles. The glass substrate thus obtained exhibits a reduced level of iridescences.
Tempered glass substrate having reduced iridescence
A process for the manufacture of a heat strengthened glass substrate, includes the application of a temporary layer including a polymer on a glass substrate including a glass sheet, then the application to the glass substrate coated with the temporary layer of a treatment for the heat strengthening of the glass including heating, leading to the removal of the temporary layer, and then cooling by blowing of air through nozzles. The glass substrate thus obtained exhibits a reduced level of iridescences.
Glass processing system with variable bending station
A glass processing may include a heating station to heat glass sheets, and a bending station disposed downstream of the heating station to bend the heated glass sheets. The bending station may include first and second independent movement mechanisms configured to independently move first and second molds when the glass processing system is operated in a first mode, and to cooperate to move a third mold when the glass processing system is operated in a second mode. The system further includes a control system to control the movement mechanisms so that they operate independently when the glass processing system is operated in the first mode, and so that they operate simultaneously when the glass processing system is operated in the second mode.
Glass processing system with variable bending station
A glass processing may include a heating station to heat glass sheets, and a bending station disposed downstream of the heating station to bend the heated glass sheets. The bending station may include first and second independent movement mechanisms configured to independently move first and second molds when the glass processing system is operated in a first mode, and to cooperate to move a third mold when the glass processing system is operated in a second mode. The system further includes a control system to control the movement mechanisms so that they operate independently when the glass processing system is operated in the first mode, and so that they operate simultaneously when the glass processing system is operated in the second mode.
OPTICAL DEVICE FABRICATION
Transparent conductive coatings are polished using particle slurries in combination with mechanical shearing force, such as a polishing pad. Substrates having transparent conductive coatings that are too rough and/or have too much haze, such that the substrate would not produce a suitable optical device, are polished using methods described herein. The substrate may be tempered prior to, or after, polishing. The polished substrates have low haze and sufficient smoothness to make high-quality optical devices.