Patent classifications
C06B21/00
Water-based explosive
An explosive, in particular a water-in-oil emulsion explosive, comprising a water-based explosive composition and a gas, wherein the gas is infused with two different ranges of sizes of nanobubbles, to provide controlled hotspots for detonation to improve emulsion stability and detonation sensitivity. Into the Nano Bubble tank (31) are fed the pressurised gas in water through valve (26) and also a sample is fed into the Nano Bubble tank (31). This then provides the NanoBubble Input NBIbp1 to be fed by NB Feed Pump (33) into static mixer (51). Also fed to the Static Mixer (51) by matrix pump (41) is the explosives containing PIBSA (Poly-Iso-Butylene Succinic Anhydride) in emulsion form as Emulsion Input EInp1 from Emulsion Matrix truck. The static mixer allows for the gas to be infused into the water-based explosive composition in at least a substantial part in the form of nanobubbles (NB) which then forms a controlled explosive output for use in the blast hole (61) by the bubbles acting as a sensitiser as so called “hot spots” which transfer the energy throughout the explosive charge once initiated. This allows the thermal “hot spot” detonation wave to travel through and carries the explosive to a full and controlled detonation.
ENERGETIC MATERIALS
The invention is directed to a radiation curable energetic composition, to a method of forming a three-dimensional energetic object, to a three-dimensional energetic object, and to uses of the radiation curable energetic composition.
The radiation curable energetic composition of the invention comprises
(a) one or more polymerisable components,
(b) one or more polymerisation initiators, and
(c) one or more energetic components.
Sorbent and devices for capturing, stabilizing and recovering volatile and semi-volatile compounds
The present invention provides an improved sorbent and corresponding device(s) and uses thereof for the capture and stabilization of volatile organic compounds (VOC) or semi-volatile organic compounds (SVOC) from a gaseous atmosphere. The sorbent is capable of rapid and high uptake of one or more compounds and provides quantitative release (recovery) of the compound(s) when exposed to elevated temperature and/or organic solvent. Uses of particular improved grades of mesoporous silica are disclosed.
System and method for uniformly manufacturing a rocket fuel grain horizontally in a single section
A system and method for producing fuel grain for a rocket engine horizontally with an additive manufacturing machine is disclosed. To begin, a fuel grain model is received. The fuel grain model is oriented in a direction of a central core axis and divided into two-dimensional layers with defined footprint areas. In accordance with the fuel grain model, a first layer is printed by applying successive fuel beads in a direction primarily parallel to the central core axis.
Coating method for energetic material and coating system for coating energetic material using said type of coating method
The invention relates to a coating method for energetic material (12), in particular in a vacuum. The energetic material (12) is coated by chemical or physical vapor deposition. The coating material (16) is electrically conductive and/or hydrophobic or hydrophilic. The energetic material (12) is shaped as grains and/or pellets and/or is in the form of a powder.
Explosives Based on Hydrogen Peroxide With Improved Sleep Time
The present invention provides an explosive composition comprising hydrogen peroxide, fuel and one or more density stabilisers. The present invention also provides methods for preparing the compositions and method of using the compositions.
Synthesis of High Explosive Nanoparticles by Turbulent Mixing
A method of making RDX nanoparticles comprises dissolving RDX in acetone; injecting the RDX/acetone through an inner tube of a turbulent mixer to form an inner flow; injecting an anti-solvent through an outer tube of a turbulent mixer to form an outer flow, wherein the inner tube is concentric with the outer tube, wherein turbulent mixing of the inner flow and outer flow precipitates nanoparticle of RDX. The concentration of RDX in acetone may be 0.5-1.0 mg RDX/mL acetone. The anti-solvent is a mixture of hexane and cyclohexanone.
Method and device for drying an explosive
A method and a device for drying an explosive, wherein the explosive contains moisture and microwave radiation causes the explosive to expel the moisture contained in the explosive. Provided is a drying chamber having magnetrons that exert the required microwave radiation on the explosive to be dried and thereby heat the explosive. During heating, the moisture in the explosive is then expelled.
Energetic feedstock for additive manufacturing
The present invention comprises formulations and method for additive manufacturing comprising: a pot-stable photo-curable polymer; one or more fillers; and one or more additives, wherein the formulation cures into a polymer in six hours or less upon exposure to light. In certain examples, the additive manufacturing is a moldless method of additive manufacturing by preparing a formulation comprising: a pot-stable photo-curable polymer, one or more fillers, and one or more additives, and exposing the formulation to light in an amount that substantially cures the polymer in 6 hours or less.
PBX COMPOSITION
The invention relates to a cast explosive composition. There is provided a precure castable explosive composition comprising an explosive material, a polymerisable binder, said cross linking reagent comprising at least two reactive groups each of which is protected by a labile blocking group.
##STR00001##