Patent classifications
C08F234/00
Black particles, black coating material, coating film, and black matrix for color filters
The present invention provides black particles that have high electrical insulation and that can achieve high blackness in the visible light region, as well as a black coating material, a coating film, and a black matrix for a color filter each containing the black particles. Provided are black particles containing a copolymer including a structural unit derived from a pyrrole compound and a structural unit derived from a quinone compound, the black particles having an aqueous dispersion number average particle size of 100 nm or less and a zeta potential of 5 mV or less.
MALEIMIDE COPOLYMER, METHOD FOR PRODUCING SAME, RESIN COMPOSITION AND INJECTION MOLDED BODY
A maleimide based copolymer, manufacturing method thereof, and a resin composition using the maleimide based copolymer is provided. The maleimide based copolymer includes 40 to 60 mass % of aromatic vinyl monomer unit, 5 to 20 mass % of vinyl cyanide monomer unit, 35 to 50 mass % of maleimide monomer unit, and 0 to 10 mass % of monomer copolymerizable with these monomer units. The maleimide based copolymer has a glass transition temperature of 165 C. or higher and a melt mass flow rate of 25 to 80 g/10 min measured at 265 C. with 98N load. By using such maleimide based copolymer, flowability can be improved without decreasing heat resistance providing ability.
MALEIMIDE COPOLYMER, METHOD FOR PRODUCING SAME, RESIN COMPOSITION AND INJECTION MOLDED BODY
A maleimide based copolymer, manufacturing method thereof, and a resin composition using the maleimide based copolymer is provided. The maleimide based copolymer includes 40 to 60 mass % of aromatic vinyl monomer unit, 5 to 20 mass % of vinyl cyanide monomer unit, 35 to 50 mass % of maleimide monomer unit, and 0 to 10 mass % of monomer copolymerizable with these monomer units. The maleimide based copolymer has a glass transition temperature of 165 C. or higher and a melt mass flow rate of 25 to 80 g/10 min measured at 265 C. with 98N load. By using such maleimide based copolymer, flowability can be improved without decreasing heat resistance providing ability.