C08G2350/00

Vibration damping material and method of producing vibration damping material

An aspect of the present invention is directed to a vibration damping material for use in a mount part for supporting a motor, the vibration damping material including: a gel of a dehydration condensation reaction product of silicone oil and boric acid, wherein the boric acid is in an amount of 25 to 75 moles based on 100 moles of the total amount of the silicone oil and the boric acid.

Viscoelastic Polyurethane Foam with Coating

A coated viscoelastic polyurethane foam includes a viscoelastic polyurethane foam having the coating thereon, the viscoelastic polyurethane foam having a resiliency of less than or equal to 20% as measured according to ASTM D3574, and a coating material on and embedded within the viscoelastic polyurethane foam, the coating material including an aqueous polymer emulsion and an encapsulated phase change material.

PRODUCTION OF POLYURETHANE FOAM

Composition for producing polyurethane foam, in particular rigid polyurethane foam, comprising at least an isocyanate component, a polyol component, optionally a catalyst that catalyses the formation of a urethane or isocyanate linkage, blowing agents, wherein the composition comprises polyester-polysiloxane block copolymers.

SUPER-VIBRATION DAMPING THERMOPLASTIC ELASTOMER BLENDS AND LOWER SPECIFIC GRAVITY ARTICLES MADE THEREWITH
20190375931 · 2019-12-12 · ·

A thermoplastic elastomer compound includes hydrogenated styrenic block copolymer having a polyisoprene soft block, styrene-isobutylene-styrene block copolymer, tackifier having a softening point of at least about 80 C according to ASTM 6493, and, optionally, one or more additional thermoplastic elastomers. The compound has a Compound Tan Delta Peak Temperature (at 10 Hz) of at least 10 C and a Compound Tan Delta Peak Height (at 10 Hz) of at least 0.85 if no thermoplastic polyurethane is present and at least 0.60 if additional thermoplastic elastomer is present and includes thermoplastic polyurethane. The thermoplastic elastomer compound exhibits superior damping properties across a broad range of temperatures, including at or above room temperature, and across a broad range of vibrational frequencies. The compound in sheet form can be used as a layer in an article of a structure susceptible to forceful impact of any item. Specific gravity can be lowered by use of a foaming agent or a blowing agent with increasing capability of absorbing G-force shock.

Hybrid systems consisting of foamed thermoplastic elastomers and polyurethanes
10501596 · 2019-12-10 · ·

The present invention relates to a hybrid material comprising a matrix of polyurethane and foamed particles of thermoplastic polyurethane comprised therein and also a process for producing such hybrid materials and the use of these hybrid materials as bicycle saddles, upholstery and shoe soles.

Low delamination mold release

Methods and combinations of a curing catalyst with a mold release mixture, which is then subsequently applied to the surface of a mold prior to the application of polyurethane reactants to said mold, where the curing catalyst component has the effect of catalyzing the reaction at the surface of the molded part. This catalysis results in greater reactivity at the surface between reacting portions and lower delamination of the surface of the foam, thereby leading to more attractive skins with a more consistent cell structure, and lower de-mold times due to skins whose nature makes them less likely to adhere to the surface of the mold. These foams will be less likely to tear upon opening of the mold, and production quality and output will be improved.

EXPANDED THERMOPLASTIC POLYURETHANE BEADS, PRODUCTION THEREOF AND PRODUCTION OF A MOLDED PART

Disclosed herein are expanded thermoplastic polyurethane beads polymerized from an isocyanate, an isocyanate-reactive compound having a molecular weight between 500 and 10 000 g/mol and a chain extender, wherein customary adjuvants may be additionally present, and the thermoplastic polyurethane has a hard phase fraction ranging from 0.1 to 0.95 and the hard phase fraction is defined by:

[00001] Hard .Math. .Math. phase .Math. .Math. fraction = .Math. x = 1 k .Math. ( ( m KVx M KV x ) .Math. M Iso + m KVx ) m ges

where M.sub.KVx represents a molar mass of chain extender x in g/mol, m.sub.KVx represents a mass of chain extender x in g, M.sub.Ixo represents a molar mass of isocyanate in g/mol, m.sub.ges represents a total mass of all starting materials without adjuvants, and k represents a number of chain extenders. Also disclosed herein are processes for producing expanded thermoplastic polyurethanes and processes for producing molded parts therefrom.

FLEXIBLE POLYURETHANE AND POLYURETHANE/POLYORGANOSILOXANE FOAM MATERIALS THAT ABSORB IMPACT ENERGY
20190345330 · 2019-11-14 ·

A polyurethane foam, a polyurethane/polyorganosiloxane foam, and a polyurethane foam polyurethane/polyorganosiloxane foam material are disclosed and described herein. The materials are formed in the presence of a polymerization reaction initiator (an isoprenoid compound), and a polymerization reaction accelerator. The polyurethane foam is formed from an isocyanate and a polyol. The polyurethane foam polyurethane/polyorganosiloxane foam material comprises the polyurethane foam which is cross-linked to the polyurethane backbone to a polyurethane/polyorganosiloxane foam. Optional gelling agents, emulsification control agents, reinforcement fillers, cross-linkers, reinforcement polymers, rubber reinforcers, silk proteins, emollients, stabilizers and colorants are also described. The polyurethane and polyurethane-polyorganosiloxane foam materials exhibit a high degree of flexibility, resilience and excellent impact absorption.

Polyol-epoxide polymers for NVH damping applications

Noise, vibration, or harshness (NVH) properties of an industrial or consumer product are reduced by incorporating therein an effective amount of a polyether- or polyester-epoxide polymer (PEEP) composition. The PEEP compositions are one-component or two-component reaction products of a polyepoxide compound and a polyol composition. The PEEP compositions have a glass-transition temperature within the range of ?50? C. to 50? C. and a loss factor of at least 0.5 by ASTM D5992 over a temperature range of at least 15 Celsius degrees at one or more frequencies within the range of 0.1 to 10,000 Hz. The PEEP compositions provide NVH damping over a broad temperature range, have improved flexibility compared with conventional epoxy technologies, avoid amine and isocyanate reactants, and can be tailored to meet target specifications.

Sustainable resilient plank

An exemplary embodiment of the present disclosure provides a polyurethane core for use in a floor or wall panel, the core comprising a polyol made, at least in part, from one or more recycled materials, and an isocyanate.