C08H3/00
Polymerized Oils & Methods of Manufacturing the Same
Described herein is a polymerized biorenewable, petroleum based, previously modified, or functionalized oil, comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.0 to about 5.0, and sulfur content ranging from 0.001 wt % to about 8 wt %. Methods of manufacturing the polymerized oil as well as its incorporation into asphalt paving, roofing, and coating applications are also described.
Polymerized Oils & Methods of Manufacturing the Same
Described herein is a polymerized biorenewable, petroleum based, previously modified, or functionalized oil, comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.0 to about 5.0, and sulfur content ranging from 0.001 wt % to about 8 wt %. Methods of manufacturing the polymerized oil as well as its incorporation into asphalt paving, roofing, and coating applications are also described.
Rejuvenating Compositions for Asphalt Applications & Methods of Manufacturing the Same
Disclosed herein are rejuvenating compositions for asphalt applications. In one aspect, the rejuvenating composition comprises a polymerized oil having a polymeric distribution ranging from about 2 to about 80 wt % oligomer content and Hildebrand solubility ranging from about 6 to about 12. In another aspect, the rejuvenating composition comprises an oil having a Hildebrand solubility ranging from about 6 to about 12 and a flash point ranging from about 100 C. to about 400 C. In yet another aspect, the rejuvenating composition comprises a modified oil having a Hildebrand solubility ranging from about 6 to about 12 and a flash point ranging from about 100 C. to about 400 C.
Rejuvenating Compositions for Asphalt Applications & Methods of Manufacturing the Same
Disclosed herein are rejuvenating compositions for asphalt applications. In one aspect, the rejuvenating composition comprises a polymerized oil having a polymeric distribution ranging from about 2 to about 80 wt % oligomer content and Hildebrand solubility ranging from about 6 to about 12. In another aspect, the rejuvenating composition comprises an oil having a Hildebrand solubility ranging from about 6 to about 12 and a flash point ranging from about 100 C. to about 400 C. In yet another aspect, the rejuvenating composition comprises a modified oil having a Hildebrand solubility ranging from about 6 to about 12 and a flash point ranging from about 100 C. to about 400 C.
POLYMERIZED OILS & METHODS OF MANUFACTURING THE SAME
Described herein is a polymerized biorenewable, previously modified, or functionalized oil, comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.30 to about 2.20, and sulfur content ranging from 0.001 wt % to about 8 wt %. Methods of manufacturing the polymerized oil as well as its incorporation into asphalt paving, roofmg, and coating applications are also described.
POLYMERIZED OILS & METHODS OF MANUFACTURING THE SAME
Described herein is a polymerized biorenewable, previously modified, or functionalized oil, comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.30 to about 2.20, and sulfur content ranging from 0.001 wt % to about 8 wt %. Methods of manufacturing the polymerized oil as well as its incorporation into asphalt paving, roofmg, and coating applications are also described.
EMULSIONS WITH POLYMERIZED OILS & METHODS OF MANUFACTURING THE SAME
Described herein is an emulsion for use in asphalt rejuvenation applications, comprising an oil phase comprising (1) a polymerized oil comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.0 to about 5.0, and sulfur content less than about 8 wt %; and (2) an aqueous phase, comprising a surfactant. The emulsion may be incorporated into asphalt paving, roofing, and coating applications and especially aged or recycled asphalt thereby obtaining rejuvenated asphalt.
EMULSIONS WITH POLYMERIZED OILS & METHODS OF MANUFACTURING THE SAME
Described herein is an emulsion for use in asphalt rejuvenation applications, comprising an oil phase comprising (1) a polymerized oil comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.0 to about 5.0, and sulfur content less than about 8 wt %; and (2) an aqueous phase, comprising a surfactant. The emulsion may be incorporated into asphalt paving, roofing, and coating applications and especially aged or recycled asphalt thereby obtaining rejuvenated asphalt.
POLYMERIZED OILS & METHODS OF MANUFACTURING THE SAME
Described herein is a polymerized biorenewable, petroleum based, previously modified, or functionalized oil, comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.0 to about 5.0, and sulfur content ranging from 0.001 wt % to about 8 wt %. Methods of manufacturing the polymerized oil as well as its incorporation into asphalt paving, roofing, and coating applications are also described.
POLYMERIZED OILS & METHODS OF MANUFACTURING THE SAME
Described herein is a polymerized biorenewable, petroleum based, previously modified, or functionalized oil, comprising a polymeric distribution having about 2 to about 80 wt % oligomer content, a polydispersity index ranging from about 1.0 to about 5.0, and sulfur content ranging from 0.001 wt % to about 8 wt %. Methods of manufacturing the polymerized oil as well as its incorporation into asphalt paving, roofing, and coating applications are also described.