C09D191/00

Coating composition and method for the protection of complex metal structures and components used in submerged environments
10577508 · 2020-03-03 · ·

A coating composition for application to a subsea component or structure includes a cellulose acetate, a plasticizer, a vegetable oil, and an ethylene-based polymer stabilizer that are mixed together. The plasticizer is epoxidized linseed oil. The vegetable oil is selected from the group including vegetable oil and soybean oil. The ethylene-based polymer stabilizer has a pigment carried therein. The ethylene-based polymer stabilizer is low-density polyethylene. The pigment is titanium dioxide and carbon black.

Coating composition and method for the protection of complex metal structures and components used in submerged environments
10577508 · 2020-03-03 · ·

A coating composition for application to a subsea component or structure includes a cellulose acetate, a plasticizer, a vegetable oil, and an ethylene-based polymer stabilizer that are mixed together. The plasticizer is epoxidized linseed oil. The vegetable oil is selected from the group including vegetable oil and soybean oil. The ethylene-based polymer stabilizer has a pigment carried therein. The ethylene-based polymer stabilizer is low-density polyethylene. The pigment is titanium dioxide and carbon black.

Coating composition and method for the protection of complex metal structures and components used in submerged environments
10577508 · 2020-03-03 · ·

A coating composition for application to a subsea component or structure includes a cellulose acetate, a plasticizer, a vegetable oil, and an ethylene-based polymer stabilizer that are mixed together. The plasticizer is epoxidized linseed oil. The vegetable oil is selected from the group including vegetable oil and soybean oil. The ethylene-based polymer stabilizer has a pigment carried therein. The ethylene-based polymer stabilizer is low-density polyethylene. The pigment is titanium dioxide and carbon black.

METHOD FOR PRODUCING ANTI-FOULING COATING FILM, AND ANTI-FOULING COATING FILM

A method for producing an anti-fouling coating film includes: a step (1) of applying a fine uneven layer forming agent containing at least one type of polysilazane as at least one type of silica raw material on at least one surface of a base substrate, the aforementioned at least one surface comprising at least one type of resin, to form a fine uneven layer containing silica and polysilazane; a step (2) of applying a modification layer forming agent containing a reactive organic compound and polysiloxane or perfluoropolyether on a surface of the fine uneven layer obtained in the step (1), to form a modification layer containing polysiloxane or perfluoropolyether, and a step (3) of applying lubricating oil containing silicone oil or fluorinated oil on a surface of the modification layer obtained in the step (2), to form a lubricating oil layer.

METHOD FOR PRODUCING ANTI-FOULING COATING FILM, AND ANTI-FOULING COATING FILM

A method for producing an anti-fouling coating film includes: a step (1) of applying a fine uneven layer forming agent containing at least one type of polysilazane as at least one type of silica raw material on at least one surface of a base substrate, the aforementioned at least one surface comprising at least one type of resin, to form a fine uneven layer containing silica and polysilazane; a step (2) of applying a modification layer forming agent containing a reactive organic compound and polysiloxane or perfluoropolyether on a surface of the fine uneven layer obtained in the step (1), to form a modification layer containing polysiloxane or perfluoropolyether, and a step (3) of applying lubricating oil containing silicone oil or fluorinated oil on a surface of the modification layer obtained in the step (2), to form a lubricating oil layer.

FURNITURE ROTARY SYSTEM HAVING REDUCED FRICTION, AND A PIECE OF FURNITURE COMPRISING SUCH SYSTEM
20200003258 · 2020-01-02 · ·

A furniture rotary system (100, 200, 300, 400, 500) for a piece of furniture (10, 20, 30, 40, 50) is provided. The furniture rotary system is forming a sliding rotary connection between a rotational member (120, 210, 320, 410, 520) and a stationary member (110, 220, 310, 420, 510), wherein said furniture rotary system (100, 200, 300, 400, 500) comprises at least one sliding surface (114, 214, 314, 414, 514) being coated with a lacquer comprising a resin, wherein said lacquer in turn is at least partly coated with a lipophilic composition coating to provide a slide layer with a lowered friction.

BIOBASED CARRIER COATINGS

The present invention describes tunable methods of treating cellulosic materials with a barrier coating comprising a prolamine and at least one polyol fatty acid ester that provides increased oil and/or grease resistance to such materials without sacrificing the biodegradability thereof. The methods as disclosed provide for adhering of the barrier coating on articles including articles comprising cellulosic materials and articles made by such methods. The materials thus treated display higher lipophobicity and may be used in any application where such features are desired.

BIOBASED CARRIER COATINGS

The present invention describes tunable methods of treating cellulosic materials with a barrier coating comprising a prolamine and at least one polyol fatty acid ester that provides increased oil and/or grease resistance to such materials without sacrificing the biodegradability thereof. The methods as disclosed provide for adhering of the barrier coating on articles including articles comprising cellulosic materials and articles made by such methods. The materials thus treated display higher lipophobicity and may be used in any application where such features are desired.

Furniture rotary system having reduced friction, and a piece of furniture comprising such system
11933358 · 2024-03-19 · ·

A furniture rotary system (100, 200, 300, 400, 500) for a piece of furniture (10, 20, 30, 40, 50) is provided. The furniture rotary system is forming a sliding rotary connection between a rotational member (120, 210, 320, 410, 520) and a stationary member (110, 220, 310, 420, 510), wherein said furniture rotary system (100, 200, 300, 400, 500) comprises at least one sliding surface (114, 214, 314, 414, 514) being coated with a lacquer comprising a resin, wherein said lacquer in turn is at least partly coated with a lipophilic composition coating to provide a slide layer with a lowered friction.

Bio-based additive for asphalt
11926760 · 2024-03-12 · ·

Compositions comprising asphalt and corn oil are provided, as are the shingles made using the compositions, methods for making the compositions, and methods for making the shingles. The compositions comprise mixtures of asphalt and corn oil, and the mixtures are oxidized to attain desirable properties.