C09J121/00

WASHER FOR SECONDARY BATTERY, SECONDARY BATTERY INCLUDING SAME, AND METHOD FOR MANUFACTURING WASHER FOR SECONDARY BATTERY

The present invention relates to a washer for a secondary battery including a film layer and an adhesive layer disposed on at least one surface of the film layer, wherein the adhesive layer includes an adhesive component and an indicator component, and the indicator component is fat-soluble, a secondary battery including the same, and a method for manufacturing the washer.

FOAM SHEET
20210070011 · 2021-03-11 ·

Provided is a foam sheet that can raise an electrostatic capacitance at the time of compression, and hence can improve sensitivity when used for an electrostatic capacitance sensor. The foam sheet includes: a foam layer; and a pressure-sensitive adhesive layer arranged on at least one side of the foam layer, wherein the foam sheet has a dielectric constant increase amount Q-P at 10% compression of 0.2 (F/m) or more, where P (F/m) represents a dielectric constant of the foam sheet immediately after the foam sheet has been left at rest under conditions of a temperature of 23 C. and a humidity of 50% for 2 hours, and Q (F/m) represents a dielectric constant of the foam sheet at a time when the foam sheet is compressed by 10% immediately after being left at rest under the conditions of a temperature of 23 C. and a humidity of 50% for 2 hours.

METHOD FOR MANUFACTURING DISSOLVABLE SLIP AND DISSOLVABLE SLIP MANUFACTURED BY SAME
20210025251 · 2021-01-28 ·

Disclosed are a method for manufacturing a dissolvable slip and a dissolvable slip manufactured by same. The manufacturing method sequentially comprises the following steps: (1) mixing an adhesive with solid particles and dissolvable particles; (2) coating the mixture prepared in step (1) on the surface of a slip body; and (3) curing the mixture coated in step (2). The dissolvable slip manufactured according to the manufacturing method not only has a stronger anchoring force with a wellbore inner wall, but also can adjust the dissolution rate of the slip after the completion of fracturing to enable the slip to degrade within a preset time. Further, the dissolvable slip has a better abrasion resistance, is suitable for various temperature conditions, and can still work normally in a concentrated acid or a concentrated alkali environment.

METHOD FOR MANUFACTURING DISSOLVABLE SLIP AND DISSOLVABLE SLIP MANUFACTURED BY SAME
20210025251 · 2021-01-28 ·

Disclosed are a method for manufacturing a dissolvable slip and a dissolvable slip manufactured by same. The manufacturing method sequentially comprises the following steps: (1) mixing an adhesive with solid particles and dissolvable particles; (2) coating the mixture prepared in step (1) on the surface of a slip body; and (3) curing the mixture coated in step (2). The dissolvable slip manufactured according to the manufacturing method not only has a stronger anchoring force with a wellbore inner wall, but also can adjust the dissolution rate of the slip after the completion of fracturing to enable the slip to degrade within a preset time. Further, the dissolvable slip has a better abrasion resistance, is suitable for various temperature conditions, and can still work normally in a concentrated acid or a concentrated alkali environment.

Label stiffener system for shelving and product displays
10902752 · 2021-01-26 · ·

Stiffening assemblies for use with labels or shelf label channels are described. The stiffening assemblies can be incorporated with one or more labels and provided so as to be conveniently used with shelf label channels or other point-of-sale displays.

Masking tape for shot peening process

Provided is a masking tape for a shot peening process, including: a substrate having a first surface and a second surface; and a pressure-sensitive adhesive layer disposed on the first surface of the substrate. The masking tape has a breaking strength of 55 N/15 mm or more and exhibits an impact absorption rate of 20% or more in a falling ball impact test. Further, the masking tape has a displacement distance of 2 mm or less after 1 h from an initial position in a holding power test at 40 C. which is performed by applying a load of 500 g.

Masking tape for shot peening process

Provided is a masking tape for a shot peening process, including: a substrate having a first surface and a second surface; and a pressure-sensitive adhesive layer disposed on the first surface of the substrate. The masking tape has a breaking strength of 55 N/15 mm or more and exhibits an impact absorption rate of 20% or more in a falling ball impact test. Further, the masking tape has a displacement distance of 2 mm or less after 1 h from an initial position in a holding power test at 40 C. which is performed by applying a load of 500 g.

FILAMENT REINFORCED TAPES USEFUL AS UNDERWATER PIPE WRAP

A member for use in undersea applications comprising a plurality of conduits assembled into a bundle; the bundle being wrapped with a pressure-sensitive tape comprising a backing, a layer of corrosion-resistant yarns on one surface of the backing, and pressure-sensitive adhesive layer that coats the corrosion-resistant yarns and binds them to the backing.

Adhesive tapes

Adhesive tapes include a plasticized polyvinyl chloride backing, a primer including an ethylene/carbon monoxide-containing terpolymer and a styrene-containing block copolymer, and an adhesive.

VIBRATION DEVICE AND ACOUSTIC DEVICE
20200368779 · 2020-11-26 · ·

A vibration device includes a piezoelectric element and an adhesive layer. The piezoelectric element includes a first principal surface and a second principal surface opposing each other. The adhesive layer is disposed on the first principal surface and is in contact with the first principal surface. A tensile strength of the adhesive layer is 10 N/cm or more and 48 N/cm or less.