C09J195/00

ADHESION PROMOTERS COMPRISING OLIGOMERIC SILANES AND METHODS OF USING THE SAME

Asphalt binders and bituminous compositions comprising oligomeric additives such as alkoxysilane oligomers compounds. In certain embodiments the oligomeric compounds may be useful as adhesion promoters for use with asphaltic bitumens and aggregates in road paving applications.

ADHESIVES FOR LOW SURFACE ENERGY MATERIALS

A roofing system includes a roofing membrane. The roofing membrane has a surface energy of 40 mN/m or less. The roofing system includes a roofing substrate. The roofing system includes an adhesive disposed between the roofing membrane and the roofing substrate. The adhesive includes a styrenic block copolymer. The styrenic block copolymer is present in an amount of 0.5 wt. % to 30 wt. % based on a total weight of the adhesive. The adhesive includes asphalt. The asphalt is present in an amount of 70 wt. % to 99.5 wt. % based on the total weight of the adhesive. A ratio of the styrenic block copolymer to the asphalt in the adhesive is 1:11 to 1:3.

ADHESIVES FOR LOW SURFACE ENERGY MATERIALS

A roofing system includes a roofing membrane. The roofing membrane has a surface energy of 40 mN/m or less. The roofing system includes a roofing substrate. The roofing system includes an adhesive disposed between the roofing membrane and the roofing substrate. The adhesive includes a styrenic block copolymer. The styrenic block copolymer is present in an amount of 0.5 wt. % to 30 wt. % based on a total weight of the adhesive. The adhesive includes asphalt. The asphalt is present in an amount of 70 wt. % to 99.5 wt. % based on the total weight of the adhesive. A ratio of the styrenic block copolymer to the asphalt in the adhesive is 1:11 to 1:3.

METHODS OF FORMING AN ADHESIVE COMPOSITION FROM ASPHALT SHINGLE WASTE POWDER

Non-limiting embodiments of the present disclosure relate to a method comprising: obtaining asphalt shingle waste (ASW) and performing grinding, screening, and separating steps on the ASW. In some embodiments, granules are removed from the ASW. In some embodiments, the method transforms ASW into ASW powder. In some embodiments, the ASW powder is formed into a plurality of briquettes. In some embodiments, at least one of: the ASW powder, the plurality of briquettes, or any combination thereof is fed into a mixing process that results in an ASW powder filled coating. In some embodiments, the ASW powder is formed into an adhesive composition.

METHODS OF FORMING AN ADHESIVE COMPOSITION FROM ASPHALT SHINGLE WASTE POWDER

Non-limiting embodiments of the present disclosure relate to a method comprising: obtaining asphalt shingle waste (ASW) and performing grinding, screening, and separating steps on the ASW. In some embodiments, granules are removed from the ASW. In some embodiments, the method transforms ASW into ASW powder. In some embodiments, the ASW powder is formed into a plurality of briquettes. In some embodiments, at least one of: the ASW powder, the plurality of briquettes, or any combination thereof is fed into a mixing process that results in an ASW powder filled coating. In some embodiments, the ASW powder is formed into an adhesive composition.

Asphalt shingle waste adhesive compositions for roofing applications and related methods

Non-limiting embodiments of the present disclosure relate to a method comprising: obtaining asphalt shingle waste (ASW) and performing grinding, screening, and separating steps on the ASW. In some embodiments, granules are removed from the ASW. In some embodiments, the method transforms ASW into ASW powder. In some embodiments, the ASW powder is formed into a plurality of briquettes. In some embodiments, at least one of: the ASW powder, the plurality of briquettes, or any combination thereof is fed into a mixing process that results in an ASW powder filled coating. In some embodiments, the ASW powder is formed into an adhesive composition.

Asphalt shingle waste adhesive compositions for roofing applications and related methods

Non-limiting embodiments of the present disclosure relate to a method comprising: obtaining asphalt shingle waste (ASW) and performing grinding, screening, and separating steps on the ASW. In some embodiments, granules are removed from the ASW. In some embodiments, the method transforms ASW into ASW powder. In some embodiments, the ASW powder is formed into a plurality of briquettes. In some embodiments, at least one of: the ASW powder, the plurality of briquettes, or any combination thereof is fed into a mixing process that results in an ASW powder filled coating. In some embodiments, the ASW powder is formed into an adhesive composition.

PROCESSES FOR FUNCTIONALIZATION AND POLYMERIZATION OF POLYAROMATIC FEEDSTOCK

Processes for chemically treating polyaromatic feedstock to form aromatic-containing oligomers or polymers are provided. The processes are characterized by treatment of a plurality of different polyaromatic hydrocarbon molecules and/or polyheterocyclic molecules present in polyaromatic feedstock with a first reagent so as to functionalize the molecules. Further treatment in a second step affords oligomeric or polymeric products which may be crosslinked. The products may be thermoplastic or thermoset materials and may find use in, for example, infrastructure applications, composites, fillers, fire retardants and 3-D printing materials.

Methods of forming an adhesive composition from asphalt shingle waste powder

Non-limiting embodiments of the present disclosure relate to a method comprising: obtaining asphalt shingle waste (ASW) and performing grinding, screening, and separating steps on the ASW. In some embodiments, granules are removed from the ASW. In some embodiments, the method transforms ASW into ASW powder. In some embodiments, the ASW powder is formed into a plurality of briquettes. In some embodiments, at least one of: the ASW powder, the plurality of briquettes, or any combination thereof is fed into a mixing process that results in an ASW powder filled coating. In some embodiments, the ASW powder is formed into an adhesive composition.

Methods of forming an adhesive composition from asphalt shingle waste powder

Non-limiting embodiments of the present disclosure relate to a method comprising: obtaining asphalt shingle waste (ASW) and performing grinding, screening, and separating steps on the ASW. In some embodiments, granules are removed from the ASW. In some embodiments, the method transforms ASW into ASW powder. In some embodiments, the ASW powder is formed into a plurality of briquettes. In some embodiments, at least one of: the ASW powder, the plurality of briquettes, or any combination thereof is fed into a mixing process that results in an ASW powder filled coating. In some embodiments, the ASW powder is formed into an adhesive composition.