Patent classifications
C22B13/00
PROCESS FOR SEPARATION OF AT LEAST ONE METAL SULFIDE FROM A MIXED SULFIDE ORE OR CONCENTRATE
A stabilization process for an arsenic solution comprising thiosulfates, the process comprising: acidifying the arsenic solution to decompose the thiosulfates, to yield an acidified solution; oxidizing the acidified solution to oxidize residual As.sup.3+ to As.sup.5+ and reduced sulfur species to sulfates, to yield a slurry comprising elemental sulfur; separating elemental sulfur from the slurry to yield a liquid; oxidizing the liquid to oxidize residual reduced sulfur species, to yield an oxidized solution; and forming a stable arsenic compound from the oxidized solution.
Stabilization process for an arsenic solution
A stabilization process for an arsenic solution comprising thiosulfates, the process comprising: acidifying the arsenic solution to decompose the thiosulfates, to yield an acidified solution; oxidizing the acidified solution to oxidize residual As.sup.3+ to As.sup.5+ and reduced sulfur species to sulfates, to yield a slurry comprising elemental sulfur; separating elemental sulfur from the slurry to yield a liquid; oxidizing the liquid to oxidize residual reduced sulfur species, to yield an oxidized solution; and forming a stable arsenic compound from the oxidized solution.
Stabilization process for an arsenic solution
A stabilization process for an arsenic solution comprising thiosulfates, the process comprising: acidifying the arsenic solution to decompose the thiosulfates, to yield an acidified solution; oxidizing the acidified solution to oxidize residual As.sup.3+ to As.sup.5+ and reduced sulfur species to sulfates, to yield a slurry comprising elemental sulfur; separating elemental sulfur from the slurry to yield a liquid; oxidizing the liquid to oxidize residual reduced sulfur species, to yield an oxidized solution; and forming a stable arsenic compound from the oxidized solution.
Treated Geothermal Brine Compositions With Reduced Concentration of Silica, Iron and Lithium
This invention relates to treated geothermal brine compositions containing reduced concentrations of lithium, iron and silica compared to the untreated brines. Exemplary compositions contain concentration of lithium ranges from 0 to 200 mg/kg, concentration of silica ranges from 0 to 30 mg/kg, concentration of iron ranges from 0 to 300 mg/kg. Exemplary compositions also contain reduced concentrations of elements like arsenic, barium, and lead.
Treated Geothermal Brine Compositions With Reduced Concentration of Silica, Iron and Lithium
This invention relates to treated geothermal brine compositions containing reduced concentrations of lithium, iron and silica compared to the untreated brines. Exemplary compositions contain concentration of lithium ranges from 0 to 200 mg/kg, concentration of silica ranges from 0 to 30 mg/kg, concentration of iron ranges from 0 to 300 mg/kg. Exemplary compositions also contain reduced concentrations of elements like arsenic, barium, and lead.
Method for the Treatment of Iron-Containing Sludge
The present invention provides a method for the treatment of sludge containing iron and between 4.5% to 12% by weight of zinc. This method includes a leaching step wherein leaching agents include hydrochloric acid and chlorate, and wherein the pH of the leachate directly resulting from this leaching step is set at a value below 1.5. A recycling method and treatment installation are also provided.
OXYGEN INJECTION IN FLUID BED ORE CONCENTRATE ROASTING
Oxygen is injected into the windbox of a fluidized bed ore roaster to form a fluidizing and oxidizing gas stream of elevated oxygen content which is fed into only the feed zone into which the ore to be fluidized is fed.
OXYGEN INJECTION IN FLUID BED ORE CONCENTRATE ROASTING
Oxygen is injected into the windbox of a fluidized bed ore roaster to form a fluidizing and oxidizing gas stream of elevated oxygen content which is fed into only the feed zone into which the ore to be fluidized is fed.
Treated geothermal brine compositions with reduced concentrations of silica, iron and lithium
This invention relates to treated geothermal brine compositions containing reduced concentrations of lithium, iron and silica compared to the untreated brines. Exemplary compositions contain concentration of lithium ranges from 0 to 200 mg/kg, concentration of silica ranges from 0 to 30 mg/kg, concentration of iron ranges from 0 to 300 mg/kg. Exemplary compositions also contain reduced concentrations of elements like arsenic, barium, and lead.
Treated geothermal brine compositions with reduced concentrations of silica, iron and lithium
This invention relates to treated geothermal brine compositions containing reduced concentrations of lithium, iron and silica compared to the untreated brines. Exemplary compositions contain concentration of lithium ranges from 0 to 200 mg/kg, concentration of silica ranges from 0 to 30 mg/kg, concentration of iron ranges from 0 to 300 mg/kg. Exemplary compositions also contain reduced concentrations of elements like arsenic, barium, and lead.