C22B9/22
Process for smelting lithium-ion batteries
The invention concerns a process for the separation of cobalt from lithium present in a charge comprising lithium-ion batteries or related products, comprising the steps of: smelting the charge using a bath furnace equipped with a submerged air-fed plasma torch for injecting plasma gas into the melt; defining and maintaining a bath redox potential where cobalt is reduced to the metallic state and reporting to an alloy phase, and whereby lithium is oxidized as Li.sub.2O and reporting to the slag phase; decanting and separating the phases. It is characterized in that the reduction and oxidizing steps are performed simultaneously. A suitably low cobalt concentration is obtained in the slag.
COMPACT COIL ASSEMBLY FOR A VACUUM ARC REMELTING SYSTEM
A vacuum arc remelting system for forming an ingot from an electrode is provided that includes a crucible assembly configured to accommodate the electrode and the ingot, an electromagnetic energy source arranged about the crucible assembly, and a lift mechanism operable to move the electromagnetic energy source along a longitudinal axis of the crucible assembly. A magnetic field generated by the electromagnetic energy source is localized to an arc region during remelting, and in one form, the electromagnetic energy source is a coil assembly having a magnetic core and a plurality of coil pairs wrapped around the core, wherein the coil assembly is operable to generate a magnetic field from the coil based on electric current flowing in the plurality of coil pairs.
Modular gun assembly for melt furnaces
An electron beam (EB) gun assembly for an EB furnace is provided. The EB gun assembly includes an EB gun-frame assembly including a skeleton frame and at least one EB gun mounted to the skeleton frame, and the EB gun-frame assembly is configured to rigidly mount onto a first EB chamber lid and melt material in a first EB chamber and be removed and rigidly mount onto a second EB chamber lid and melt material in a second EB chamber. In some forms, the EB gun assembly includes at least one mounting frame and the at least one EB gun is mounted to the at least one mounting frame and the at least one mounting frame is mounted to the skeleton frame.
High-purity titanium ingots, manufacturing method therefor, and titanium sputtering target
Provided is a high-purity titanium ingot having a purity, excluding an additive element and gas components, of 99.99 mass % or more, wherein at least one nonmetallic element selected from S, P, and B is contained in a total amount of 0.1 to 100 mass ppm as the additive component and the variation in the content of the nonmetallic element between the top, middle, and bottom portions of the ingot is within 200%. Provided is a method of manufacturing a titanium ingot containing a nonmetallic element in an amount of 0.1 to 100 mass ppm, wherein S, P, or B, which is a nonmetallic element, is added to molten titanium as an intermetallic compound or a master alloy to produce a high-purity titanium ingot having a purity, excluding an additive element and gas components, of 99.99 mass % or more. It is an object of the present invention to provide a high-purity titanium having decreased intra- and inter-ingot variations in the content of the nonmetallic element, a uniform structure, and improved strength by containing at least one nonmetallic element selected from S, P, and B.
High-purity titanium ingots, manufacturing method therefor, and titanium sputtering target
Provided is a high-purity titanium ingot having a purity, excluding an additive element and gas components, of 99.99 mass % or more, wherein at least one nonmetallic element selected from S, P, and B is contained in a total amount of 0.1 to 100 mass ppm as the additive component and the variation in the content of the nonmetallic element between the top, middle, and bottom portions of the ingot is within 200%. Provided is a method of manufacturing a titanium ingot containing a nonmetallic element in an amount of 0.1 to 100 mass ppm, wherein S, P, or B, which is a nonmetallic element, is added to molten titanium as an intermetallic compound or a master alloy to produce a high-purity titanium ingot having a purity, excluding an additive element and gas components, of 99.99 mass % or more. It is an object of the present invention to provide a high-purity titanium having decreased intra- and inter-ingot variations in the content of the nonmetallic element, a uniform structure, and improved strength by containing at least one nonmetallic element selected from S, P, and B.
Tantalum Based Alloy That Is Resistant to Aqueous Corrosion
A tantalum or tantalum alloy which contains pure or substantially pure tantalum and at least one metal element selected from the group consisting of Ru, Rh, Pd, Os, Ir, Pt, Mo, W and Re to form a tantalum alloy that is resistant to aqueous corrosion. The invention also relates to the process of preparing the tantalum alloy.
Tantalum Based Alloy That Is Resistant to Aqueous Corrosion
A tantalum or tantalum alloy which contains pure or substantially pure tantalum and at least one metal element selected from the group consisting of Ru, Rh, Pd, Os, Ir, Pt, Mo, W and Re to form a tantalum alloy that is resistant to aqueous corrosion. The invention also relates to the process of preparing the tantalum alloy.
Methods and systems for processing materials, including shape memory materials
A method for treating a material comprising: applying energy to a predetermined portion of the material in a controlled manner such that the local chemistry of the predetermined portion is altered to provide a predetermined result. When the material is a shape memory material, the predetermined result may be to provide an additional memory to the predetermined portion or to alter the pseudo-elastic properties of the shape memory material. In other examples, which are not necessarily restricted to shape memory materials, the process may be used to adjust the concentration of components at the surface to allow the formation of an oxide layer at the surface of the material to provide corrosion resistance; to remove contaminants from the material; to adjust surface texture; or to generate at least one additional phase particle in the material to provide a nucleation site for grain growth, which in turn, can strengthen the material.
Processes for producing tantalum alloys and niobium alloys
Processes for the production of tantalum alloys and niobium are disclosed. The processes use aluminothermic reactions to reduce tantalum pentoxide to tantalum metal or niobium pentoxide to niobium metal.
Continuous moldless fabrication of amorphous alloy pieces
Described herein is a method of producing an alloy. The method includes pouring a stream of molten mixture of component elements of the alloy, separating the stream into discrete pieces, solidifying the discrete pieces by cooling before the discrete pieces contact any liquid or solid. Also described herein is another method of producing an alloy. This method includes pouring and solidifying a stream of molten mixture of component elements of the alloy into a rod or pulling a rod from a molten mixture of component elements of the alloy, before the rod contacts any liquid or solid, separating the rod into discrete pieces. An apparatus suitable for carrying out the methods above can include a container from which the molten stream is poured or the solid rod extends, one or more coil, conductive plates, a laser source, or an electron beam source arranged around the molten stream or the solid rod and configured to separate the molten stream or the solid rod into discrete pieces.