C22B34/34

OPPORTUNITIES FOR RECOVERY AUGMENTATION PROCESS AS APPLIED TO MOLYBDENUM PRODUCTION
20210071283 · 2021-03-11 ·

A copper/molybdenum separation processor is provide featuring a slurry/media mixture stage configured to receive a conditioned pulp containing hydrophobic molybdenite and hydrophilic copper, iron and other minerals that is conditioned with sodium hydrosulfide together with an engineered polymeric hydrophobic media, and provide a slurry/media mixture; and a slurry/media separation stage configured to receive the slurry/media mixture, and provide a slurry product having a copper concentrate and a polymerized hydrophobic media product having a molybdenum concentrate that are separately directed for further processing. The slurry/media mixture stage include a molybdenum loading stage configured to contact the conditioned pulp with the engineered polymeric hydrophobic media in an agitated reaction chamber, and load the hydrophobic molybdenite on the engineered polymeric hydrophobic media.

Separation of copper and molybdenum sulfides from pyrite using a sea water/desalinated water hybrid process

A copper/molybdenum separation system uses sea water in the roughing circuit and desalinated water in cleaning circuit. In both roughing circuit and cleaning circuit, hydrophobic engineered media are used to recover the mineral particles of interest. The cleaning circuit includes a molybdenum loading stage configured to contact the conditioned pulp with the engineered media in an agitated reaction chamber, and load the hydrophobic molybdenite on the engineered media.

Separation of copper and molybdenum sulfides from pyrite using a sea water/desalinated water hybrid process

A copper/molybdenum separation system uses sea water in the roughing circuit and desalinated water in cleaning circuit. In both roughing circuit and cleaning circuit, hydrophobic engineered media are used to recover the mineral particles of interest. The cleaning circuit includes a molybdenum loading stage configured to contact the conditioned pulp with the engineered media in an agitated reaction chamber, and load the hydrophobic molybdenite on the engineered media.

METHOD FOR CLEAN METALLURGY OF MOLYBDENUM
20200399738 · 2020-12-24 · ·

Disclosed is a method for clean metallurgy of molybdenum, including steps: 1) roasting molybdenite with calcium to obtain calcified molybdenum calcine, and leaching the calcified molybdenum calcine with an inorganic acid to obtain a molybdenum-containing inorganic acid leachate; 2) extracting molybdenum in the leachate with a cationic extractant to obtain an organic phase loaded with molybdyl cations and a raffinate; 3) using a hydrogen peroxide solution as a stripping agent to obtain a molybdenum stripping liquor; and 4) heating the molybdenum stripping liquor to dissociate peroxymolybdic acid therein so as to form a molybdic acid precipitate, and then calcining to obtain a molybdenum trioxide product. The method solves the problem of ammonia nitrogen wastewater production and can also be used for the enrichment and recovery of rhenium.

METHOD FOR CLEAN METALLURGY OF MOLYBDENUM
20200399738 · 2020-12-24 · ·

Disclosed is a method for clean metallurgy of molybdenum, including steps: 1) roasting molybdenite with calcium to obtain calcified molybdenum calcine, and leaching the calcified molybdenum calcine with an inorganic acid to obtain a molybdenum-containing inorganic acid leachate; 2) extracting molybdenum in the leachate with a cationic extractant to obtain an organic phase loaded with molybdyl cations and a raffinate; 3) using a hydrogen peroxide solution as a stripping agent to obtain a molybdenum stripping liquor; and 4) heating the molybdenum stripping liquor to dissociate peroxymolybdic acid therein so as to form a molybdic acid precipitate, and then calcining to obtain a molybdenum trioxide product. The method solves the problem of ammonia nitrogen wastewater production and can also be used for the enrichment and recovery of rhenium.

Thermochemical processing of exothermic metallic system
10870153 · 2020-12-22 · ·

This invention relates to a method for controlling exothermic reactions between metal chlorides of Zn, V, Cr, Co, Sn, Ag, Ta, Ni, Fe, Nb Cu, Pt, W, Pd, and Mo, and Al and the use of the method for preparation of metallic alloys and compounds based on base metals Zn, V, Cr, Co, Sn, Ag, Ta, Ni, Fe, Nb Cu, Pt, W, Pd, and Mo. The method provides for a mixture of precursor chemicals including at least one solid base metal chloride to be mixed and reacted exothermically with a control powder based on Zn, V, Cr, Co, Sn, Ag, Ta, Ni, Fe, Nb Cu, Pt, W, Pd, and Mo and then reacting the resulting intermediates with an Al scavenger. Reduction is carried out in a controlled manner to regulate reaction rates and prevent excessive rise in the temperature of the reactants and the reaction products.

METHOD OF MANUFACTURING URANIUM TARGET TO BE SOLUBLE IN BASIC SOLUTION AND METHOD OF EXTRACTING RADIOACTIVE MO-99 USING THE SAME

Disclosed are a method of manufacturing a uranium target, the method including (a) a step of preparing a conjugate including a matrix and a uranium target green compact formed in the matrix; and (b) a step of performing thermo-mechanical treatment through additional heat treatment at 530 C. to 600 C. during a hot rolling pass in a process of hot-rolling the conjugate, and a method of extracting radioactive Mo-99 using the uranium target.

System and method for parallel solution extraction of one or more metal values from metal-bearing materials

A process and system is provided for recovery of one or more metal values using solution extraction techniques and for metal value recovery. In an exemplary embodiment, the solution extraction system comprises a first solution extraction circuit and a second solution extraction circuit. A first metal-bearing solution is provided to the first and second circuit, and a second metal-bearing solution is provided to the first circuit. The first circuit produces a first rich electrolyte solution, which can be forwarded to primary metal value recovery, and a low-grade raffinate, which is forwarded to secondary metal value recovery. The second circuit produces a second rich electrolyte solution, which is also forwarded to primary metal value recovery. The first and second solution extraction circuits have independent organic phases and each circuit can operate independently of the other circuit.

System and method for parallel solution extraction of one or more metal values from metal-bearing materials

A process and system is provided for recovery of one or more metal values using solution extraction techniques and for metal value recovery. In an exemplary embodiment, the solution extraction system comprises a first solution extraction circuit and a second solution extraction circuit. A first metal-bearing solution is provided to the first and second circuit, and a second metal-bearing solution is provided to the first circuit. The first circuit produces a first rich electrolyte solution, which can be forwarded to primary metal value recovery, and a low-grade raffinate, which is forwarded to secondary metal value recovery. The second circuit produces a second rich electrolyte solution, which is also forwarded to primary metal value recovery. The first and second solution extraction circuits have independent organic phases and each circuit can operate independently of the other circuit.

Opportunities for recovery augmentation process as applied to molybdenum production

A copper/molybdenum separation processor is provided featuring a slurry/media mixture stage configured to receive a conditioned pulp containing hydrophobic molybdenite and hydrophilic copper, iron and other minerals that is conditioned with sodium hydrosulfide together with an engineered polymeric hydrophobic media, and provide a slurry/media mixture; and a slurry/media separation stage configured to receive the slurry/media mixture, and provide a slurry product having a copper concentrate and a polymerized hydrophobic media product having a molybdenum concentrate that are separately directed for further processing. The slurry/media mixture stage include a molybdenum loading stage configured to contact the conditioned pulp with the engineered polymeric hydrophobic media in an agitated reaction chamber, and load the hydrophobic molybdenite on the engineered polymeric hydrophobic media.