C22C38/30
High-strength hot-dip zinc plated steel material having excellent plating properties and method for preparing same
Provided are a hot-dip zinc plated steel material and a method for preparing same, the hot-dip zinc plated steel material comprising: base iron comprising 0.01-1.6 wt % of Si and 1.2-3.1 wt % of Mn; a Zn—Al—Mg alloy plating layer; and an Al-rich layer formed on the interface of the base iron and Zn—Al—Mg alloy plating layer, wherein the rate of occupied surface area of the Al-rich layer is 70% or higher (including 100%).
Light-colored magnetic particles having improved durability and chemical resistance
The present invention can provide light-colored magnetic particles having a zirconium oxide coating layer formed on a magnetic core, and having a silver coating layer formed on the zirconium oxide coating layer, and a part of the surface of the zirconium oxide coating layer is exposed to the outside, but chemical resistance is excellent, and thus the magnetic particles hardly cause a change of magnetic characteristics so as to be suitable for security elements.
High strength precipitation hardening stainless steel alloy and article made therefrom
High strength precipitation hardening stainless steel alloy is disclosed. The steel alloy has a composition by weight %, about: 30.0% max nickel (Ni), 0.0 to 15.0% cobalt (Co), 25.0% max chromium (Cr), 5.0% max molybdenum (Mo), 5.0% max titanium (Ti), 5.0% max vanadium (V), about 0.5% max lanthanum (La) and/or cerium (Ce), and in balance iron (Fe) and inevitable impurities. The steel alloy provides a unique combination of corrosion resistance, strength and toughness and is a material for aircraft landing gears and structures.
High strength precipitation hardening stainless steel alloy and article made therefrom
High strength precipitation hardening stainless steel alloy is disclosed. The steel alloy has a composition by weight %, about: 30.0% max nickel (Ni), 0.0 to 15.0% cobalt (Co), 25.0% max chromium (Cr), 5.0% max molybdenum (Mo), 5.0% max titanium (Ti), 5.0% max vanadium (V), about 0.5% max lanthanum (La) and/or cerium (Ce), and in balance iron (Fe) and inevitable impurities. The steel alloy provides a unique combination of corrosion resistance, strength and toughness and is a material for aircraft landing gears and structures.
Steel for mold, and mold
The present invention relates to a steel for mold, containing: 0.28 mass %≤C≤0.65 mass %, 0.01 mass %≤Si≤0.30 mass %, 1.5 mass %≤Mn≤3.0 mass %, 0.5 mass %≤Cr≤1.4 mass %, 1.9 mass %≤Mo+W/2≤4.0 mass %, 0.2 mass %≤V≤1.0 mass %, and 0.01≤N≤0.10 mass %, with the balance being Fe and inevitable impurities, in which, in a state after quenching and tempering, the steel has: a (Mo, W) carbide having a diameter of 0.2 μm or less being in an amount of 1.2 mass % or more, a ratio (mass ratio) of the amount of the (Mo, W) carbide to an amount of a Cr carbide being 11 or more, and a hardness change of 15 HRC or less.
Steel for mold, and mold
The present invention relates to a steel for mold, containing: 0.28 mass %≤C≤0.65 mass %, 0.01 mass %≤Si≤0.30 mass %, 1.5 mass %≤Mn≤3.0 mass %, 0.5 mass %≤Cr≤1.4 mass %, 1.9 mass %≤Mo+W/2≤4.0 mass %, 0.2 mass %≤V≤1.0 mass %, and 0.01≤N≤0.10 mass %, with the balance being Fe and inevitable impurities, in which, in a state after quenching and tempering, the steel has: a (Mo, W) carbide having a diameter of 0.2 μm or less being in an amount of 1.2 mass % or more, a ratio (mass ratio) of the amount of the (Mo, W) carbide to an amount of a Cr carbide being 11 or more, and a hardness change of 15 HRC or less.
Grain-oriented electrical steel sheet and manufacturing method therefor
The present invention relates to a grain-oriented electrical steel sheet including 2.0 to 6.0 wt % of Si, 0.01 wt % or less (excluding 0 wt %) of C, 0.01 wt % or less (excluding 0 wt %) of N, and 0.005 to 0.1 wt % of Co, and including a balance of Fe and other inevitable impurities.
Grain-oriented electrical steel sheet and manufacturing method therefor
The present invention relates to a grain-oriented electrical steel sheet including 2.0 to 6.0 wt % of Si, 0.01 wt % or less (excluding 0 wt %) of C, 0.01 wt % or less (excluding 0 wt %) of N, and 0.005 to 0.1 wt % of Co, and including a balance of Fe and other inevitable impurities.
Fe—Al-based plated hot-stamped member and manufacturing method of Fe—Al-based plated hot-stamped member
Fe-Al-based plated hot-stamped member exhibiting excellent formed part corrosion resistance and post-coating corrosion resistance and manufacturing method. The hot-stamping member includes Fe-Al-based plated layer on one or both surfaces of a base material, the base material has a predetermined steel component, Fe-Al-based plated layer has a thickness of 10 μm or more and 60 μm or less, formed by A, B, C and D layers sequentially from a surface toward the base material, and each of the four layers is a Fe-Al-based intermetallic compound containing Al, Fe, Si, Mn and Cr for predetermined contents with the balance made up of impurities, the D layer further contains Kirkendall voids each of which cross-sectional area is 3 μm.sup.2-30 μm.sup.2 for 10 pieces/6000 μm.sup.2 or more and 40 pieces/6000 μm.sup.2 or less.
Fe—Al-based plated hot-stamped member and manufacturing method of Fe—Al-based plated hot-stamped member
Fe-Al-based plated hot-stamped member exhibiting excellent formed part corrosion resistance and post-coating corrosion resistance and manufacturing method. The hot-stamping member includes Fe-Al-based plated layer on one or both surfaces of a base material, the base material has a predetermined steel component, Fe-Al-based plated layer has a thickness of 10 μm or more and 60 μm or less, formed by A, B, C and D layers sequentially from a surface toward the base material, and each of the four layers is a Fe-Al-based intermetallic compound containing Al, Fe, Si, Mn and Cr for predetermined contents with the balance made up of impurities, the D layer further contains Kirkendall voids each of which cross-sectional area is 3 μm.sup.2-30 μm.sup.2 for 10 pieces/6000 μm.sup.2 or more and 40 pieces/6000 μm.sup.2 or less.