C22C38/38

Hot-rolled steel sheet having excellent durability and method for manufacturing same
11535908 · 2022-12-27 · ·

The present invention relates to steel used for a sash component and the like of a vehicle and, more specifically, to a hot-rolled steel sheet having excellent durability and a method for manufacturing same, the hot-rolled steel sheet having no cracks formed on a material and a welding heat-affected zone (HAZ) even after pipemaking and molding due to a smaller decrease in the strength of the welding heat-affected zone formed during electric resistance welding in comparison with the strength of the material (base material).

Hot-rolled steel sheet having excellent durability and method for manufacturing same
11535908 · 2022-12-27 · ·

The present invention relates to steel used for a sash component and the like of a vehicle and, more specifically, to a hot-rolled steel sheet having excellent durability and a method for manufacturing same, the hot-rolled steel sheet having no cracks formed on a material and a welding heat-affected zone (HAZ) even after pipemaking and molding due to a smaller decrease in the strength of the welding heat-affected zone formed during electric resistance welding in comparison with the strength of the material (base material).

Steel for mold, and mold
11535917 · 2022-12-27 · ·

The present invention relates to a steel for mold, containing: 0.28 mass %≤C≤0.65 mass %, 0.01 mass %≤Si≤0.30 mass %, 1.5 mass %≤Mn≤3.0 mass %, 0.5 mass %≤Cr≤1.4 mass %, 1.9 mass %≤Mo+W/2≤4.0 mass %, 0.2 mass %≤V≤1.0 mass %, and 0.01≤N≤0.10 mass %, with the balance being Fe and inevitable impurities, in which, in a state after quenching and tempering, the steel has: a (Mo, W) carbide having a diameter of 0.2 μm or less being in an amount of 1.2 mass % or more, a ratio (mass ratio) of the amount of the (Mo, W) carbide to an amount of a Cr carbide being 11 or more, and a hardness change of 15 HRC or less.

Steel for mold, and mold
11535917 · 2022-12-27 · ·

The present invention relates to a steel for mold, containing: 0.28 mass %≤C≤0.65 mass %, 0.01 mass %≤Si≤0.30 mass %, 1.5 mass %≤Mn≤3.0 mass %, 0.5 mass %≤Cr≤1.4 mass %, 1.9 mass %≤Mo+W/2≤4.0 mass %, 0.2 mass %≤V≤1.0 mass %, and 0.01≤N≤0.10 mass %, with the balance being Fe and inevitable impurities, in which, in a state after quenching and tempering, the steel has: a (Mo, W) carbide having a diameter of 0.2 μm or less being in an amount of 1.2 mass % or more, a ratio (mass ratio) of the amount of the (Mo, W) carbide to an amount of a Cr carbide being 11 or more, and a hardness change of 15 HRC or less.

AUSTENITIC STAINLESS STEEL HAVING INCREASED YIELD RATIO AND MANUFACTURING METHOD THEREOF
20220403491 · 2022-12-22 · ·

Disclosed is an austenitic stainless steel having an increased yield ratio. The disclosed austenitic stainless steel is characterized by comprising, in percent by weight (wt %), 0.1% or less (exclusive of 0) of C, 0.2% or less (exclusive of 0) of N, 1.5 to 2.5% of Si, 6.0 to 10.0% of Mn, 15.0 to 17.0% of Cr, 0.3% or less (exclusive of 0) of Ni, 2.0 to 3.0% of Cu, and the remainder of Fe and other inevitable impurities, and satisfying Expressions (1) and (2) below.


3.2≤5.53+1.4Ni−0.16Cr+17.1(C+N)+0.722Mn+1.4Cu−5.59Si≤7  Expression (1):


551-462(C+N)−9.2Si−8.1Mn−13.7Cr−29(Ni+Cu)≤110  Expression (2): wherein C, N, Si, Mn, Cr, Ni, and Cu indicate the content (wt %) of respective elements.

THICK COMPOSITE-PHASE STEEL HAVING EXCELLENT DURABILITY AND MANUFACTURING METHOD THEREFOR
20220403489 · 2022-12-22 ·

Provided are thick hot-rolled composite-phase steel having excellent durability and a manufacturing method therefor. The thick composite-phase steel having excellent durability according to the present invention comprises, by wt %, C: 0.05 to 0.15%, Si: 0.01 to 1.0%, Mn: 1.0 to 2.3%, Al: 0.01 to 0.1%, Cr: 0.005 to 1.0%, P: 0.001 to 0.05%, S: 0.001 to 0.01%, N: 0.001 to 0.01%, Nb: 0.005 to 0.07%, Ti: 0.005 to 0.11%, Fe, and inevitable impurities, and has a mixed phase of ferrite and bainite as a base structure, wherein, in the base structure, the area fraction of each of a pearlite phase and a martensite and austenite (MA) phase is less than 5%, and the area fraction of a martensite phase is less than 10%.

THICK COMPOSITE-PHASE STEEL HAVING EXCELLENT DURABILITY AND MANUFACTURING METHOD THEREFOR
20220403489 · 2022-12-22 ·

Provided are thick hot-rolled composite-phase steel having excellent durability and a manufacturing method therefor. The thick composite-phase steel having excellent durability according to the present invention comprises, by wt %, C: 0.05 to 0.15%, Si: 0.01 to 1.0%, Mn: 1.0 to 2.3%, Al: 0.01 to 0.1%, Cr: 0.005 to 1.0%, P: 0.001 to 0.05%, S: 0.001 to 0.01%, N: 0.001 to 0.01%, Nb: 0.005 to 0.07%, Ti: 0.005 to 0.11%, Fe, and inevitable impurities, and has a mixed phase of ferrite and bainite as a base structure, wherein, in the base structure, the area fraction of each of a pearlite phase and a martensite and austenite (MA) phase is less than 5%, and the area fraction of a martensite phase is less than 10%.

HOT STAMPED BODY

A hot stamped body with high strength, good bendability and crack propagation resistance, consisting of: in mass %, C: 0.06% or more to less than 0.20%, Si: 0.010-1.00%, Mn: 0.80-2.00%, P: 0.100% or less, S: 0.010% or less, Al: 0.010-0.500%, N: 0.010% or less, Nb: more than 0.020% to 0.10% or less, Ti: 0-0.10%, V: 0-0.10%, Cr: 0-0.50%, Mo: 0-1.00%, B: 0-0.0100%, Ni: 0-0.50%, REM: 0-0.0100%, Mg: 0-0.010%, Ca: 0-0.0100%, and Co: 0-2.0%, with the balance: Fe and impurities, wherein a microstructure includes, in area fraction, ferrite: 5-50%, and martensite: 50-95%, a proportion of regions in the martensite where GAIQ values are 35000 or more to less than 45000 is 30 area % or more, and a maximum bending angle α (deg) is 90 or more.

HOT STAMPED BODY

A hot stamped body with high strength and good bendability, comprising a chemical composition consisting of: in mass %, C: 0.06% or more to less than 0.20%, Si: 0.010 to 1.00%, Mn: 1.20 to 3.00%, P: 0.100% or less, S: 0.010% or less, Al: 0.010 to 0.500%, N: 0.010% or less, Nb: 0.0010 to 0.020%, Ti: 0 to 0.10%, V: 0 to 0.10%, Cr: 0 to 0.50%, Mo: 0 to 1.00%, B: 0 to 0.0100%, Ni: 0 to 0.50%, REM: 0 to 0.0100%, Mg: 0 to 0.010%, Ca: 0 to 0.0100%, and Co: 0 to 2.0%, with the balance: Fe and impurities, wherein a microstructure includes martensite: 85% or more, a proportion of regions in the martensite where GAIQ values are 35000 or more to less than 45000 is 30 area % or more, and TS×α, is 105000 or more, and α is 75 or more.

HOT STAMPED BODY

A hot stamped body with high strength and good bendability, comprising a chemical composition consisting of: in mass %, C: 0.06% or more to less than 0.20%, Si: 0.010 to 1.00%, Mn: 1.20 to 3.00%, P: 0.100% or less, S: 0.010% or less, Al: 0.010 to 0.500%, N: 0.010% or less, Nb: 0.0010 to 0.020%, Ti: 0 to 0.10%, V: 0 to 0.10%, Cr: 0 to 0.50%, Mo: 0 to 1.00%, B: 0 to 0.0100%, Ni: 0 to 0.50%, REM: 0 to 0.0100%, Mg: 0 to 0.010%, Ca: 0 to 0.0100%, and Co: 0 to 2.0%, with the balance: Fe and impurities, wherein a microstructure includes martensite: 85% or more, a proportion of regions in the martensite where GAIQ values are 35000 or more to less than 45000 is 30 area % or more, and TS×α, is 105000 or more, and α is 75 or more.