C23C24/06
METHOD OF COMPACTING AN ANTI-CORROSIVE PAINT OF A TURBINE ENGINE PART
A method of compacting an anti-corrosive paint comprising metal particles and covering a mechanical part such as a turbine engine part, the method comprising a step of at least one spraying of solid ice particles on the part so as to densify and to make the paint electrically conductive.
METHOD OF COMPACTING AN ANTI-CORROSIVE PAINT OF A TURBINE ENGINE PART
A method of compacting an anti-corrosive paint comprising metal particles and covering a mechanical part such as a turbine engine part, the method comprising a step of at least one spraying of solid ice particles on the part so as to densify and to make the paint electrically conductive.
FORMING METHOD OF YTTRIUM OXIDE FLUORIDE COATING FILM AND YTTRIUM OXIDE FLUORIDE COATING FILM PREPARED THEREBY
A forming method of an yttrium oxide fluoride (YOF) coating film and a (YOF) coating film formed thereby are disclosed. The YOF coating film has no or extremely small pores therein and a nanostructure to increase light transmittance thereof, and has high hardness and high bonding strength and thus can protect a transparent window of a display device. The method for forming an YOF coating film involves the steps of: providing pretreated YOF powder having a particle diameter ranging from 0.1 to 12 m; receiving a transfer gas supplied from a transfer gas supply unit and receiving the pretreated YOF powder supplied from a powder supply unit to transfer the pretreated YOF powder in an aerosol state; and colliding/smashing (spraying) the pretreated YOF powder transferred in the aerosol state with/onto a substrate in a process chamber to form an YOF coating film on the substrate.
FORMING METHOD OF YTTRIUM OXIDE FLUORIDE COATING FILM AND YTTRIUM OXIDE FLUORIDE COATING FILM PREPARED THEREBY
A forming method of an yttrium oxide fluoride (YOF) coating film and a (YOF) coating film formed thereby are disclosed. The YOF coating film has no or extremely small pores therein and a nanostructure to increase light transmittance thereof, and has high hardness and high bonding strength and thus can protect a transparent window of a display device. The method for forming an YOF coating film involves the steps of: providing pretreated YOF powder having a particle diameter ranging from 0.1 to 12 m; receiving a transfer gas supplied from a transfer gas supply unit and receiving the pretreated YOF powder supplied from a powder supply unit to transfer the pretreated YOF powder in an aerosol state; and colliding/smashing (spraying) the pretreated YOF powder transferred in the aerosol state with/onto a substrate in a process chamber to form an YOF coating film on the substrate.
System for increasing the bulk density of metal powder
An apparatus for increasing the bulk density of metal powder includes a sealed chamber, a nozzle, and a target. The sealed chamber has an inert environment. The nozzle is coupled to an inert gas source and is configured to introduce raw metal powder into a flow of the inert gas for discharge as a cold spray mixture of the raw metal powder and the inert gas into the sealed chamber. The target is housed within the sealed chamber and is configured to receive an impact of the cold spray mixture. The nozzle and the target are configured to flatten the raw metal particles into flattened metal particles in response to the cold spray mixture impacting the target.
System for increasing the bulk density of metal powder
An apparatus for increasing the bulk density of metal powder includes a sealed chamber, a nozzle, and a target. The sealed chamber has an inert environment. The nozzle is coupled to an inert gas source and is configured to introduce raw metal powder into a flow of the inert gas for discharge as a cold spray mixture of the raw metal powder and the inert gas into the sealed chamber. The target is housed within the sealed chamber and is configured to receive an impact of the cold spray mixture. The nozzle and the target are configured to flatten the raw metal particles into flattened metal particles in response to the cold spray mixture impacting the target.
Coatings for SOFC metallic interconnects
Various methods of treating a chromium iron interconnect for a solid oxide fuel cell stack and coating the interconnect with a ceramic layer are provided.
Coatings for SOFC metallic interconnects
Various methods of treating a chromium iron interconnect for a solid oxide fuel cell stack and coating the interconnect with a ceramic layer are provided.
MACRO-MOLECULAR LEAKAGE-FREE SELF-ADHERING ALUMINUM FOIL AND MANUFACTURING METHOD THEREOF
A macro-molecular leakage-free self-adhering aluminum foil has two layers of aluminum foil compounded using a PET film, and the other surfaces of each layer coated with a modified PE adhesive layer respectively; or air gaps in one surface or two surfaces are filled with nano-aluminum to form a permeable air gap-free surface. The foil has advantages: 1. high folding resistance, fatigue resistance and strength 2, wrapping self-adhering performance is good, and stripping strength formed after adhesion is several times as high as that of the prior art; 3, air gaps in the surface of the aluminum foil filled with nano-aluminum powder result in improved compactness; manufacture from low-grade aluminum foil, and so that rolling precision requirements are lowered, and manufacturing cost reduced; 4, insulating strength is high, shielding effect is good, the return loss phenomenon is avoided, and tensile strength is good.
MACRO-MOLECULAR LEAKAGE-FREE SELF-ADHERING ALUMINUM FOIL AND MANUFACTURING METHOD THEREOF
A macro-molecular leakage-free self-adhering aluminum foil has two layers of aluminum foil compounded using a PET film, and the other surfaces of each layer coated with a modified PE adhesive layer respectively; or air gaps in one surface or two surfaces are filled with nano-aluminum to form a permeable air gap-free surface. The foil has advantages: 1. high folding resistance, fatigue resistance and strength 2, wrapping self-adhering performance is good, and stripping strength formed after adhesion is several times as high as that of the prior art; 3, air gaps in the surface of the aluminum foil filled with nano-aluminum powder result in improved compactness; manufacture from low-grade aluminum foil, and so that rolling precision requirements are lowered, and manufacturing cost reduced; 4, insulating strength is high, shielding effect is good, the return loss phenomenon is avoided, and tensile strength is good.