C30B25/06
Deposition system for growth of inclined c-axis piezoelectric material structures
Systems and methods for growing hexagonal crystal structure piezoelectric material with a c-axis that is tilted (e.g., 25 to 50 degrees) relative to normal of a face of a substrate are provided. A deposition system includes a linear sputtering apparatus, a translatable multi-aperture collimator, and a translatable substrate table arranged to hold multiple substrates, with the substrate table and/or the collimator being electrically biased to a nonzero potential. An enclosure includes first and second deposition stations each including a linear sputtering apparatus, a collimator, and a deposition aperture.
Metal nitride material for thermistor, method for producing same, and film type thermistor sensor
Provided are a metal nitride material for a thermistor, which exhibits high reliability and high heat resistance and can be directly deposited on a film or the like without firing, a method for producing the metal nitride material for a thermistor, and a film type thermistor sensor. The metal nitride material for a thermistor consists of a metal nitride represented by the general formula: Ti.sub.xAl.sub.yN.sub.z (where 0.70y/(x+y)0.95, 0.4z0.5, and x+y+z=1), and the crystal structure thereof is a hexagonal wurtzite-type single phase.
Metal nitride material for thermistor, method for producing same, and film type thermistor sensor
Provided are a metal nitride material for a thermistor, which exhibits high reliability and high heat resistance and can be directly deposited on a film or the like without firing, a method for producing the metal nitride material for a thermistor, and a film type thermistor sensor. The metal nitride material for a thermistor consists of a metal nitride represented by the general formula: Ti.sub.xAl.sub.yN.sub.z (where 0.70y/(x+y)0.95, 0.4z0.5, and x+y+z=1), and the crystal structure thereof is a hexagonal wurtzite-type single phase.
Radiation detector, scintillator panel, and method for manufacturing the same
According to the embodiment, a radiation detector includes a photoelectric conversion substrate converting light to an electrical signal and a scintillator layer being in contact with the photoelectric conversion substrate and converting externally incident radiation to light. The scintillator layer is made of a phosphor containing Tl as an activator in CsI, which is a halide. A concentration of the activator in the phosphor is 1.6 mass %0.4 mass %, and a concentration distribution of the activator in an in-plane direction and a film thickness direction is within 15%.
Radiation detector, scintillator panel, and method for manufacturing the same
According to the embodiment, a radiation detector includes a photoelectric conversion substrate converting light to an electrical signal and a scintillator layer being in contact with the photoelectric conversion substrate and converting externally incident radiation to light. The scintillator layer is made of a phosphor containing Tl as an activator in CsI, which is a halide. A concentration of the activator in the phosphor is 1.6 mass %0.4 mass %, and a concentration distribution of the activator in an in-plane direction and a film thickness direction is within 15%.
Monolithic integrated lattice mismatched crystal template and preparation method thereof
The present invention provides a monolithic integrated lattice mismatched crystal template and a preparation method thereof by using low-viscosity material, the preparation method for the crystal template includes: providing a first crystal layer with a first lattice constant; growing a buffer layer on the first crystal layer; below the melting point of the buffer layer, growing a second crystal layer and a template layer by sequentially performing the growth process of a second crystal layer and the growth process of a first template layer on the buffer layer, or growing a template layer by directly performing a first template layer growth process on the buffer layer; melting and converting the buffer layer to an amorphous state, performing a second template layer growth process on the template layer grown by the first template layer growth process at the growth temperature above the glass transition temperature of the buffer layer, sequentially growing a template layer until the lattice of the template layer is fully relaxed. Compared to the prior art, the invention has advantages of simple preparation, achieving in various lattice constant material combinations on one substrate and low dislocation density, high crystal quality.
Monolithic integrated lattice mismatched crystal template and preparation method thereof
The present invention provides a monolithic integrated lattice mismatched crystal template and a preparation method thereof by using low-viscosity material, the preparation method for the crystal template includes: providing a first crystal layer with a first lattice constant; growing a buffer layer on the first crystal layer; below the melting point of the buffer layer, growing a second crystal layer and a template layer by sequentially performing the growth process of a second crystal layer and the growth process of a first template layer on the buffer layer, or growing a template layer by directly performing a first template layer growth process on the buffer layer; melting and converting the buffer layer to an amorphous state, performing a second template layer growth process on the template layer grown by the first template layer growth process at the growth temperature above the glass transition temperature of the buffer layer, sequentially growing a template layer until the lattice of the template layer is fully relaxed. Compared to the prior art, the invention has advantages of simple preparation, achieving in various lattice constant material combinations on one substrate and low dislocation density, high crystal quality.
METHOD OF MANUFACTURING SEMICONDUCTOR DEVICE, SUBSTRATE PROCESSING APPARATUS, AND RECORDING MEDIUM
There is provided a method of manufacturing a semiconductor device. The method includes: forming a first amorphous silicon film on a substrate in a process chamber; and etching a portion of the first amorphous silicon film using a hydrogen chloride gas under a temperature at which an amorphous state of the first amorphous silicon film is maintained, in the process chamber.
Electron Beam Heating and Atomic Surface Restructuring of Sapphire Surface
Systems, methods, and devices of the various embodiments may provide a mechanism to enable the growth of a rhombohedral epitaxy at a lower substrate temperature by energizing the atoms in flux, thereby reducing the substrate temperature to a moderate level. In various embodiments, sufficiently energized atoms provide the essential energy needed for the rhombohedral epitaxy process which deforms the original cubic crystalline structure approximately into a rhombohedron by physically aligning the crystal structure of both materials at a lower substrate temperature.
Depositing calcium fluoride template layers for solar cells
A biaxially textured crystalline layer formed on a substrate using ion beam assisted deposition (IBAD) is provided. The biaxially textured crystalline layer includes an oriented CaF.sub.2 crystalline layer having crystalline grains oriented in both in-plane and out-of-plane directions, where the out-of-plane orientation is a (111) out-of-plane orientation. The oriented CaF.sub.2 crystalline layer is disposed for growth of a subsequent epitaxial layer and the CaF.sub.2 crystalline layer is an IBAD CaF.sub.2 layer. The biaxially textured CaF.sub.2 layer can be used in a photovoltaic cell, an electronic or optoelectronic device, an integrated circuit, an optical sensor, or a magnetic device.