Patent classifications
C03B2201/28
OPTICAL FIBER WITH LOW LOSS AND NANOSCALE STRUCTURALLY HOMOGENEOUS CORE
An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup.1, the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius.
According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.
Reducing light-induced loss in optical fibre
A supercontinuum source including a pump source and a supercontinuum generator configured for receiving electromagnetic radiation derived from the pump source and for generating supercontinuum radiation, the supercontinuum generator including a nonlinear microstructured optical fibre having a core region comprising silica. The core region includes a dopant selected to reduce light-induced non-bridging oxygen hole centre loss in the nonlinear microstructured optical fibre.
LOW BEND LOSS SINGLE MODE OPTICAL FIBER WITH BROMINE UP-DOPED CLADDING
According to embodiments, an optical fiber may include a core portion comprising an outer radius r.sub.C and a maximum relative refractive index .sub.Cmax. A cladding may surround the core portion and include a low-index trench and an outer cladding. The low index trench may surround the core portion and includes an outer radius r.sub.T and relative refractive index .sub.T. The outer cladding may surround and be in direct contact with the low-index trench. The outer cladding may be formed from silica-based glass comprising greater than 1.0 wt. % bromine and has a relative refractive index .sub.OC, wherein .sub.cmas>.sub.OC>.sub.T. The optical fiber may have a cable cutoff of less than or equal to 1530 nm. An attenuation of the optical fiber may be less than or equal to 0.185 dB/km at a wavelength of 1550 nm.
Optical fiber with low loss and nanoscale structurally homogeneous core
An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup.1, the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius. According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.
OPTICAL FIBER AND METHOD OF PRODUCING AN OPTICAL FIBER
An optical fiber package is described comprising a light transmitting core having a core diameter, a coating layer surrounding the core, and wherein the amount of chlorine in the light transmitting core region is homogeneous and comprises at least 3000 ppm. The fiber package is such that the optical fiber core exhibits a reduction in the hydrogen induced attenuation losses. A method for fabricating the optical fiber package is also disclosed.
High strength and aesthetic lithium disilicate crystalline glass-ceramics containing cristobalite crystal and preparation method thereof
Provided is lithium disilicate crystalline glass containing cristobalite crystal phase for high strength and aesthetic traits and its manufacturing process thereof. Exemplary embodiments of the present invention provide the high strength and aesthetic lithium disilicate crystalline glass, one kind of dental restoration materials, and its manufacturing method which induces the growth of the different crystal phase, cristobalite, from glass with lithium disilicate crystal.
REDUCING LIGHT-INDUCED LOSS IN OPTICAL FIBRE
A supercontinuum source including a pump source and a supercontinuum generator configured for receiving electromagnetic radiation derived from the pump source and for generating supercontinuum radiation, the supercontinuum generator including a nonlinear microstructured optical fibre having a core region comprising silica. The core region includes a dopant selected to reduce light-induced non-bridging oxygen hole centre loss in the nonlinear microstructured optical fibre.
OPTICAL FIBER WITH LOW LOSS AND NANOSCALE STRUCTURALLY HOMOGENEOUS CORE
An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup., the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius.
According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.
Optical Fiber, Optical Fiber Preparation Method, and Optical Fiber Amplifier
Proportions of the element erbium, the element aluminum, and the element phosphorus are adjusted during optical fiber preparation so that aluminum phosphate is formed around the element erbium in a prepared optical fiber, a probability that the element erbium in the optical fiber transits to a high energy level is reduced, and an excited-state absorption effect of the element erbium in the optical fiber on an optical signal is suppressed.