C03C3/064
ANTIBACTERIAL GLASS COMPOSITION AND PREPARATION METHOD THEREFOR
There is disclosed an antibacterial glass composite that may be made of components harmless to the human body and have excellent durability and chemical resistance, thereby maintaining an antibacterial function for a long time, and a manufacturing method thereof.
ANTIBACTERIAL GLASS COMPOSITION AND PREPARATION METHOD THEREFOR
There is disclosed an antibacterial glass composite that may be made of components harmless to the human body and have excellent durability and chemical resistance, thereby maintaining an antibacterial function for a long time, and a manufacturing method thereof.
Flexible ceramic coatings for metals and methods of making same
Bulk paint and ceramic powder systems, methods of forming same, and methods of forming a flexible ceramic coating on a metal substrate are disclosed. The systems may include a ceramic composition having between 2 to 30 weight percent of an alkali metal oxide, such as K.sub.2O, Na.sub.2O, and Li.sub.2O or mixtures thereof, between 10 to 74 weight percent SiO.sub.2, and between 23 to 79 weight percent B.sub.2O.sub.3. Additives that are nonwetting with molten metals, such as boron nitride, provide durable coatings for metal processing operations. The ceramic composition may include less than 5 weight percent additional metal oxides. The bulk paint system further may include water and a cellulosic suspension agent to form a bulk paint. The ceramic powder system may be processed to form a uniform powder. The bulk paint or uniform powder may be applied to a metal substrate, such as a ferrous metal substrate, dried, and heated to form a flexible coating on the metal substrate.
Flexible ceramic coatings for metals and methods of making same
Bulk paint and ceramic powder systems, methods of forming same, and methods of forming a flexible ceramic coating on a metal substrate are disclosed. The systems may include a ceramic composition having between 2 to 30 weight percent of an alkali metal oxide, such as K.sub.2O, Na.sub.2O, and Li.sub.2O or mixtures thereof, between 10 to 74 weight percent SiO.sub.2, and between 23 to 79 weight percent B.sub.2O.sub.3. Additives that are nonwetting with molten metals, such as boron nitride, provide durable coatings for metal processing operations. The ceramic composition may include less than 5 weight percent additional metal oxides. The bulk paint system further may include water and a cellulosic suspension agent to form a bulk paint. The ceramic powder system may be processed to form a uniform powder. The bulk paint or uniform powder may be applied to a metal substrate, such as a ferrous metal substrate, dried, and heated to form a flexible coating on the metal substrate.
Low dielectric loss glasses for electronic devices
An article including a glass having that includes SiO.sub.2, Al.sub.2O.sub.3, and B.sub.2O.sub.3 and least one of Li.sub.2O, Na.sub.2O, K.sub.2O, MgO, CaO, SrO, BaO, SnO.sub.2, ZnO, La.sub.2O.sub.3, F, and Fe.sub.2O.sub.3, wherein the glass includes a dielectric constant of about 10 or less and/or a loss tangent of about 0.01 or less, both as measured with signals at 10 GHz.
Tubular member for exhaust gas treatment device and exhaust gas treatment device using the tubular member, and method of manufacturing tubular member for exhaust gas treatment device
A tubular member for an exhaust gas treatment device according to at least one embodiment of the present invention includes: a tubular main body made of a metal; and an insulating layer formed at least on an inner peripheral surface of the tubular main body. The insulating layer contains glass containing a crystalline substance, and the glass contains silicon, boron, and magnesium.
WAVELENGTH CONVERSION MEMBER, AND LIGHT EMITTING DEVICE USING SAME
Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.
WAVELENGTH CONVERSION MEMBER, AND LIGHT EMITTING DEVICE USING SAME
Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO.sub.2, 0 to 20% B.sub.2O.sub.3, 0 to 25% Al.sub.2O.sub.3, 0 to 3% Li.sub.2O, 0 to 3% Na.sub.2O, 0 to 3% K.sub.2O, 0 to 3% Li.sub.2O+Na.sub.2O+K.sub.2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.
Antimicrobial glass compositions, glasses and polymeric articles incorporating the same
Embodiments of the present invention pertain to antimicrobial glass compositions, glasses, and articles. The articles include a glass, which may include a glass phase and a cuprite phase. In other embodiments, the glasses include a plurality of Cu.sup.1+ ions, a degradable phase including B.sub.2O.sub.3, P.sub.2O.sub.5 and K.sub.2O, and a durable phase including SiO.sub.2. Other embodiments include glasses having a plurality of Cu.sup.1+ ions disposed on the surface of the glass and in the glass network and/or the glass matrix. The article may also include a polymer. The glasses and articles disclosed herein exhibit a 2 log reduction or greater in a concentration of at least one of Staphylococcus aureus, Enterobacter aerogenes, Pseudomonas aeruginosa bacteria, Methicillin Resistant Staphylococcus aureus, and E. coli, under the EPA Test Method for Efficacy of Copper Alloy as a Sanitizer testing condition and under Modified JIS Z 2801 for Bacteria testing conditions.
Antimicrobial glass compositions, glasses and polymeric articles incorporating the same
Embodiments of the present invention pertain to antimicrobial glass compositions, glasses, and articles. The articles include a glass, which may include a glass phase and a cuprite phase. In other embodiments, the glasses include a plurality of Cu.sup.1+ ions, a degradable phase including B.sub.2O.sub.3, P.sub.2O.sub.5 and K.sub.2O, and a durable phase including SiO.sub.2. Other embodiments include glasses having a plurality of Cu.sup.1+ ions disposed on the surface of the glass and in the glass network and/or the glass matrix. The article may also include a polymer. The glasses and articles disclosed herein exhibit a 2 log reduction or greater in a concentration of at least one of Staphylococcus aureus, Enterobacter aerogenes, Pseudomonas aeruginosa bacteria, Methicillin Resistant Staphylococcus aureus, and E. coli, under the EPA Test Method for Efficacy of Copper Alloy as a Sanitizer testing condition and under Modified JIS Z 2801 for Bacteria testing conditions.