C03C2201/22

Photonic crystal fiber, a method of production thereof and a supercontinuum light source

The invention concerns a Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and comprises a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region comprises a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF comprises hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further comprises a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below Th, wherein Th is at least about 50? C., preferably 50? C.<Th<250? C.

Method of processing optical fiber
09919964 · 2018-03-20 · ·

A method of processing an optical fiber of the invention includes: a determination step of determining at least an ambient temperature of conditions of a diffusion treatment that causing an optical fiber to be subjected to an non-oxygen bridging atmosphere; an exposure step of exposing the optical fiber to a gas including an oxygen bridging element that is capable of processing the Non-Bridging Oxygen Hole Centers by being bonded to a non-bridging oxygen in the optical fiber, and causing the oxygen bridging element to infiltrate into the optical fiber; and a diffusion step of subsequently causing the optical fiber to be subjected to the non-oxygen bridging atmosphere in the exposure ambient temperature which is determined by the determination step and at which the optical fiber is subjected to the non-oxygen bridging atmosphere, and thereby diffusing the oxygen bridging element into the optical fiber.

Optical fiber with reducing hydrogen sensitivity

The present disclosure is directed to a method of making an optical fiber with improved bend performance, the optical fiber having a core and at least one cladding layer, and a chlorine content in the in the last layer of the at least one cladding layer that is greater than 500 ppm by weight. The fiber is prepared using a mixture of a carrier gas, a gaseous chlorine source material and a gaseous reducing agent during the sintering of the last or outermost layer of the at least one cladding layer. The inclusion of the reducing gas into a mixture of the carrier gas and gaseous chlorine material reduces oxygen-rich defects that results in at least a 20% reduction in TTP during hydrogen aging testing.

Photonic crystal fiber, a method of production thereof and a supercontinuum light source

A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein T.sub.h is at least about 50 C., preferably 50 C.<T.sub.h<250 C.

OPTICAL FIBER WITH REDUCING HYDROGEN SENSITIVITY

The present disclosure is directed to a method of making an optical fiber with improved bend performance, the optical fiber having a core and at least one cladding layer, and a chlorine content in the in the last layer of the at least one cladding layer that is greater than 500 ppm by weight. The fiber is prepared using a mixture of a carrier gas, a gaseous chlorine source material and a gaseous reducing agent during the sintering of the last or outermost layer of the at least one cladding layer. The inclusion of the reducing gas into a mixture of the carrier gas and gaseous chlorine material reduces oxygen-rich defects that results in at least a 20% reduction in TTP during hydrogen aging testing.

Optical fiber with reducing hydrogen sensitivity

The present disclosure is directed to a method of making an optical fiber with improved bend performance, the optical fiber having a core and at least one cladding layer, and a chlorine content in the in the last layer of the at least one cladding layer that is greater than 500 ppm by weight. The fiber is prepared using a mixture of a carrier gas, a gaseous chlorine source material and a gaseous reducing agent during the sintering of the last or outermost layer of the at least one cladding layer. The inclusion of the reducing gas into a mixture of the carrier gas and gaseous chlorine material reduces oxygen-rich defects that results in at least a 20% reduction in TTP during hydrogen aging testing.

PHOTONIC CRYSTAL FIBER, A METHOD OF PRODUCTION THEREOF AND A SUPERCONTINUUM LIGHT SOURCE

A Photonic Crystal Fiber (PCF) a method of its production and a supercontinuum light source comprising such PCF. The PCF has a longitudinal axis and includes a core extending along the length of said longitudinal axis and a cladding region surrounding the core. At least the cladding region includes a plurality of microstructures in the form of inclusions extending along the longitudinal axis of the PCF in at least a microstructured length section. In at least a degradation resistant length section of the microstructured length section the PCF includes hydrogen and/or deuterium. In at least the degradation resistant length section the PCF further includes a main coating surrounding the cladding region, which main coating is hermetic for the hydrogen and/or deuterium at a temperature below T.sub.h, wherein T.sub.h is at least about 50 C., preferably 50 C.<T.sub.h<250 C.

METHOD OF NANOFIBER FABRICATION WITH A DEUTERIUM OR TRITIUM FLAME
20250296868 · 2025-09-25 ·

The present invention relates to a fabrication technique of nanofiber devices particularly useful for applications with telecommunication wavelengths. By utilizing deuterium or tritium gases in the heating process, we mitigate the absorption losses associated with OH-bond vibrations in silica glass during high-temperature flame stretching. The shifted absorption bands of OD (deuterated hydroxyl group) or OT (tritiated hydroxyl group) result in reduced transmission losses at the telecommunication bands and improve the performance of nanofiber devices in optical communication, quantum computing and quantum communication applications.