C03C2201/28

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES

Systems and methods for forming an oxidation protection system, on a composite structure is provided. In various embodiments, an oxidation protection system disposed on a substrate may comprise a borosilicate glass layer comprising a borosilicate glass, a base layer comprising a first pre-slurry composition comprising a first phosphate glass composition, and/or a sealing layer comprising a second pre-slurry composition comprising a second phosphate glass composition. The borosilicate glass layer, base layer, and/or sealing layer may be disposed in any suitable order relative to the composite structure.

OPTICAL FIBER
20190204512 · 2019-07-04 · ·

An optical fiber includes: a core that includes quartz glass doped with a core updopant; an inner cladding that includes quartz glass doped with a cladding updopant and a downdopant and that covers a circumferential surface of the core; and an outer cladding that includes quartz glass and that covers an outer circumferential surface of the inner cladding. A refractive index of the inner cladding is substantially equal to a refractive index of the outer cladding. The inner cladding contains the cladding updopant at a concentration such that a refractive index increase rate ascribed to the cladding updopant falls within a range of 0.25% to 0.5%.

Optical fiber with low loss and nanoscale structurally homogeneous core

An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup.1, the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius. According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.

OPTICAL FIBER WITH LOW LOSS AND NANOSCALE STRUCTURALLY HOMOGENEOUS CORE

An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup.1, the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius.

According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.

GLASS COMPOSITE FOR USE IN EXTREME ULTRA VIOLET LITHOGRAPHY
20180105452 · 2018-04-19 · ·

A glass composite for use in Extreme Ultra-Violet Lithography (EUVL) is provided. The glass composite includes a first silica-titania glass section. The glass composite further includes a second doped silica-titania glass section mechanically bonded to a surface of the first silica-titania glass section, wherein the second doped silica-titania glass section has a thickness of greater than about 1.0 inch.

Optical fiber with low loss and nanoscale structurally homogeneous core

An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup.1, the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius. According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.

Multimode optical fiber

The present invention relates to an MMF with a structure for relaxing wavelength dependence of transmission bandwidth. In the MMF, a doping amount of a dopant for control of refractive index is adjusted, so as to make each of an OFL bandwidth at a wavelength of 850 nm and an OFL bandwidth at a wavelength of at least one of 980 nm, 1060 nm, and 1300 nm become not less than 1500 MHz.Math.km, make the OFL bandwidth at the wavelength of at least one of 980 nm, 1060 nm, and 1300 nm become wider than the OFL bandwidth at the wavelength of 850 nm, and effectively suppress increase in transmission loss.

MULTIMODE OPTICAL FIBER
20170139130 · 2017-05-18 ·

The present invention relates to an MMF with a structure for relaxing wavelength dependence of transmission bandwidth. In the MMF, a doping amount of a dopant for control of refractive index is adjusted, so as to make each of an OFL bandwidth at a wavelength of 850 nm and an OFL bandwidth at a wavelength of at least one of 980 nm, 1060 nm, and 1300 nm become not less than 1500 MHz.Math.km, make the OFL bandwidth at the wavelength of at least one of 980 nm, 1060 nm, and 1300 nm become wider than the OFL bandwidth at the wavelength of 850 nm, and effectively suppress increase in transmission loss.

OPTICAL FIBER WITH LOW LOSS AND NANOSCALE STRUCTURALLY HOMOGENEOUS CORE

An optical fiber has a core region that is doped with one or more viscosity-reducing dopants in respective amounts that are configured, such that, in a Raman spectrum with a frequency shift of approximately 600 cm.sup., the fiber has a nanoscale structure having an integrated D2 line defect intensity of less than 0.025. Alternatively, the core region is doped with one or more viscosity-reducing dopants in respective amounts that are configured such that the fiber has a residual axial compressive stress with a stress magnitude of more than 20 MPa and a stress radial extent between 2 and 7 times the core radius.

According to another aspect of the invention a majority of the optical propagation through the fiber is supported by an identified group of fiber regions comprising the core region and one or more adjacent cladding regions. The fiber regions are doped with one or more viscosity-reducing dopants in respective amounts and radial positions that are configured to achieve viscosity matching among the fiber regions in the identified group.

EAR IMPLANT
20250195208 · 2025-06-19 · ·

The invention relates to an ear implant for improving or restoring the hearing ability in the event of defects in the area of the ossicles of the ear or posterior wall of the auditory canal, said implant consisting of lithium disilicate glass ceramic having a molar ratio of SiO.sub.2 to Li.sub.2O of 2 to 3, wherein the glass ceramic material being doped and stabilized with P.sub.2O.sub.5 and ZrO.sub.2, as well as a method for the production of the implant and the use of lithium disilicate glass ceramics in ear implants.