Patent classifications
C03C2217/944
SOLAR-CONTROL GLAZING
The present invention relates to solar-control glazings intended to be fitted in buildings, but also in motor vehicles. They comprise a glass substrate carrying a transparent multilayer stack comprising an alternation of n silver-based functional layers that reflect infrared radiation and of n+1 dielectric coatings, with n1, such that each functional layer is surrounded by dielectric coating. At least one of the dielectric coatings comprises a substantially metallic solar radiation absorbing layer based on Pd, enclosed between and in contact with two dielectric oxide layers of at least one element selected from Zn, Sn, Al, In, Nb, Ti and Zr.
Transparent pane
A transparent pane comprising a transparent substrate and an electrically conductive coating on a surface of the transparent substrate is disclosed. The electrically conductive coating comprises four functional layers arranged one atop another. Each functional layer comprises a layer of optically highly refractive material with a refractive index >1.3, a first matching layer above the layer of optically highly refractive material, an electrically conductive layer above the first matching layer, and a second matching layer above the electrically conductive layer. The layer thickness of each conductive layer can be 5 nm to 25 nm and the total layer thickness of all electrically conductive layers can be 20 nm to 100 nm.
Low-E matchable coated articles having absorber film and corresponding methods
A low-E coating has good color stability (a low E* value) upon heat treatment (HT). Thermal stability may be improved by the provision of an as-deposited crystalline or substantially crystalline layer of or including zinc oxide, doped with at least one dopant (e.g., Sn), immediately under an infrared (IR) reflecting layer of or including silver; and/or by the provision of at least one dielectric layer of or including an oxide of zirconium. These have the effect of significantly improving the coating's thermal stability (i.e., lowering the E* value). An absorber film may be designed to adjust visible transmission and provide desirable coloration, while maintaining durability and/or thermal stability. The dielectric layer (e.g., of or including an oxide of Zr) may be sputter-deposited so as to have a monoclinic phase in order to improve thermal stability.
Transparent Conductive Oxide having an Embedded Film
The present invention is directed to coated articles. A substrate is coated with an underlayer having at a first underlayer film made of a first high refractive index material. A transparent conductive oxide layer over at least a portion of the underlayer. An embedded film is embedded within the transparent conductive oxide layer wherein the embedded film comprises a second high refractive index material.
Transparent conductive oxide having an embedded film
The present invention is directed to coated articles. A substrate is coated with an underlayer having at a first underlayer film made of a first high refractive index material. A transparent conductive oxide layer over at least a portion of the underlayer. An embedded film is embedded within the transparent conductive oxide layer wherein the embedded film comprises a second high refractive index material.
METHOD OF MANUFACTURE OF A COATED GLAZING
A method of manufacture of a coated glazing includes the following steps in sequence a) providing a transparent glass substrate, b) etching a surface of the substrate with an acidic gas, and c) directly or indirectly coating said surface with at least one layer based on a transparent conductive coating (TCC) and/or at least one layer based on a material with a refractive index of at least 1.75.
LOW-E MATCHABLE COATED ARTICLES HAVING ABSORBER FILM AND CORRESPONDING METHODS
A low-E coating has good color stability (a low E* value) upon heat treatment (HT). Thermal stability may be improved by the provision of an as-deposited crystalline or substantially crystalline layer of or including zinc oxide, doped with at least one dopant (e.g., Sn), immediately under an infrared (IR) reflecting layer of or including silver; and/or by the provision of at least one dielectric layer of or including an oxide of zirconium. These have the effect of significantly improving the coating's thermal stability (i.e., lowering the E* value). An absorber film may be designed to adjust visible transmission and provide desirable coloration, while maintaining durability and/or thermal stability. The dielectric layer (e.g., of or including an oxide of Zr) may be sputter-deposited so as to have a monoclinic phase in order to improve thermal stability.
Transparent conductive oxide having an embedded film
The present invention is directed to coated articles. A substrate is coated with an underlayer having at a first underlayer film made of a first high refractive index material. A transparent conductive oxide layer over at least a portion of the underlayer. An embedded film is embedded within the transparent conductive oxide layer wherein the embedded film comprises a second high refractive index material.
Coated Article Having a Protective Coating Containing Silicon Nitride and/or Silicon Oxynitride
A coated article includes a substrate, a functional layer over at least a portion of the substrate, and a protective coating over at least a portion of the functional layer, wherein an uppermost layer of the functional layer is a metal oxide layer, and wherein the protective coating comprises a metal nitride layer and a metal oxynitride layer that is disposed between and in contact with at least part of the metal nitride layer and the metal oxide layer of the functional layer.
Coated glazing
A coated glazing comprising: a transparent glass substrate, wherein a surface of the substrate is directly or indirectly coated with at least one layer based on a transparent conductive coating (TCC) and/or at least one layer based on a material with a refractive index of at least 1.75, and wherein said surface has an arithmetical mean height of the surface value, Sa, of at least 0.4 nm prior to said coating of said surface.