C04B14/047

Magnesium phosphate cement

Magnesium phosphate cement binder systems and method for providing magnesium phosphate cements are described. In an embodiment, a magnesium phosphate cement binder system may include magnesium oxide that has been calcined at a temperature of between about 900° F. to about 1800° F. The magnesium phosphate cement binder system may also include a phosphate material. Other formulations, compositions, and methods are also described.

Magnesium phosphate cement

Magnesium phosphate cement binder systems and method for providing magnesium phosphate cements are described. In an embodiment, a magnesium phosphate cement binder system may include magnesium oxide that has been calcined at a temperature of between about 900° F. to about 1800° F. The magnesium phosphate cement binder system may also include a phosphate material. Other formulations, compositions, and methods are also described.

Weighted Composition for Treatment of a Subterranean Formation

Various embodiments disclosed relate to a weighted composition for treatment of a subterranean formation. In various embodiments, the present invention provides a method of treating a subterranean formation. The method can include placing in a subterranean formation a weighted composition. The weighted composition can include a weighting agent and an inorganic coating material on the weighting agent. The inorganic coating material can be a crystalline inorganic coating material. The inorganic coating material can be an amorphous inorganic coating material.

Weighted Composition for Treatment of a Subterranean Formation

Various embodiments disclosed relate to a weighted composition for treatment of a subterranean formation. In various embodiments, the present invention provides a method of treating a subterranean formation. The method can include placing in a subterranean formation a weighted composition. The weighted composition can include a weighting agent and an inorganic coating material on the weighting agent. The inorganic coating material can be a crystalline inorganic coating material. The inorganic coating material can be an amorphous inorganic coating material.

Compositions containing kiln dust and/or biowaste ash and methods of use

An embodiment comprises a method of treating a subterranean formation comprising: providing a treatment fluid comprising a kiln dust, biowaste ash, and water; and introducing the treatment fluid into a subterranean formation. Another embodiment comprises a method of cementing comprising: introducing a cement composition into a subterranean formation, wherein the cement composition comprises a kiln dust, biowaste ash, and water; and allowing the cement composition to set in the subterranean formation. Yet another embodiment comprises a method comprising: providing a spacer fluid comprising biowaste ash and water; introducing the spacer fluid into a well bore to displace at least a portion of a first fluid from the well bore; and introducing a cement composition into the well bore, wherein the spacer fluid separates the cement composition and the first fluid.

Compositions containing kiln dust and/or biowaste ash and methods of use

An embodiment comprises a method of treating a subterranean formation comprising: providing a treatment fluid comprising a kiln dust, biowaste ash, and water; and introducing the treatment fluid into a subterranean formation. Another embodiment comprises a method of cementing comprising: introducing a cement composition into a subterranean formation, wherein the cement composition comprises a kiln dust, biowaste ash, and water; and allowing the cement composition to set in the subterranean formation. Yet another embodiment comprises a method comprising: providing a spacer fluid comprising biowaste ash and water; introducing the spacer fluid into a well bore to displace at least a portion of a first fluid from the well bore; and introducing a cement composition into the well bore, wherein the spacer fluid separates the cement composition and the first fluid.

Sealant compositions and methods utilizing nano-particles

The present invention includes well treatment fluids and methods utilizing nano-particles and, in certain embodiments, to sealant compositions and methods utilizing nano-particles. The nano-particles may be incorporated into the sealant composition in different forms, including as discrete nano-particles, encapsulated nano-particles, agglomerated nano-particles, or in a liquid suspension.

Sealant compositions and methods utilizing nano-particles

The present invention includes well treatment fluids and methods utilizing nano-particles and, in certain embodiments, to sealant compositions and methods utilizing nano-particles. The nano-particles may be incorporated into the sealant composition in different forms, including as discrete nano-particles, encapsulated nano-particles, agglomerated nano-particles, or in a liquid suspension.

Gypsum plaster-based material containing an EDTA metal complex

A plaster-based material, in particular a plasterboard intended for the interior fitting of dwellings, contains a metal complex of EDTA. The plaster-based material is used for reducing the amount of volatile organic compounds present in the atmosphere inside dwellings, offices or public buildings.

Gypsum plaster-based material containing an EDTA metal complex

A plaster-based material, in particular a plasterboard intended for the interior fitting of dwellings, contains a metal complex of EDTA. The plaster-based material is used for reducing the amount of volatile organic compounds present in the atmosphere inside dwellings, offices or public buildings.