C04B41/4574

APPARATUS AND METHOD FOR SPRAYING COLOR INTO CRACKS OF A MOVING FORMED QUARTZ SLAB TO CREATE VEINS IN AN ENGINEERED STONE
20190201928 · 2019-07-04 ·

An apparatus including a first device which moves a first portion of a soft, damp, slightly pressed slab out of alignment with a majority of the slab and thus introduces a first crack in the slab; and a device for spraying a first colored material into the first crack of the slab. The first device which moves the first portion of the slab out of alignment with the rest of the slab may include a first cylinder. The device for spraying the first colored material in the first crack of the slab may include a robotic apparatus. In at least one embodiment, the apparatus may also include a second device which moves a second portion of the slab out of alignment with the majority of the slab and thereby introduces a second crack in the slab.

Carbon-carbon composite component with antioxidant coating

In one example, a method including depositing an antioxidant material on a first surface region of a carbon-carbon composite substrate via a print head of a three-dimensional printing device to form a first layer of the antioxidant material on the first surface region of the substrate, and depositing the antioxidant material on a second surface region of the substrate via the print head of the three-dimensional printing device to form a second layer of the antioxidant material on the second surface region. The method may be, for example, a method for forming a carbon-carbon composite component including an antioxidant coating, the antioxidant coating including the first layer and second layer of the antioxidant material.

Carbon-carbon composite component with antioxidant coating

In one example, a method including depositing an antioxidant material on a first surface region of a carbon-carbon composite substrate via a print head of a three-dimensional printing device to form a first layer of the antioxidant material on the first surface region of the substrate, and depositing the antioxidant material on a second surface region of the substrate via the print head of the three-dimensional printing device to form a second layer of the antioxidant material on the second surface region. The method may be, for example, a method for forming a carbon-carbon composite component including an antioxidant coating, the antioxidant coating including the first layer and second layer of the antioxidant material.

Airfoil having environmental barrier topcoats that vary in composition by location

An airfoil includes an airfoil wall that defines a leading end, a trailing end, and suction and pressure sides that join the leading end and the trailing end. The airfoil wall is formed of a silicon-containing ceramic. A first environmental barrier topcoat is disposed on the suction side of the airfoil wall, and a second, different environmental barrier topcoat is disposed on the pressure side of the airfoil wall. The first topcoat is vaporization-resistant and the second topcoat is resistant to calcium-magnesium-aluminosilicate.

Airfoil having environmental barrier topcoats that vary in composition by location

An airfoil includes an airfoil wall that defines a leading end, a trailing end, and suction and pressure sides that join the leading end and the trailing end. The airfoil wall is formed of a silicon-containing ceramic. A first environmental barrier topcoat is disposed on the suction side of the airfoil wall, and a second, different environmental barrier topcoat is disposed on the pressure side of the airfoil wall. The first topcoat is vaporization-resistant and the second topcoat is resistant to calcium-magnesium-aluminosilicate.

Apparatus and method for spraying color into cracks of a moving formed quartz slab to create veins in an engineered stone
10189041 · 2019-01-29 ·

An apparatus including a device which moves a first portion of a soft, damp, and/or wet slab out of alignment with a majority of the slab and thus introduces a first crack in the slab; and a device for spraying a first colored material into the first crack of the slab. The device which moves the first portion of the slab out of alignment with the rest of the slab may include a first lift bar. The device for spraying the first colored material in the first crack of the slab may include a first spray bar having a plurality of nozzles fixed thereto, arranged in a substantially straight line. In at least one embodiment, the apparatus may also include a device which moves a second portion of the slab out of alignment with the majority of the slab and thereby introduces a second crack in the slab.

Apparatus and method for spraying color into cracks of a moving formed quartz slab to create veins in an engineered stone
10189041 · 2019-01-29 ·

An apparatus including a device which moves a first portion of a soft, damp, and/or wet slab out of alignment with a majority of the slab and thus introduces a first crack in the slab; and a device for spraying a first colored material into the first crack of the slab. The device which moves the first portion of the slab out of alignment with the rest of the slab may include a first lift bar. The device for spraying the first colored material in the first crack of the slab may include a first spray bar having a plurality of nozzles fixed thereto, arranged in a substantially straight line. In at least one embodiment, the apparatus may also include a device which moves a second portion of the slab out of alignment with the majority of the slab and thereby introduces a second crack in the slab.

Thin-film thermocouple for measuring the temperature of a ceramic matrix composite (CMC) component
10161807 · 2018-12-25 · ·

A thin-film thermocouple for measuring the temperature of a ceramic matrix composite (CMC) component includes a first thermocouple leg and a second thermocouple leg deposited on a surface of a CMC component, where each of the first and second thermocouple legs has a length extending from a reference end to a working end thereof. The working ends of the first and second thermocouple legs are joined at a junction region on the surface. At least one of the first thermocouple leg and the second thermocouple leg comprises silicon carbide.

Thin-film thermocouple for measuring the temperature of a ceramic matrix composite (CMC) component
10161807 · 2018-12-25 · ·

A thin-film thermocouple for measuring the temperature of a ceramic matrix composite (CMC) component includes a first thermocouple leg and a second thermocouple leg deposited on a surface of a CMC component, where each of the first and second thermocouple legs has a length extending from a reference end to a working end thereof. The working ends of the first and second thermocouple legs are joined at a junction region on the surface. At least one of the first thermocouple leg and the second thermocouple leg comprises silicon carbide.

Apparatus and method for spraying color into cracks of a moving formed quartz slab to create veins in an engineered stone
10099236 · 2018-10-16 ·

An apparatus including a device which moves a first portion of a soft, damp, and/or wet slab out of alignment with a majority of the slab and thus introduces a first crack in the slab; and a device for spraying a first colored material into the first crack of the slab. The device which moves the first portion of the slab out of alignment with the rest of the slab may include a first lift bar. The device for spraying the first colored material in the first crack of the slab may include a first spray bar having a plurality of nozzles fixed thereto, arranged in a substantially straight line. In at least one embodiment, the apparatus may also include a device which moves a second portion of the slab out of alignment with the majority of the slab and thereby introduces a second crack in the slab.