C04B41/85

ENVIRONMENTAL BARRIER COATING FOR ENHANCED RESISTANCE TO ATTACK BY MOLTEN SILICATE DEPOSITS

An environmental barrier coating, comprising a substrate containing silicon; an environmental barrier layer applied to said substrate; said environmental barrier layer comprising a rare earth composition.

Pillar shaped honeycomb structure, exhaust gas purifying device, exhaust system, and method for producing honeycomb structure

A pillar shaped honeycomb structure includes: a porous partition wall that defines a plurality of cells, the cells forming flow paths for a fluid, the cells extending from an inflow end face to an outflow end face; and an outer peripheral wall located at the outermost circumference. At least a part of surfaces of the partition walls has a surface layer, and the surface layer includes magnetic particles and has permeability.

ARTICLE FOR HIGH TEMPERATURE SERVICE
20230090598 · 2023-03-23 ·

An article for high temperature service is presented herein. One embodiment is an article including a substrate having a silicon-bearing ceramic matrix composite; and a layer disposed over the substrate, wherein the layer includes silicon and a dopant, the dopant including aluminum. In another embodiment, the article includes a ceramic matrix composite substrate, wherein the composite includes a silicon-bearing ceramic and a dopant, the dopant including aluminum; a bond coat disposed over the substrate, where the bond coat includes elemental silicon, a silicon alloy, a silicide, or combinations including any of the aforementioned; and a coating disposed over the bond coat, the coating including a silicate (such as an aluminosilicate or rare earth silicate), yttria-stabilized zirconia, or a combination including any of the aforementioned.

ARTICLE FOR HIGH TEMPERATURE SERVICE
20230090598 · 2023-03-23 ·

An article for high temperature service is presented herein. One embodiment is an article including a substrate having a silicon-bearing ceramic matrix composite; and a layer disposed over the substrate, wherein the layer includes silicon and a dopant, the dopant including aluminum. In another embodiment, the article includes a ceramic matrix composite substrate, wherein the composite includes a silicon-bearing ceramic and a dopant, the dopant including aluminum; a bond coat disposed over the substrate, where the bond coat includes elemental silicon, a silicon alloy, a silicide, or combinations including any of the aforementioned; and a coating disposed over the bond coat, the coating including a silicate (such as an aluminosilicate or rare earth silicate), yttria-stabilized zirconia, or a combination including any of the aforementioned.

METHOD FOR PRODUCING A CERAMIC PART WITH A MOTHER-OF-PEARL EFFECT, PARTICULARLY FOR WATCHMAKING
20220339816 · 2022-10-27 · ·

A method may produce a ceramic part with a mother-of-pearl effect, in particular for watchmaking. Such methods may include: forming a ceramic body; depositing a layer of an oxy-nitride component of the OxNy type on at least a portion of the ceramic body; and oxidizing at least a portion of the oxy-nitride layer, preferably by heating.

METHOD FOR PRODUCING A CERAMIC PART WITH A MOTHER-OF-PEARL EFFECT, PARTICULARLY FOR WATCHMAKING
20220339816 · 2022-10-27 · ·

A method may produce a ceramic part with a mother-of-pearl effect, in particular for watchmaking. Such methods may include: forming a ceramic body; depositing a layer of an oxy-nitride component of the OxNy type on at least a portion of the ceramic body; and oxidizing at least a portion of the oxy-nitride layer, preferably by heating.

ENVIRONMENTAL BARRIER COATING

An article includes a ceramic-based substrate and a barrier layer on the ceramic-based substrate. The barrier layer includes a matrix phase and gettering particles in the matrix phase. The gettering particles with an aspect ratio greater than one are aligned such that a maximum dimension of the gettering particles extends along an axis that is generally parallel to the substrate. The barrier layer includes a dispersion of diffusive particles in the matrix phase. A composite material and a method of applying a barrier layer to a substrate are also disclosed.

Lithium-stuffed garnet thin films and pellets having an oxyfluorinated and/or fluorinated surface and methods of making and using the thin films and pellets

Set forth herein are processes for making lithium-stuffed garnet oxides (e.g., Li.sub.7La.sub.3Zr.sub.2O.sub.12, also known as LLZO) that have passivated surfaces comprising a fluorinate and/or an oxyfluorinate species. These surfaces resist the formation of oxides, carbonates, hydroxides, peroxides, and organics that spontaneously form on LLZO surfaces under ambient conditions. Also set forth herein are new materials made by these processes.

High temperature oxidation protection for composites

Systems and methods for forming an oxidation protection system on a composite structure are provided. In various embodiments, an oxidation protection system disposed on a substrate may comprise a boron-silicon-glass layer formed directly on the composite structure. The boron-silicon-glass layer may comprise a boron compound, a silicon compound, and a glass compound.

Barrier coating resin formulations, and related methods

A barrier coating resin formulation comprising at least one polycarbosilane preceramic polymer, at least one organically modified silicon dioxide preceramic polymer, at least one filler, and at least one solvent. A barrier coating comprising a reaction product of the at least one polycarbosilane preceramic polymer and the at least one organically modified silicon dioxide preceramic polymer and the at least one filler is also disclosed, as are articles comprising the barrier coating, rocket motors comprising the barrier coating, and methods of forming the articles.