C04B41/89

Silicon bond coat with columnar grains and methods of its formation

Methods for forming a coated component, along with the resulting coated components, are provided. The method may include forming a silicon-based bond coating on a surface of a substrate and forming a barrier coating on the silicon-based bond coating. The silicon-based bond coating comprises columnar grains of crystalline silicon. Chemical vapor depositing (CVD) may be used to form the silicon-based bond coating through CVD of a silicon-containing precursor at a deposition temperature and deposition pressure that causes crystallization of the silicon material during the deposition of the silicon-based bond coating. The silicon-containing precursor may be silane, monochlorosilane, dichlorosilane, and/or trichlorosilane.

ENVIRONMENTAL BARRIER COATING FOR ENHANCED RESISTANCE TO ATTACK BY MOLTEN SILICATE DEPOSITS

An environmental barrier coating, comprising a substrate containing silicon; an environmental barrier layer applied to said substrate; said environmental barrier layer comprising a rare earth composition.

PROTECTIVE COATING SYSTEMS FOR GAS TURBINE ENGINE APPLICATIONS AND METHODS FOR FABRICATING THE SAME

A method of applying a protective coating to a substrate includes the steps of: providing a turbine engine component substrate formed of a ceramic matrix composite material, forming an environmental barrier coating layer including a rare earth disilicate material directly on the substrate, treating an outer surface of the environmental barrier coating layer to form a thermal barrier coating layer including a porous rare earth monociliate material directly on the environmental barrier coating layer. The step of treating the outer surface is performed using a thermal process consisting of the application of heat or a chemical-thermal process consisting of the application of heat and a chemical. The method further includes infiltrating at least a portion of the pores with a metal solution or suspension.

PROTECTIVE COATING SYSTEMS FOR GAS TURBINE ENGINE APPLICATIONS AND METHODS FOR FABRICATING THE SAME

A protective coating system includes a turbine engine component substrate formed of a ceramic matrix composite material, an environmental barrier coating layer including a rare earth disilicate material formed directly on the substrate, and a thermal barrier coating layer including a porous rare earth monosilicate material having a metal silicate material infiltrated within at least a portion of the pores formed directly on the environmental barrier coating layer.

ARTICLE FOR HIGH TEMPERATURE SERVICE
20230090598 · 2023-03-23 ·

An article for high temperature service is presented herein. One embodiment is an article including a substrate having a silicon-bearing ceramic matrix composite; and a layer disposed over the substrate, wherein the layer includes silicon and a dopant, the dopant including aluminum. In another embodiment, the article includes a ceramic matrix composite substrate, wherein the composite includes a silicon-bearing ceramic and a dopant, the dopant including aluminum; a bond coat disposed over the substrate, where the bond coat includes elemental silicon, a silicon alloy, a silicide, or combinations including any of the aforementioned; and a coating disposed over the bond coat, the coating including a silicate (such as an aluminosilicate or rare earth silicate), yttria-stabilized zirconia, or a combination including any of the aforementioned.

ARTICLE FOR HIGH TEMPERATURE SERVICE
20230090598 · 2023-03-23 ·

An article for high temperature service is presented herein. One embodiment is an article including a substrate having a silicon-bearing ceramic matrix composite; and a layer disposed over the substrate, wherein the layer includes silicon and a dopant, the dopant including aluminum. In another embodiment, the article includes a ceramic matrix composite substrate, wherein the composite includes a silicon-bearing ceramic and a dopant, the dopant including aluminum; a bond coat disposed over the substrate, where the bond coat includes elemental silicon, a silicon alloy, a silicide, or combinations including any of the aforementioned; and a coating disposed over the bond coat, the coating including a silicate (such as an aluminosilicate or rare earth silicate), yttria-stabilized zirconia, or a combination including any of the aforementioned.

CONTACT JOULE HEATING FOR SINTERING HIGH TEMPERATURE COATINGS
20220348513 · 2022-11-03 ·

A method for forming a high temperature coating includes forming a pre-sintered ceramic coating on a ceramic composite substrate. The pre-sintered ceramic coating includes a plurality of ceramic particles. The method further includes sintering at least a portion of the pre-sintered ceramic coating by heating the portion of the pre-sintered ceramic coating to a sintering temperature of the plurality of ceramic particles using joule heating. The sintering temperature is greater than about 1000 degrees Celsius (° C.).

CONTACT JOULE HEATING FOR SINTERING HIGH TEMPERATURE COATINGS
20220348513 · 2022-11-03 ·

A method for forming a high temperature coating includes forming a pre-sintered ceramic coating on a ceramic composite substrate. The pre-sintered ceramic coating includes a plurality of ceramic particles. The method further includes sintering at least a portion of the pre-sintered ceramic coating by heating the portion of the pre-sintered ceramic coating to a sintering temperature of the plurality of ceramic particles using joule heating. The sintering temperature is greater than about 1000 degrees Celsius (° C.).

NON-CONTACT RADIATIVE HEATING FOR SINTERING HIGH TEMPERATURE COATINGS
20220348511 · 2022-11-03 ·

A method for forming a high temperature coating includes forming a pre-sintered ceramic coating on a ceramic composite substrate. The pre-sintered ceramic coating comprises a plurality of ceramic particles. The method further includes sintering at least a portion of the pre-sintered ceramic coating by heating the portion of the pre-sintered ceramic coating to a sintering temperature of the pre-sintered ceramic coating using one or more non-contact radiative heating elements. The sintering temperature is greater than about 1000 degrees Celsius (° C.).

Antimicrobial Ceramic Tile and Manufacturing Method Thereof
20230091820 · 2023-03-23 ·

The present invention provides an antimicrobial ceramic tile and manufacturing method thereof. A manufacturing method of an antimicrobial ceramic tile comprises: grinding soils into slurries; drying the slurries into powders by hot air; pressing the powders into a green body through a molding machine; dotting or spraying or showering a glaze slurry on the surface of the green body to form an engobe; dotting the glaze slurry on the engobe to form a ground glaze; mixing a surface glaze and an antimicrobial material into an antimicrobial glaze in a weight ratio of 100:5˜10; grinding water and the antimicrobial glaze into the antimicrobial glaze in a weight ratio of 5˜6:4˜5; and dotting antimicrobial glaze on the ground glaze; finally, rapidly firing the ceramic tile and the antimicrobial glaze into an antimicrobial ceramic tile.