C04B2111/0062
Borate and silicate coating for improved acoustical panel performance and methods of making same
The disclosure provides a coating composition for improving the sag resistance of a fibrous panel, the composition including 10 to 100 wt. % inorganic binder, based on the total weight of the dry coating, wherein the inorganic binder includes a borate salt and at least one of an alkali metal silicate or an alkaline earth metal silicate, and the inorganic binder is water soluble. Further provided are fibrous panels having a backing side and an opposing facing side including the coating of the disclosure, and methods of preparing same.
Cement board with water-resistant additive
In the present disclosure, a cement board is disclosed. The cement board comprises a core having a first surface and a second surface opposite the first surface and a binder including a pozzolan material and a water-resistant additive, wherein the water-resistant additive is present in an amount of less than 5 wt. % based on the weight of the pozzolan material.
HIGH-CARBON RECOVERED PAPER AND PLASTIC MATERIALS WITH REDUCED ENDOTOXIN LEVELS
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
Cement Board with Water-Resistant Additive
In the present disclosure, a cement board is disclosed. The cement board comprises a core having a first surface and a second surface opposite the first surface and a binder including a pozzolan material and a water-resistant additive, wherein the water-resistant additive is present in an amount of less than 5 wt. % based on the weight of the pozzolan material.
High-carbon recovered paper and plastic materials with reduced endotoxin levels
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
GYPSUM BOARD FROM GYPSUM HAVING HIGH LEVEL OF CHLORIDE SALT AND A POLYMER LAYER AND METHODS ASSOCIATED THEREWITH
Gypsum boards formed from synthetic gypsum and other gypsum sources having high chloride salt concentrations. Gypsum boards may include a board core including set gypsum between a front cover sheet and a back cover sheet. A total concentration of the chloride anion in the board core ranges from about 150 to 4000 parts by weight (pbw) chloride, typically about 300 to about 3000 pbw, more typically from about 400 to about 2000 pbw, further typically from about 1000 to about 2000 pbw, and further typically from about 600 to about 1000 pbw, per 1,000,000 pbw calcium sulfate dihydrate. A polymer layer contacts an inner surface of the back cover sheet. A densified gypsum layer contacts an inner surface of the front cover sheet. Methods of making the gypsum board, and a wall system for employing the gypsum boards, are also provided.
Antimicrobial Coating for Building Panel
In general, the present invention is directed to a building panel, such as a gypsum board, comprising a core having a first side and a second side opposing the first side and at least one facing material having a coating comprising at least one fungicide, at least one polymeric binder, and at least one pigment. The panel satisfies at least one of the following: the board exhibits a rating of 2 or less when tested in accordance to ASTM G21-15 or the board exhibits a rating of at least 8 when tested in accordance to ASTM D3273-16. The panel may also exhibit at least a Level 3 finish.
HIGH-CARBON RECOVERED PAPER AND PLASTIC MATERIALS WITH REDUCED ENDOTOXIN LEVELS
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
Construction panel having improved fixing strength
A plasterboard comprises a gypsum matrix having a polymeric additive distributed therein in an amount of at least 1 wt % relative to the gypsum, the gypsum matrix further having a first group of fibres and a second group of fibres embedded therein, wherein the fibres of the first group of fibres have an average length that is at least three times the average length of the fibres of the second group of fibres.
STABILIZED GYPSUM PARTICLES
The present invention is directed to a construction chemical composition for the preparation of gypsum articles, said construction chemical composition comprising fine calcium sulfate and a dispersant being a polyarylether. Further the present invention is directed to a process for preparing said construction chemical composition as well as an article comprising said construction chemical composition.