C04B2235/32

Grain boundary enhanced UN and U3Si2 pellets with improved oxidation resistance

A method of forming a water resistant boundary on a fissile material for use in a water cooled nuclear reactor is described. The method comprises mixing a powdered fissile material selected from the group consisting of UN and U.sub.3Si.sub.2 with an additive selected from oxidation resistant materials having a melting or softening point lower than the sintering temperature of the fissile material, pressing the mixed fissile and additive materials into a pellet, sintering the pellet to a temperature greater than the melting point of the additive. Alternatively, if the melting point of the oxidation resistant particles is greater than the sintering temperature of UN or U.sub.3Si.sub.2, then the oxidation resistant particles can have a particle size distribution less than that of the UN or U.sub.3Si.sub.2.

Ceramic material comprising a pseudo-cubic phase, a process for preparing and uses of the same

The present invention relates to a bismuth-based solid solution ceramic material, as well as a process for preparing the ceramic material and uses thereof, particularly in an actuator component employed, for example, in a droplet deposition apparatus. In particular, the present invention relates to a ceramic material having a general chemical formula (I): (I): x(Bi.sub.0.5Na.sub.0.5)TiO.sub.3-y(Bi.sub.0.5K.sub.0.5)TiO.sub.3-z.sub.1SrHfO.sub.3-z.sub.2SrZrO.sub.3, wherein x+y+Z.sub.1+Z.sub.2=1; y, (z.sub.1+z.sub.2)≠0; x≥0. In embodiments, the present invention also relates to a ceramic material having a general chemical formula (II): x(Bi0.5Na0.5)TiO3-y(Bi0.5K0.5)TiO3-y(Bi0.5K0.5)TiO3-ZiSrHfO3-z2SrZrO3, wherein x+y+z−i+z2=1; x, y, fa+z2)≠0; as well as a ceramic material of general formula (III): y(Bi.sub.0.5K.sub.0.5)TiO.sub.3-z.sub.1SrHfO.sub.3-z.sub.2SrZrO.sub.3, wherein y+z.sub.1,+z.sub.2=1; y, (z.sub.1+z.sub.2)≠0.

CERAMIC SUBSTRATE AND ELECTROSTATIC CHUCK
20210246071 · 2021-08-12 ·

A ceramic substrate includes a substrate main body, and a conductor layer provided inside of the substrate main body. The substrate main body includes an insulator layer that is ceramics composed of aluminum oxide, and a composite oxide layer of aluminum and silicon, the composite oxide layer being formed between the insulator layer and the conductor layer.

MICROCHEMICAL SYSTEM APPARATUS AND RELATED METHODS OF FABRICATION
20210178387 · 2021-06-17 ·

The disclosure relates to microchemical (or microfluidic) apparatus as well as related methods for making the same. The methods generally include partial sintering of sintering powder (e.g., binderless or otherwise free-flowing sintering powder) that encloses a fugitive phase material having a shape corresponding to a desired cavity structure in the formed apparatus. Partial sintering removes the fugitive phase and produces a porous compact, which can then be machined if desired and then further fully sintered to form the final apparatus. The process can produce apparatus with small, controllable cavities shaped as desired for various microchemical or microfluidic unit operations, with a generally smooth interior cavity finish, and with materials (e.g., ceramics) able to withstand harsh environments for such unit operations.

NANO PARTICLE AGGLOMERATE REDUCTION TO PRIMARY PARTICLE
20210276926 · 2021-09-09 ·

A nanoparticle cluster reduction method yields a new composition of matter including a large percentage (e.g., 75% or higher percentage) of primary nanoparticles in the new composition of matter. The particle reduction method reduces the size of nanoparticle clusters in material of the new composition of matter, allows particle reduction of specific nanoparticle cluster sizes, and allows particle reduction to primary nanoparticles. This new composition of matter can include a high permittivity and high resistivity dielectric compound. This new composition of matter, according to certain examples, has high permittivity, high resistivity, and low leakage current. In certain examples, the new composition of matter constitutes a dielectric energy storage device that is a battery with very high energy density, high operating voltage per cell, and an extended battery life cycle. An example method can include a controlled gas evolution reaction to reduce the size of nanoparticle clusters.

A ceramic nuclear fuel pellet, a fuel rod, and a fuel assembly

A fuel assembly for a nuclear reactor, a fuel rod of the fuel assembly, and a ceramic nuclear fuel pellet of the fuel rod are disclosed. The fuel pellet includes a first fissile material of UB.sub.2, The boron of the UB.sub.2 is enriched to have a concentration of the isotope .sup.11B that is higher than for natural B.

INORGANIC MEMBRANE FILTRATION ARTICLES AND METHODS THEREOF
20210107838 · 2021-04-15 ·

An inorganic membrane filtration article and methods for making the same. The membrane filtration article includes a sintered flow-through ceramic honeycomb with a plurality of partition walls defining a plurality of open channels from an inlet end of the honeycomb to an outlet end of the honeycomb. The honeycomb is formed from a cordierite composition with low-sodium and/or low-potassium content for enhanced filtration performance.

METHOD FOR PRODUCING A CERAMIC ABSORBER, CERAMIC ABSORBER, AND USE OF SAME

A ceramic absorber for damping, in particular absorbing, vibrations, in particular combustion vibrations, preferably in gas turbines, which has a foam structure. For the ceramic absorber, the sound absorption capacity is set in a defined way and the efficiency is improved. The foam structure is based on a ceramic powder which contains either a component from the class of silicates or a component from the class of oxides, or a combination of a component from the class of silicates and a component from the class of oxides, and the foam structure has a homogeneous pore distribution.

Multilayer ceramic capacitor

A multilayer ceramic capacitor includes: a ceramic body in which dielectric layers and first and second internal electrodes are alternately stacked; and first and second external electrodes formed on an outer surface of the ceramic body and electrically connected to the first and second internal electrodes, respectively. In a microstructure of the dielectric layer, dielectric grains are divided by a dielectric grain size into sections each having an interval of 50 nm, respectively, a fraction of the dielectric grains in each of the sections within a range of 50 nm to 450 nm is within a range of 0.025 to 0.20, and a thickness of the dielectric layer is 0.8 μm or less.

Microchemical system apparatus and related methods of fabrication

The disclosure relates to microchemical (or microfluidic) apparatus as well as related methods for making the same. The methods generally include partial sintering of sintering powder (e.g., binderless or otherwise free-flowing sintering powder) that encloses a fugitive phase material having a shape corresponding to a desired cavity structure in the formed apparatus. Partial sintering removes the fugitive phase and produces a porous compact, which can then be machined if desired and then further fully sintered to form the final apparatus. The process can produce apparatus with small, controllable cavities shaped as desired for various microchemical or microfluidic unit operations, with a generally smooth interior cavity finish, and with materials (e.g., ceramics) able to withstand harsh environments for such unit operations.