C04B2235/6567
Dielectric ceramic composition and ceramic electronic component
A dielectric ceramic composition including a first component and a second component. The first component comprises an oxide of Ca of 0.00 mol % to 35.85 mol % an oxide of Sr of 0.00 mol % to 47.12 mol %, an oxide of Ba of 0.00 mol % to 51.22 mol %, an oxide of Ti of 0.00 mol % to 17.36 mol %, an oxide of Zr of 0.00 mol % to 17.36 mol %, an oxide of Sn of 0.00 mol % to 2.60 mol %, an oxide of Nb of 0.00 mol % to 35.32 mol %, an oxide of Ta of 0.00 mol % to 35.32 mol %, and an oxide of V of 0.00 mol % to 2.65 mol %. The second component includes (by mass) at least (a) an oxide of Mn of 0.005% to 3.500% and (b) one or both of an oxide of Cu of 0.080% to 20.000% and an oxide of Ru of 0.300% to 45.000%.
MEMBER FOR OPTICAL GLASS MANUFACTURING APPARATUS
Provided is a member for optical glass manufacturing apparatus. The member is used for optical glass manufacturing apparatus and exposed to a gas containing a halogen element in a high temperature environment of 1100° C. or higher. The member includes dense ceramics containing silicon nitride as a main component, and a porosity of a surface layer of the member is smaller than a porosity of the inside of the member.
SINTERED BODY WITH HIGH IMPACT RESISTANCE
To provide a sintered body with improved impact resistance due to impact absorption through plastic deformation before brittle fracture for an impact exceeding the fracture resistance of the sintered body, and/or a method for producing the sintered body.
A sintered body including: zirconia containing a stabilizer; and a region in which an impact mark is formed when an impact force is applied.
CUTTING TOOL
A cutting tool (1) formed of a silicon nitride-based sintered body (2) including a matrix phase (3), a hard phase (4), and a grain boundary phase (10) in which a glass phase (11) and a crystal phase (12) exist. The sintered body (2) contains yttrium in an amount of 5.0 wt % to 15.0 wt % in terms of an oxide, and contains titanium nitride as the hard phase (4) in an amount of 5.0 wt % to 25.0 wt %. In an X-ray diffraction peak, a halo pattern appears at 2θ ranging from 25° to 35° in an internal region of the sintered body (2). A ratio B/A of a maximum peak intensity B to a maximum peak intensity A satisfies 0.11≤B/A≤0.40 . . . Expression (1) in a surface region of the sintered body (2), and satisfies 0.00≤B/A≤0.10 . . . Expression (2) in the internal region of the sintered body (2).
CUBIC BORON NITRIDE SINTERED MATERIAL AND METHOD OF PRODUCING SAME
A cubic boron nitride sintered material includes: 0 to 85 volume % of cubic boron nitride grains; and a binder phase, wherein the binder phase includes at least one selected from a group consisting of one or more first compounds and a solid solution originated from the first compounds, the cubic boron nitride grains include, on number basis, more than or equal to 50% of cubic boron nitride grains each having an equivalent circle diameter of more than 0.5 μm, and includes, on number basis, less than or equal to 50% of cubic boron nitride grains each having an equivalent circle diameter of more than 2 μm, and when a mass of the cubic boron nitride grains is assumed as 100 mass %, a total content of lithium, magnesium, calcium, strontium, beryllium, and barium in the cubic boron nitride grains is less than 0.001 mass %.
CUBIC BORON NITRIDE SINTERED MATERIAL AND METHOD OF PRODUCING SAME
A cubic boron nitride sintered material includes: to 98 volume % of cubic boron nitride grains; and a binder phase, wherein the binder phase includes at least one selected from a group consisting of one or more first compounds and a solid solution originated from the first compounds, the cubic boron nitride grains include, on number basis, more than or equal to 50% of cubic boron nitride grains each having an equivalent circle diameter of more than 0.5 μm, and includes, on number basis, less than or equal to 50% of cubic boron nitride grains each having an equivalent circle diameter of more than 2 μm, and when a mass of the cubic boron nitride grains is assumed as 100 mass %, a total content of lithium, magnesium, calcium, strontium, beryllium, and barium in the cubic boron nitride grains is less than 0.001 mass %.
LITHIUM-ION-CONDUCTIVE OXIDE SINTERED BODY AND USE THEREOF
The present invention aims to provide a lithium-ion-conducting oxide sintered body capable of providing a solid electrolyte with an excellent ion conductivity, and a solid electrolyte, an electrode and an all-solid-state battery using the same. The lithium-ion-conducting oxide sintered body including at least lithium, tantalum, phosphorus, silicon, and oxygen as constituent elements, and having a polycrystalline structure consisting of crystal grains and grain interfaces formed between the crystal grains.
CERMET AND/OR CERAMIC MULTI-COLOURED ARTICLE AND METHOD FOR MANUFACTURING SAME
A cermet and/or ceramic multi-coloured article, and in particular a bezel (1) of a timepiece, produced by a method for compressing at least two materials (2, 3) of distinct colours, the article including a relief decoration (8) of a different colour from the rest of the article, the decoration (8) being produced by laser ablation on one of the materials (3) after compression of the two materials (2, 3).
Filamentous organism-derived carbon-based materials, and methods of making and using same
The invention provides filamentous organism-derived carbonaceous materials doped with organic and/or inorganic compounds, and methods of making the same. In certain embodiments, these carbonaceous materials are used as electrodes in solid state batteries and/or lithium-ion batteries. In another aspect, these carbonaceous materials are used as a catalyst, catalyst support, adsorbent, filter and/or other carbon-based material or adsorbent. In yet another aspect, the invention provides battery devices incorporating the carbonaceous electrode materials.
METAL-Si BASED POWDER, METHOD FOR PRODUCING SAME, METAL-Si BASED SINTERED BODY, SPUTTERING TARGET, AND METAL-Si BASED THIN FILM MANUFACTURING METHOD
A metal-Si based powder contains a metal-Si based particle including a plurality of crystal phase grains. The crystal phase grains include a crystal phase containing a compound of a metal and Si. The crystal phase grains have an average grain size of, for example, 20 μm or less. The metal-Si based particle has an average particle size of, for example, 5 to 100 μm.