Patent classifications
C04B2237/122
HIGH OPTICAL POWER LIGHT CONVERSION DEVICE USING A PHOSPHOR ELEMENT WITH SOLDER ATTACHMENT
A light generator comprises a light conversion device and a light source arranged to apply a light beam to the light conversion element. The light conversion device includes an optoceramic or other solid phosphor element comprising one or more phosphors embedded in a ceramic, glass, or other host, a metal heat sink, and a solder bond attaching the optoceramic phosphor element to the metal heat sink. The optoceramic phosphor element does not undergo cracking in response to the light source applying a light beam of beam energy effective to heat the optoceramic phosphor element to the phosphor quenching point.
METHOD FOR MANUFACTURING CIRCUIT BOARD INCLUDING METAL-CONTAINING LAYER
Provided is a method for manufacturing a circuit board including: (a) preparing a mixture of a metal powder, an anti-sintering agent, and an activator; (b) immersing a dielectric substrate in the mixture; (c) forming a metal-containing layer on the surface of the dielectric substrate by heating the mixture under an inert atmosphere or under a reducing atmosphere; (d) forming a first metal layer on the metal-containing layer by electroless plating and forming a second metal layer thereon by electroplating; and (e) forming a metal pattern on the dielectric substrate, wherein the first metal layer includes Cu, Ni, Co, Au, Pd, or an alloy thereof, the second metal layer includes Cu, Ni, Fe, Co, Cr, Zn, Au, Ag, Pt, Pd, Rh, or an alloy thereof, and the method further includes performing heat treatment at least once after step (c).
Contact and Method for Making the Same
The present application discloses a contact, which comprises a contact opening, and a Ti layer, a glue layer and a tungsten layer which completely fill the contact opening; the Ti layer is subjected to annealing treatment; the tungsten layer comprises a tungsten seed layer and a tungsten body layer; the glue layer consists of a TiN layer which is divided into a plurality of TiN sub-layers, all or part of the TiN sub-layers are subjected to the annealing treatment, and the size of grains of the TiN sub-layer subjected to the annealing treatment is limited by the thickness of the corresponding TiN sub-layer. The present application further discloses a method for making a contact. The present application can prevent the annealing treatment of the TiSi layer from producing large lattice grains in the glue layer, thus can make the tungsten seed layer be a continuous structure.
Method for manufacturing circuit board including metal-containing layer
Provided is a method for manufacturing a circuit board including: (a) preparing a mixture of a metal powder, an anti-sintering agent, and an activator; (b) immersing a dielectric substrate in the mixture; (c) forming a metal-containing layer on the surface of the dielectric substrate by heating the mixture under an inert atmosphere or under a reducing atmosphere; (d) forming a first metal layer on the metal-containing layer by electroless plating and forming a second metal layer thereon by electroplating; and (e) forming a metal pattern on the dielectric substrate, wherein the first metal layer includes Cu, Ni, Co, Au, Pd, or an alloy thereof, the second metal layer includes Cu, Ni, Fe, Co, Cr, Zn, Au, Ag, Pt, Pd, Rh, or an alloy thereof, and the method further includes performing heat treatment at least once after step (c).
BONDED SUBSTRATE AND MANUFACTURING METHOD OF BONDED SUBSTRATE
A second main surface of the copper plate is opposite a first main surface of the copper plate, and is bonded to a silicon nitride ceramic substrate by the bonding layer. A first portion and a second portion of an end surface of the copper plate form an angle of 135° to 165° on an outside of the copper plate. An extended plane of the first portion and the second main surface form an angle of 110° to 145° a side where the second portion is located. A distance from the second main surface to an intersection of the first portion and the second portion in a direction of a thickness of the copper plate is 10 to 100 μm. The second main surface extends beyond the extended plane of the first portion by a distance of 10 μm or more.
Semiconductor substrate support with multiple electrodes and method for making same
A method for manufacturing an electrostatic chuck with multiple chucking electrodes made of ceramic pieces using metallic aluminum as the joining. The aluminum may be placed between two pieces and the assembly may be heated in the range of 770 C to 1200 C. The joining atmosphere may be non-oxygenated. After joining the exclusions in the electrode pattern may be machined by also machining through one of the plate layers. The machined exclusion slots may then be filled with epoxy or other material. An electrostatic chuck or other structure manufactured according to such methods.
ELECTROCHEMICAL ENERGY STORAGE DEVICES
Provided herein are energy storage devices. In some cases, the energy storage devices are capable of being transported on a vehicle and storing a large amount of energy. An energy storage device is provided comprising at least one liquid metal electrode, an energy storage capacity of at least about 1 MWh and a response time less than or equal to about 100 milliseconds (ms).
SEMICONDUCTOR PROCESSING EQUIPMENT WITH HIGH TEMPERATURE RESISTANT NICKEL ALLOY JOINTS AND METHODS FOR MAKING SAME
A method for the joining of ceramic pieces includes applying a layer of titanium on a first ceramic piece and applying a layer of titanium on a second ceramic piece; applying a layer of nickel on each of the layers of titanium on the first ceramic piece and the second ceramic piece; applying a layer of nickel phosphorous to each of the layers of nickel on the first ceramic piece and the second ceramic piece; assembling the first ceramic piece and the second ceramic piece with the layers of titanium, nickel, and nickel phosphorous therebetween; pressing the layer of nickel phosphorous of the first ceramic piece against the layer of nickel phosphorous of the second ceramic piece; heating the first ceramic piece and the second ceramic piece to a joining temperature in a vacuum; and cooling the first ceramic piece and the second ceramic piece. A hermetic seal is formed between the first ceramic piece and the second ceramic piece.
MULTI-LAYER CERAMIC PLATE DEVICE
An electrostatic chuck includes a ceramic top plate layer made of a beryllium oxide material, a ceramic bottom plate layer made of a beryllium oxide material, a ceramic middle plate layer disposed between the ceramic top plate layer and the ceramic bottom plate layer, an electrode layer disposed between the ceramic top plate layer and the ceramic middle plate layer, and a heater layer disposed between the ceramic middle plate layer and the ceramic bottom plate layer. The electrode layer joins and hermetically seals the ceramic top plate layer to the ceramic middle plate layer, and the heater layer joins and hermetically seals the ceramic middle plate layer to the ceramic bottom plate layer.
CERAMIC MATERIALS AND SEALS FOR HIGH TEMPERATURE REACTIVE MATERIAL DEVICES
The disclosure provides seals for devices that operate at elevated temperatures and have reactive metal vapors, such as lithium, sodium or magnesium. In some examples, such devices include energy storage devices that may be used within an electrical power grid or as part of a standalone system. The energy storage devices may be charged from an electricity production source for later discharge, such as when there is a demand for electrical energy consumption.