C04B2237/38

CERAMIC MATRIX COMPOSITE ARTICLES

A method for forming a ceramic matrix composite article includes laying up a first group of plies; laying up a second group of plies, the first and second groups of plies being adjacent to each other; compacting the first group of plies and the second group of plies in the same processing step; and performing a first infiltration process on the first group of plies. The method also includes performing a second infiltration process on the second group of plies, the first infiltration process being one of a melt infiltration process or a chemical vapor infiltration process, and the second infiltration process being the other of the melt infiltration process or the chemical vapor infiltration process.

METHODS FOR REPAIRING COMPOSITE CYLINDERS

Methods for repairing composite cylindrical components are provided. One exemplary method for repairing a cylindrical component defining an axial direction, a radial direction, and a circumferential direction includes removing a damaged region of the cylindrical component. A flange extending from a cylindrical body of the cylindrical component is included in the damaged region. One or more arc segments that extend along the circumferential direction are connected with the existing cylindrical component. At least one of the arc segments includes a prefabricated flange. One or more plies are laid up to connect the arc segments with the existing cylindrical component to repair the damaged region of the cylindrical body and the prefabricated flange formed integrally with one of the arc segments replaces the damaged portion of the flange. Repaired cylindrical components are also provided.

Forming a ceramic matrix composite having a silicide layer

A ceramic matrix composite component and methods of making are described herein. The ceramic matrix composite may include a silicon containing matrix and refractory fibers embedded within the silicon containing matrix. The ceramic matrix composite component may further include a silicide layer sandwiched between the silicon containing matrix and the refractory fibers. A method of forming a ceramic matrix composite may include infiltrating a fluid that includes a refractory metal element containing compound into a fiber preform that includes fibers. The method may further include depositing the refractory metal element from the refractory metal element containing compound onto the fibers and forming, from the refractory metal element deposited onto the fibers, a refractory metal silicide.

Carbon fiber tube with increased rigidity and decreased weight
10232581 · 2019-03-19 ·

A carbon fiber tube preferably includes first, second and third carbon fiber sheets. The first carbon fiber sheet includes a cross weave pattern of fibers, which cross each other at substantially 90 degrees. One axis of the fibers of the first carbon fiber sheet is aligned to form a lengthwise axis of the carbon fiber tube. The second carbon fiber sheet includes the same cross weave pattern as the first carbon fiber sheet. One axis of the fibers of the second carbon fiber sheet is turned 45 degrees relative to the lengthwise axis. The third carbon fiber sheet includes the same cross weave pattern as the first carbon fiber sheet. One axis of the fibers of the third carbon fiber sheet is aligned with the lengthwise axis of the carbon fiber tube. The first, second and third carbon fiber sheets are baked in an autoclave.

Compliant interlayer

A brake component is disclosed. In various embodiments, the brake component includes a ceramic matrix composite (CMC) structure including a plurality of nominally dense plies, interleaved with a plurality of interlayers, wherein the plurality of nominally dense plies and the plurality of interlayers are bonded by at least one of a Field Assisted Sintering Technique (FAST), a Spark Plasma Sintering (SPS) process, or a localized heating process. In various embodiments, the brake component is a rotor disk or a stator disk.

CERAMIC MATRIX COMPOSITE COMPONENT AND METHOD OF PRODUCING THE SAME

A ceramic matrix composite component includes a first substrate and a second substrate each formed of a silicide-containing ceramic matrix composite, silicon carbide layers respectively coating a bonding surface of the first substrate and a bonding surface of the second substrate, and a bonding layer formed of a silicon-containing alloy and provided between the silicon carbide layer coating the bonding surface of the first substrate and the silicon carbide layer coating the bonding surface of the second substrate.

ARTICLES FOR CREATING HOLLOW STRUCTURES IN CERAMIC MATRIX COMPOSITES
20190071363 · 2019-03-07 ·

The present disclosure relates to a method of fabricating a ceramic composite components. The method may include providing at least a first layer of reinforcing fiber material which may be a pre-impregnated fiber. An additively manufactured component may be provided on or near the first layer. A second layer of reinforcing fiber, which may be a pre-impregnated fiber may be formed on top the additively manufactured component. A precursor is densified to consolidates at least the first and second layer into a densified composite, wherein the additively manufactured material defines at least one cooling passage in the densified composite component.

HEAT-PERMEABLE TUBE CONTAINING COMPOSITE FIBER CERAMIC
20190062224 · 2019-02-28 · ·

The present invention relates to a heat-permeable tube which has a double-walled construction. The material of the interior wall contains fiber composite ceramic. The material of the exterior wall contains metal. The present invention further relates to the use of this tube in a rotary tube furnace and the use of the rotary tube furnace for thermal treatment of materials. Furthermore, the invention relates to the use of a single-walled tube containing fiber composite ceramic as rotary tube.

FLOW PATH ASSEMBLIES FOR GAS TURBINE ENGINES AND ASSEMBLY METHODS THEREFORE

Flow path assemblies and methods for forming such flow path assemblies for gas turbine engines are provided. For example, a method for assembling an airfoil with a boundary structure to form a flow path assembly is provided. The method includes machining an opening into the boundary structure. The opening is sized to receive an airfoil or other component. The method also includes machining a cutout into the boundary structure proximate the opening. A locking feature is inserted into the cutout. When the airfoil is inserted into the opening, the locking feature interlocks the airfoil with the boundary structure. To seal the airfoil with the boundary structure, the airfoil is pressed against or into the boundary structure. When the airfoil is pressed, the locking feature is compressed such that a seal is formed between the airfoil and the boundary structure to seal the flow path assembly.

Method for joining silicon carbide components to one another

A method for fabricating assemblies that includes providing a first component that further includes silicon carbide and that has an upper portion and a tapered lower portion; providing a second component that further includes silicon carbide and that has an upper portion that is adapted to receive the tapered lower portion of the first component; providing a predetermined amount of multiphase AlSi braze foil; grinding the AlSi braze foil into a powder; mixing a predetermined amount of braze paste binder with the AlSi powder to form a slurry; uniformly applying the slurry to the tapered lower portion of the first component; uniformly applying the slurry to the upper portion of the second component and inserting the tapered lower portion of the first component into the upper portion of the second component; and heating the applied slurry to a temperature of 725 C. to 1450 C. for a predetermined period of time.