C07C1/322

Butadiene sequestration via sulfur dioxide charged zeolite beds

In an example, a method of butadiene sequestration includes receiving an input stream that includes butadiene. The method includes directing the input stream to a first sulfur dioxide charged zeolite bed for butadiene sequestration via a first chemical reaction of butadiene and sulfur dioxide to form sulfolene.

System and method for low-cost methane upgrading to added-valuable products

The present disclosure is generally directed to a new and innovative system, process and method that utilize a new non-oxygen type of oxidizers process for methane (CH.sub.4) upgrading to value-added products such as olefins and aromatics (i.e., benzene, toluene and xylene (BTX)) etc. and further removing toxic impurities such as sulphur-containing compounds (i.e. H.sub.2S) by using the sulphur as a source of radical.

Process for conversion of methane to higher hydrocarbons, including liquid fuels

Aspects of the invention are associated with the discovery of processes for converting methane (CH.sub.4), present in a methane-containing feedstock that may be obtained from a variety of sources such as natural gas, to higher hydrocarbons (e.g., C.sub.4.sup.+ hydrocarbons) such as gasoline, diesel fuel, or jet fuel boiling-range hydrocarbons, which may optionally be separated (e.g., by fractionation) for use as transportation fuels, or otherwise as blending components for such fuels. Particular aspects of the invention are associated with advantages arising from maintaining reaction conditions that improve the yield of C.sub.4.sup.+ hydrocarbons. Further aspects relate to the advantages gained by integration of the appropriate reactions to carry out the methane conversion, with downstream separation to recover and recycle desirable components of the reaction effluent, thereby improving process economics to the extent needed for commercial viability.

BUTADIENE SEQUESTRATION VIA SULFUR DIOXIDE CHARGED ZEOLITE BEDS
20180093221 · 2018-04-05 ·

In an example, a method of butadiene sequestration includes receiving an input stream that includes butadiene. The method includes directing the input stream to a first sulfur dioxide charged zeolite bed for butadiene sequestration via a first chemical reaction of butadiene and sulfur dioxide to form sulfolene.

BUTADIENE SEQUESTRATION VIA SULFUR DIOXIDE CHARGED ZEOLITE BEDS
20180093221 · 2018-04-05 ·

In an example, a method of butadiene sequestration includes receiving an input stream that includes butadiene. The method includes directing the input stream to a first sulfur dioxide charged zeolite bed for butadiene sequestration via a first chemical reaction of butadiene and sulfur dioxide to form sulfolene.

Phosphorous Modified Molecular Sieves, Their Use in Conversion of Organics to Olefins

The present invention is a phosphorous modified zeolite (A) made by a process comprising in that order: selecting a zeolite with low Si/Al ratio (advantageously lower than 30) among H.sup.+ or NH.sub.4.sup.+-form of MFI, MEL, FER, MOR, clinoptilolite, said zeolite having been made preferably without direct addition of organic template; steaming at a temperature ranging from 400 to 870 C. for 0.01-200h; leaching with an aqueous acid solution containing the source of P at conditions effective to remove a substantial part of Al from the zeolite and to introduce at least 0.3 wt % of P; separation of the solid from the liquid; an optional washing step or an optional drying step or an optional drying step followed by a washing step; a calcination step.

The present invention also relates to a process (hereunder referred as XTO process) for making an olefin product from an oxygen-containing, halogenide-containing or sulphur-containing organic feedstock wherein said oxygen-containing, halogenide-containing or sulphur-containing organic feedstock is contacted with the above catalyst (in the XTO reactor) under conditions effective to convert at least a portion of the oxygen-containing, halogenide-containing or sulphur-containing organic feedstock to olefin products (the XTO reactor effluent).

The present invention also relates to a process (hereunder referred as combined XTO and OCP process) to make light olefins from an oxygen-containing, halogenide-containing or sulphur-containing organic feedstock comprising: contacting said oxygen-containing, halogenide-containing or sulphur-containing organic feedstock in the XTO reactor with the above catalyst at conditions effective to convert at least a portion of the feedstock to form an XTO reactor effluent comprising light olefins and a heavy hydrocarbon fraction; separating said light olefins from said heavy hydrocarbon fraction; contacting said heavy hydrocarbon fraction in the OCP reactor at conditions effective to convert at least a portion of said heavy hydrocarbon fraction to light olefins.

Phosphorous Modified Molecular Sieves, Their Use in Conversion of Organics to Olefins

The present invention is a phosphorous modified zeolite (A) made by a process comprising in that order: selecting a zeolite with low Si/Al ratio (advantageously lower than 30) among H.sup.+ or NH.sub.4.sup.+-form of MFI, MEL, FER, MOR, clinoptilolite, said zeolite having been made preferably without direct addition of organic template; steaming at a temperature ranging from 400 to 870 C. for 0.01-200h; leaching with an aqueous acid solution containing the source of P at conditions effective to remove a substantial part of Al from the zeolite and to introduce at least 0.3 wt % of P; separation of the solid from the liquid; an optional washing step or an optional drying step or an optional drying step followed by a washing step; a calcination step.

The present invention also relates to a process (hereunder referred as XTO process) for making an olefin product from an oxygen-containing, halogenide-containing or sulphur-containing organic feedstock wherein said oxygen-containing, halogenide-containing or sulphur-containing organic feedstock is contacted with the above catalyst (in the XTO reactor) under conditions effective to convert at least a portion of the oxygen-containing, halogenide-containing or sulphur-containing organic feedstock to olefin products (the XTO reactor effluent).

The present invention also relates to a process (hereunder referred as combined XTO and OCP process) to make light olefins from an oxygen-containing, halogenide-containing or sulphur-containing organic feedstock comprising: contacting said oxygen-containing, halogenide-containing or sulphur-containing organic feedstock in the XTO reactor with the above catalyst at conditions effective to convert at least a portion of the feedstock to form an XTO reactor effluent comprising light olefins and a heavy hydrocarbon fraction; separating said light olefins from said heavy hydrocarbon fraction; contacting said heavy hydrocarbon fraction in the OCP reactor at conditions effective to convert at least a portion of said heavy hydrocarbon fraction to light olefins.

Butadiene sequestration via sulfur dioxide charged zeolite beds

In an example, a method of butadiene sequestration includes receiving an input stream that includes butadiene. The method includes directing the input stream to a first sulfur dioxide charged zeolite bed for butadiene sequestration via a first chemical reaction of butadiene and sulfur dioxide to form sulfolene.

Butadiene sequestration via sulfur dioxide charged zeolite beds

In an example, a method of butadiene sequestration includes receiving an input stream that includes butadiene. The method includes directing the input stream to a first sulfur dioxide charged zeolite bed for butadiene sequestration via a first chemical reaction of butadiene and sulfur dioxide to form sulfolene.

Material ITQ-55, method for preparation and use

This invention refers to a microporous crystalline material of zeolitic nature that has, in its calcined state and in the absence of defects in its crystalline matrix manifested by the presence of silanols, the empirical formula
x(M.sub.1/nXO.sub.2):yYO.sub.2:gGeO.sub.2:(1-g)SiO2 in which M is selected between H.sup.+, at least one inorganic cation of charge +n, and a mixture of both, X is at least one chemical element of oxidation state +3, Y is at least one chemical element with oxidation state +4 different from Si, x takes a value between 0 and 0.2, both included, y takes a value between 0 and 0.1, both included, g takes a value between 0 and 0.5, both included that has been denoted ITQ-55, a method for its preparation and its use.