C08F290/067

RESIN COMPOSITION AND DISPLAY UNIT
20230004040 · 2023-01-05 · ·

A display unit that includes an image display part and a light-transmitting protective part arranged on the image display part. A cured resin layer is arranged between the display part and the protective part. The cured resin layer can have a transmittance of 90% or higher in the visible range and a storage modulus at 25° C. of 1×10.sup.7 Pa or less. The cured resin layer can be formed from a resin composition that has a cure shrinkage of 5% or less.

METHODS OF PRODUCING THREE-DIMENSIONAL OBJECTS WITH APPARATUS HAVING FEED CHANNELS

A method of forming a three-dimensional object is carried out by: (a) providing a carrier and an optically transparent member having a build surface, the carrier and the build surface defining a build region therebetween; (b) filling the build region with a polymerizable liquid, the polymerizable liquid including a mixture of (i) a light polymerizable liquid first component, and (ii) a second solidifiable component that is different from the first component; (c) irradiating the build region with light through the optically transparent member to form a solid polymer scaffold from the first component and also advancing the carrier away from the build surface to form a three-dimensional intermediate having the same shape as, or a shape to be imparted to, the three-dimensional object, and containing the second solidifiable component carried in the scaffold in unsolidified and/or uncured form; and (d) concurrently with or subsequent to the irradiating step, solidifying and/or curing the second solidifiable component in the three-dimensional intermediate to form the three-dimensional object.

METHODS OF PRODUCING THREE-DIMENSIONAL OBJECTS WITH APPARATUS HAVING FEED CHANNELS

A method of forming a three-dimensional object is carried out by: (a) providing a carrier and an optically transparent member having a build surface, the carrier and the build surface defining a build region therebetween; (b) filling the build region with a polymerizable liquid, the polymerizable liquid including a mixture of (i) a light polymerizable liquid first component, and (ii) a second solidifiable component that is different from the first component; (c) irradiating the build region with light through the optically transparent member to form a solid polymer scaffold from the first component and also advancing the carrier away from the build surface to form a three-dimensional intermediate having the same shape as, or a shape to be imparted to, the three-dimensional object, and containing the second solidifiable component carried in the scaffold in unsolidified and/or uncured form; and (d) concurrently with or subsequent to the irradiating step, solidifying and/or curing the second solidifiable component in the three-dimensional intermediate to form the three-dimensional object.

TRIAZINE RING-CONTAINING POLYMER AND FILM FORMING COMPOSITION CONTAINING SAME
20230002555 · 2023-01-05 · ·

For example, a triazine ring-containing polymer containing a repeating unit structure represented by Formula (24) below,

##STR00001## wherein R.sup.102 represents a crosslinking group.

TRIAZINE RING-CONTAINING POLYMER AND FILM FORMING COMPOSITION CONTAINING SAME
20230002555 · 2023-01-05 · ·

For example, a triazine ring-containing polymer containing a repeating unit structure represented by Formula (24) below,

##STR00001## wherein R.sup.102 represents a crosslinking group.

Inhibition of crystallization in polyurethane resins
11713367 · 2023-08-01 · ·

A resin composition useful for additive manufacturing is provided, which resin composition may exhibit improved shelf life through inhibition of crystallization. Such resin composition may include a crystallization inhibitor as taught herein, and/or a prepolymer produced by reaction of an isocyanate with multiple isomers and comprising a lower percentage of the structurally symmetric isomer. Methods of forming a three-dimensional object using such resin composition are also provided.

A METHOD FOR IMPROVING THE FLAME, SMOKE AND/OR TOXICITY RETARDANCY IN POLYISOCYANURATE / POLYURETHANE (PIR/PUR) COMPRISING MATERIALS

A polyisocyanurate and/or polyurethane (PIR/PUR) comprising material having improved Flame, Smoke and/or Toxicity (FST) retardancy is disclosed and a method for forming said PIR/PUR comprising material. The PIR/PUR material is comprising at least 0.2 wt % of compounds having a number average equivalent weight <160 g/mol and at least one non-polymerized ethylenically unsaturated moiety based on the total weight of the PIR/PUR comprising material, and optionally 0.01 wt % up to 1 wt % of one or more radical initiator compounds based on the total weight of the PIR/PUR comprising material.

A METHOD FOR IMPROVING THE FLAME, SMOKE AND/OR TOXICITY RETARDANCY IN POLYISOCYANURATE / POLYURETHANE (PIR/PUR) COMPRISING MATERIALS

A polyisocyanurate and/or polyurethane (PIR/PUR) comprising material having improved Flame, Smoke and/or Toxicity (FST) retardancy is disclosed and a method for forming said PIR/PUR comprising material. The PIR/PUR material is comprising at least 0.2 wt % of compounds having a number average equivalent weight <160 g/mol and at least one non-polymerized ethylenically unsaturated moiety based on the total weight of the PIR/PUR comprising material, and optionally 0.01 wt % up to 1 wt % of one or more radical initiator compounds based on the total weight of the PIR/PUR comprising material.

Optical film

The present invention provides a method for producing an optical film excellent in anti-fouling properties and scratch resistance as well as anti-reflection properties. The method includes the steps of: (1) applying a lower layer resin and an upper layer resin; (2) forming a resin layer having the uneven structure on a surface thereof by pressing a mold against the lower layer resin and the upper layer resin from the upper layer resin side in the state where the applied lower layer resin and upper layer resin are stacked; and (3) curing the resin layer, the lower layer resin containing at least one kind of first monomer that contains no fluorine atoms, the upper layer resin containing a fluorine-containing monomer and at least one kind of second monomer that contains no fluorine atoms, at least one of the first monomer and the second monomer containing a compatible monomer that is compatible with the fluorine-containing monomer and being dissolved in the lower layer resin and the upper layer resin.

Optical film

The present invention provides a method for producing an optical film excellent in anti-fouling properties and scratch resistance as well as anti-reflection properties. The method includes the steps of: (1) applying a lower layer resin and an upper layer resin; (2) forming a resin layer having the uneven structure on a surface thereof by pressing a mold against the lower layer resin and the upper layer resin from the upper layer resin side in the state where the applied lower layer resin and upper layer resin are stacked; and (3) curing the resin layer, the lower layer resin containing at least one kind of first monomer that contains no fluorine atoms, the upper layer resin containing a fluorine-containing monomer and at least one kind of second monomer that contains no fluorine atoms, at least one of the first monomer and the second monomer containing a compatible monomer that is compatible with the fluorine-containing monomer and being dissolved in the lower layer resin and the upper layer resin.