C08L2666/06

Starch nanocomposite materials

In one aspect, the invention provides a substantially exfoliated nanocomposite material including starch and hydrophobically modified layered silicate clay. In another aspect, the invention provides packaging made from material including the substantially exfoliated nanocomposite material described above. The nanocomposite material has improved mechanical and rheological properties and reduced sensitivity to moisture in that the rates of moisture update and/or loss are reduced. In another aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material described above, including a step of mixing the starch in the form of an aqueous gel with the hydrophobic clay in a melt mixing device. In a further aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material, including the steps of mixing the starch with the hydrophobic clay to form a masterbatch (hereinafter “the masterbatch process”) and mixing the masterbatch with further starch.

Starch nanocomposite materials

In one aspect, the invention provides a substantially exfoliated nanocomposite material including starch and hydrophobically modified layered silicate clay. In another aspect, the invention provides packaging made from material including the substantially exfoliated nanocomposite material described above. The nanocomposite material has improved mechanical and rheological properties and reduced sensitivity to moisture in that the rates of moisture update and/or loss are reduced. In another aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material described above, including a step of mixing the starch in the form of an aqueous gel with the hydrophobic clay in a melt mixing device. In a further aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material, including the steps of mixing the starch with the hydrophobic clay to form a masterbatch (hereinafter “the masterbatch process”) and mixing the masterbatch with further starch.

METHOD OF MAKING A MICROPOROUS MATERIAL

A method for producing a microporous material comprising the steps of: providing an ultrahigh molecular weight polyethylene (UHMWPE); providing a filler; providing a processing plasticizer; adding the filler to the UHMWPE in a mixture being in the range of from about 1:9 to about 15:1 filler to UHMWPE by weight; adding the processing plasticizer to the mixture; extruding the mixture to form a sheet from the mixture; calendering the sheet; extracting the processing plasticizer from the sheet to produce a matrix comprising UHMWPE and the filler distributed throughout the matrix; stretching the microporous material in at least one direction to a stretch ratio of at least about 1.5 to produce a stretched microporous matrix; and subsequently calendering the stretched microporous matrix to produce a microporous material which exhibits improved physical and dimensional stability properties over the stretched microporous matrix.

METHOD OF MAKING A MICROPOROUS MATERIAL

A method for producing a microporous material comprising the steps of: providing an ultrahigh molecular weight polyethylene (UHMWPE); providing a filler; providing a processing plasticizer; adding the filler to the UHMWPE in a mixture being in the range of from about 1:9 to about 15:1 filler to UHMWPE by weight; adding the processing plasticizer to the mixture; extruding the mixture to form a sheet from the mixture; calendering the sheet; extracting the processing plasticizer from the sheet to produce a matrix comprising UHMWPE and the filler distributed throughout the matrix; stretching the microporous material in at least one direction to a stretch ratio of at least about 1.5 to produce a stretched microporous matrix; and subsequently calendering the stretched microporous matrix to produce a microporous material which exhibits improved physical and dimensional stability properties over the stretched microporous matrix.

COMPOSITE FOR MANUFACTURING BARRIER LAYER, BARRIER LAYER, METHOD FOR MANUFACTURING BARRIER LAYER, AND PACKAGING MATERIAL

A composite for manufacturing a barrier layer, a barrier layer, a method for manufacturing the barrier layer, and a packaging material are provided. Based on the total mass of the composite as 100 parts by mass, the composite includes the following components by mass: Polyhydroxyalkanoate, 70 to 96 parts by mass; polylactic acid, 1 to 15 parts by mass; modified layered silicate, 1 to 5 parts by mass; polyalkylene carbonate, 1 to 20 parts by mass; and auxiliary agent, 1.3 to 12 parts by mass.

High-density polyethylene compositions, method of making the same, injection molded articles made therefrom, and method of making such articles

A high-density polyethylene composition that is formulated for being injection molded into an injection-molded bottle cap closure comprising a skirt that axially extends from the periphery of a base, and internal screw threads for securing the cap to a container, and method of producing the same.

High-density polyethylene compositions, method of making the same, injection molded articles made therefrom, and method of making such articles

A high-density polyethylene composition that is formulated for being injection molded into an injection-molded bottle cap closure comprising a skirt that axially extends from the periphery of a base, and internal screw threads for securing the cap to a container, and method of producing the same.

Starch Nanocomposite Materials

In one aspect, the invention provides a substantially exfoliated nanocomposite material including starch and hydrophobically modified layered silicate clay. In another aspect, the invention provides packaging made from material including the substantially exfoliated nanocomposite material described above. The nanocomposite material has improved mechanical and rheological properties and reduced sensitivity to moisture in that the rates of moisture update and/or loss are reduced. In another aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material described above, including a step of mixing the starch in the form of an aqueous gel with the hydrophobic clay in a melt mixing device. In a further aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material, including the steps of mixing the starch with the hydrophobic clay to form a masterbatch (hereinafter “the masterbatch process”) and mixing the masterbatch with further starch.

Starch Nanocomposite Materials

In one aspect, the invention provides a substantially exfoliated nanocomposite material including starch and hydrophobically modified layered silicate clay. In another aspect, the invention provides packaging made from material including the substantially exfoliated nanocomposite material described above. The nanocomposite material has improved mechanical and rheological properties and reduced sensitivity to moisture in that the rates of moisture update and/or loss are reduced. In another aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material described above, including a step of mixing the starch in the form of an aqueous gel with the hydrophobic clay in a melt mixing device. In a further aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material, including the steps of mixing the starch with the hydrophobic clay to form a masterbatch (hereinafter “the masterbatch process”) and mixing the masterbatch with further starch.

Starch nanocomposite materials

In one aspect, the invention provides a substantially exfoliated nanocomposite material including starch and hydrophobically modified layered silicate clay. In another aspect, the invention provides packaging made from material including the substantially exfoliated nanocomposite material described above. The nanocomposite material has improved mechanical and rheological properties and reduced sensitivity to moisture in that the rates of moisture update and/or loss are reduced. In another aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material described above, including a step of mixing the starch in the form of an aqueous gel with the hydrophobic clay in a melt mixing device. In a further aspect, the invention provides a process for preparing the substantially exfoliated nanocomposite material, including the steps of mixing the starch with the hydrophobic clay to form a masterbatch (hereinafter “the masterbatch process”) and mixing the masterbatch with further starch.