C09D5/084

COATING COMPOSITIONS FOR APPLICATION UTILIZING A HIGH TRANSFER EFFICIENCY APPLICATOR AND METHODS AND SYSTEMS THEREOF

A system for applying a coating composition is provided herein. The system includes a first high transfer efficiency applicator defining a first nozzle orifice and a second high transfer efficiency applicator defining a second nozzle orifice. The system further includes a reservoir. The system further includes a substrate defining a first target area and a second target area. The first high transfer efficiency applicator and the second high transfer efficiency applicator are configured to receive the coating composition from the reservoir and configured to expel the coating composition through the first nozzle orifice to the first target area of the substrate and to expel the coating composition through the second nozzle orifice to the second target area of the substrate.

COATING COMPOSITIONS FOR APPLICATION UTILIZING A HIGH TRANSFER EFFICIENCY APPLICATOR AND METHODS AND SYSTEMS THEREOF

A coating composition for application to a substrate utilizing a high transfer efficiency applicator. The coating composition includes a carrier, a binder, a corrosion inhibiting pigment. The coating composition has an Ohnesorge number (Oh) of from about 0.01 to about 12.6. The coating composition has a Reynolds number (Re) of from about 0.02 to about 6,200. The coating composition has a Deborah number (De) of from greater than 0 to about 1730.

COATING COMPOSITIONS FOR APPLICATION UTILIZING A HIGH TRANSFER EFFICIENCY APPLICATOR AND METHODS AND SYSTEMS THEREOF

A coating composition for application to a substrate utilizing a high transfer efficiency applicator is provided herein. The coating composition includes a carrier, a binder, and a radar reflective pigment or a LiDAR reflective pigment. The coating composition has an Ohnesorge number (Oh) of from about 0.01 to about 12.6. The coating composition has a Reynolds number (Re) of from about 0.02 to about 6,200. The coating composition has a Deborah number (De) of from greater than 0 to about 1730.

METHODS AND COMPOSITIONS FOR INHIBITING CORROSION ON METAL SURFACES

Methods and compositions for inhibiting corrosion of a metal product are provided. The metal product can be contacted with water that includes at least one carbonate and/or bicarbonate salt, or otherwise has components that increase the alkalinity of the water. In addition, or as an alternative, the water can include a stannous corrosion inhibitor. The water can be evaporated off of a surface of the metal product to provide a residual of the salt on the surface and/or a protective stannous film on the surface.

Electrically-conductive corrosion-protective covering

A corrosion-protected electrical assembly includes a metallic component (e.g. a utility pole or a guy anchor rod or direct buried tower steel) having an outer surface, and a water-impermeable, electrically-conductive, covering applied to at least a portion of the outer surface. A covering for a metallic component includes a water-impermeable polymeric matrix, and a particulate carbonaceous material dispersed in the polymeric matrix. A method for protecting a metallic component from corrosion includes applying a covering to an outer surface of the metallic component at the bottom portion of the metallic component. The covering is water-impermeable and electrically-conductive.

ANODE COATING COMPOSITIONS AND USES THEREOF
20210261791 · 2021-08-26 ·

The present document describes an aqueous coating composition for preventing or reducing air oxidation of a carbon material, and aqueous priming coating composition for application to a carbon material prior to application of the aqueous coating composition, chemical treatment of a carbon material comprising both the aqueous coating composition and aqueous priming coating composition, and methods of coating carbon material with the compositions.

FAST COATING COMPOSITIONS
20210283652 · 2021-09-16 ·

An anticorrosive coating includes a first curable liquid layer to the associated substrate, the first layer having a thickness of at least about 100 micrometers, wherein the first layer includes at least one polymer or at least one monomer, quasi-one-dimensional particles or quasi-two-dimensional particles, sacrificial metal particles, and a solvent, wherein a percolation threshold of the particles is not reached in the presence of the solvent, wherein the percolation threshold of the particles is reached when between about 1% and about 20% of the solvent evaporates, applying a second curable liquid layer having a thickness of at least 100 micrometers on the top of the first layer after the percolation threshold of the particles is reached and viscosity of the first layer increases more than 50%, and allowing the first layer and the second layer to cure simultaneously.

FAST COATING COMPOSITIONS
20210283653 · 2021-09-16 ·

An anticorrosive coating includes a first curable liquid layer to the associated substrate, the first layer having a thickness of at least about 100 micrometers, wherein the first layer includes at least one polymer or at least one monomer, quasi-one-dimensional particles or quasi-two-dimensional particles, sacrificial metal particles, and a solvent, wherein a percolation threshold of the particles is not reached in the presence of the solvent, wherein the percolation threshold of the particles is reached when between about 1% and about 20% of the solvent evaporates, applying a second curable liquid layer having a thickness of at least 100 micrometers on the top of the first layer after the percolation threshold of the particles is reached and viscosity of the first layer increases more than 50%, and allowing the first layer and the second layer to cure simultaneously.

FAST COATING COMPOSITIONS
20210283654 · 2021-09-16 ·

An anticorrosive coating includes a first curable liquid layer to the associated substrate, the first layer having a thickness of at least about 100 micrometers, wherein the first layer includes at least one polymer or at least one monomer, quasi-one-dimensional particles or quasi-two-dimensional particles, sacrificial metal particles, and a solvent, wherein a percolation threshold of the particles is not reached in the presence of the solvent, wherein the percolation threshold of the particles is reached when between about 1% and about 20% of the solvent evaporates, applying a second curable liquid layer having a thickness of at least 100 micrometers on the top of the first layer after the percolation threshold of the particles is reached and viscosity of the first layer increases more than 50%, and allowing the first layer and the second layer to cure simultaneously.

Development of a sol-gel anticorrosion treatment

The invention relates to a process for treating a metal alloy part, characterized in that it comprises the following steps: —producing a stock formulation by mixing, in equal molar parts of silicon, an alcoholic solution of hydrolysed epoxysilane and an alcoholic solution of hydrolysed aminosilane, —mixing the stock formulation with a suspension comprising conductive nanowires in an amount by weight of between 0.1% and 10% relative to the total weight of the stock formulation in order to obtain a dilute formulation, and —depositing the dilute formulation on the part in order to obtain the coating.