C09D123/06

ETHYLENE-BASED POLYMER COMPOSITIONS FOR IMPROVED EXTRUSION COATINGS

The invention provides a composition comprising at least the following: a) a first composition comprising at least one first ethylene-based polymer, formed by high pressure, free-radical polymerization, and wherein the first composition comprises the following properties: a melt index (I2) from 1.0 to 15.0 g/10 min, and density from 0.910 to 0.940 g/cc; b) a second composition comprising at least one second ethylene-based polymer, and wherein the second composition comprises the following properties; a melt index (I2) from 1.0 to 1000 g/10 min, a density greater than 0.940 g/cc; wherein the composition comprises the following properties: melt index (I2) from 2.0 to 20.0 g/10 min, and a density from 0.915 to 0.940 g/cc; and wherein the first composition is present in an amount from 65 to 95 wt %, based on the weight of the composition.

ETHYLENE-BASED POLYMER COMPOSITIONS FOR IMPROVED EXTRUSION COATINGS

The invention provides a composition comprising at least the following: a) a first composition comprising at least one first ethylene-based polymer, formed by high pressure, free-radical polymerization, and wherein the first composition comprises the following properties: a melt index (I2) from 1.0 to 15.0 g/10 min, and density from 0.910 to 0.940 g/cc; b) a second composition comprising at least one second ethylene-based polymer, and wherein the second composition comprises the following properties; a melt index (I2) from 1.0 to 1000 g/10 min, a density greater than 0.940 g/cc; wherein the composition comprises the following properties: melt index (I2) from 2.0 to 20.0 g/10 min, and a density from 0.915 to 0.940 g/cc; and wherein the first composition is present in an amount from 65 to 95 wt %, based on the weight of the composition.

ETHYLENE-BASED POLYMER COMPOSITIONS FOR IMPROVED EXTRUSION COATINGS

The invention provides a composition comprising at least the following: a) a first composition comprising at least one first ethylene-based polymer, formed by high pressure, free-radical polymerization, and wherein the first composition comprises the following properties: a melt index (I2) from 1.0 to 15.0 g/10 min, and density from 0.910 to 0.940 g/cc; b) a second composition comprising at least one second ethylene-based polymer, and wherein the second composition comprises the following properties; a melt index (I2) from 1.0 to 1000 g/10 min, a density greater than 0.940 g/cc; wherein the composition comprises the following properties: melt index (I2) from 2.0 to 20.0 g/10 min, and a density from 0.915 to 0.940 g/cc; and wherein the first composition is present in an amount from 65 to 95 wt %, based on the weight of the composition.

Light stabilizers

The present invention relates to symmetric diesters of hydroxyalkyl-4-hydroxy-tetraalkylpiperidine compounds and their use as light stabilizers. They are compatible with and soluble in coating formulations of different polarity.

Light stabilizers

The present invention relates to symmetric diesters of hydroxyalkyl-4-hydroxy-tetraalkylpiperidine compounds and their use as light stabilizers. They are compatible with and soluble in coating formulations of different polarity.

Modified ethylene-based polymer compositions and methods of their production

Polymeric compositions comprising an ethylene-based thermoplastic polymer and an olefinic thermoplastic elastomer. Processes for producing polymeric compositions comprising an ethylene-based thermoplastic polymer and an olefinic thermoplastic elastomer. Such polymeric compositions can be employed in forming coated wires and cables.

Modified ethylene-based polymer compositions and methods of their production

Polymeric compositions comprising an ethylene-based thermoplastic polymer and an olefinic thermoplastic elastomer. Processes for producing polymeric compositions comprising an ethylene-based thermoplastic polymer and an olefinic thermoplastic elastomer. Such polymeric compositions can be employed in forming coated wires and cables.

Modified ethylene-based polymer compositions and methods of their production

Polymeric compositions comprising an ethylene-based thermoplastic polymer and an olefinic thermoplastic elastomer. Processes for producing polymeric compositions comprising an ethylene-based thermoplastic polymer and an olefinic thermoplastic elastomer. Such polymeric compositions can be employed in forming coated wires and cables.

Polyethylene composition for having high impact and stress cracking resistance

Polyethylene composition with improved balance of impact resistance at low temperatures and Environmental Stress Cracking Resistance (ESCR), particularly suited for producing protective coatings on metal pipes, said composition having the following features: 1) density from 0.938 to 0.948 g/cm.sup.3; 2) ratio MIF/MIP from 15 to 25; 3) MIF from 30 to 45 g/10 min.; 4) Mz equal to or greater than 1000000 g/mol; 5) LCBI equal to or greater than 0.55.

Polyethylene composition for having high impact and stress cracking resistance

Polyethylene composition with improved balance of impact resistance at low temperatures and Environmental Stress Cracking Resistance (ESCR), particularly suited for producing protective coatings on metal pipes, said composition having the following features: 1) density from 0.938 to 0.948 g/cm.sup.3; 2) ratio MIF/MIP from 15 to 25; 3) MIF from 30 to 45 g/10 min.; 4) Mz equal to or greater than 1000000 g/mol; 5) LCBI equal to or greater than 0.55.