Patent classifications
C09J123/12
ADHESIVE COMPOSITION AND ADHESION METHOD
An object of the present invention is to provide an adhesive composition having an excellent adhesive force even in the presence of hot water in an assembly in which at least one of two or more members to be bonded to each other via the adhesive composition is a low-polarity metal member, and an adhesion method. The present invention relates to an adhesive composition and an adhesion method for bonding a metal member. The adhesive composition contains a polyolefin (A) component having an acidic group and/or an acid anhydride group and having an acid value of 0.01 mgKOH/g to 6.5 mgKOH/g. The metal member has a ratio of a dipole term in surface free energy of 0.01% to 5.0%.
ADHESIVE COMPOSITION AND ADHESION METHOD
An object of the present invention is to provide an adhesive composition having an excellent adhesive force even in the presence of hot water in an assembly in which at least one of two or more members to be bonded to each other via the adhesive composition is a low-polarity metal member, and an adhesion method. The present invention relates to an adhesive composition and an adhesion method for bonding a metal member. The adhesive composition contains a polyolefin (A) component having an acidic group and/or an acid anhydride group and having an acid value of 0.01 mgKOH/g to 6.5 mgKOH/g. The metal member has a ratio of a dipole term in surface free energy of 0.01% to 5.0%.
HIGH-FREQUENCY DIELECTRIC HEATING ADHESIVE SHEET
A high-frequency-dielectric-heating-adhesive-sheet includes: a first adhesive layer containing a first thermoplastic resin; a second adhesive layer containing a second thermoplastic resin; and an intermediate layer, a ratio DPM/DP1 of dielectric property DPM of the intermediate layer to dielectric property DP1 of the first adhesive layer and a ratio DPM/DP2 of the dielectric property DPM of the intermediate layer to dielectric property DP2 of the second adhesive layer are each less than one, and the dielectric property DP1, the dielectric property DP2, and the dielectric property DPM are values of dielectric property (tanδ/ε’r) of the first adhesive layer, the second adhesive layer, and the intermediate layer, respectively. tanδ denotes a dielectric dissipation factor at 23° C. and a frequency of 40.68 MHz and ε‘r denotes a relative permittivity at 23° C. and the frequency of 40.68 MHz.
HIGH-FREQUENCY DIELECTRIC HEATING ADHESIVE SHEET
A high-frequency-dielectric-heating-adhesive-sheet includes: a first adhesive layer containing a first thermoplastic resin; a second adhesive layer containing a second thermoplastic resin; and an intermediate layer, a ratio DPM/DP1 of dielectric property DPM of the intermediate layer to dielectric property DP1 of the first adhesive layer and a ratio DPM/DP2 of the dielectric property DPM of the intermediate layer to dielectric property DP2 of the second adhesive layer are each less than one, and the dielectric property DP1, the dielectric property DP2, and the dielectric property DPM are values of dielectric property (tanδ/ε’r) of the first adhesive layer, the second adhesive layer, and the intermediate layer, respectively. tanδ denotes a dielectric dissipation factor at 23° C. and a frequency of 40.68 MHz and ε‘r denotes a relative permittivity at 23° C. and the frequency of 40.68 MHz.
Antacids for polymers
The present invention provides polymer compositions having improved corrosivity, color stability and clarity. Also disclosed is a process of preparing the polymers. The process may comprise incorporating into the polymer an acid neutralizing amount of an amorphous aluminum silicate. The amorphous aluminum silicate may be present in the polymer in an amount such that the polymer composition having a Corrosivity Index of less than 6. A refractive index of the amorphous aluminum silicate may be the same or substantially the same as a refractive index of the polymer.
Antacids for polymers
The present invention provides polymer compositions having improved corrosivity, color stability and clarity. Also disclosed is a process of preparing the polymers. The process may comprise incorporating into the polymer an acid neutralizing amount of an amorphous aluminum silicate. The amorphous aluminum silicate may be present in the polymer in an amount such that the polymer composition having a Corrosivity Index of less than 6. A refractive index of the amorphous aluminum silicate may be the same or substantially the same as a refractive index of the polymer.
Adhesives containing post-consumer polymer, adhesive additives containing post-consumer polymer and methods of making the same
Adhesive and additive for adhesive made from post-consumer polypropylene.
Adhesives containing post-consumer polymer, adhesive additives containing post-consumer polymer and methods of making the same
Adhesive and additive for adhesive made from post-consumer polypropylene.
HOT-MELT ADHESIVE FOR WOODWORKING
Provided is a hot-melt adhesive for woodworking, containing a component (a) of an olefinic polymer (A) having a specific tensile modulus of elasticity and a specific glass transition temperature (Tg), and a component (b) of an olefinic polymer (B) having a specific glass transition temperature (Tg), wherein the content of the component (a) is 31 to 95% by mass relative to 100% by mass of the total amount of the component (a) and the component (b).
HOT-MELT ADHESIVE FOR WOODWORKING
Provided is a hot-melt adhesive for woodworking, containing a component (a) of an olefinic polymer (A) having a specific tensile modulus of elasticity and a specific glass transition temperature (Tg), and a component (b) of an olefinic polymer (B) having a specific glass transition temperature (Tg), wherein the content of the component (a) is 31 to 95% by mass relative to 100% by mass of the total amount of the component (a) and the component (b).