C22B23/0461
METHOD FOR INHIBITING EXTRACTANT DEGRADATION OF DSX PROCESS THROUGH METAL EXTRACTION CONTROL
Provided is a method for inhibiting extractant degradation in the DSX process through the metal extraction control, the method comprising steps of: (a) adding limestone to a copper solvent extraction-raffinate to precipitate iron (Fe) and aluminum (Al) as a slurry, recovering a clarifying liquid; and (b) adding sulfuric acid to the recovered clarifying liquid to adjust the pH thereof.
RECOVERY OF METALS FROM LITHIUM-ION BATTERIES
The present disclosure provides methods and systems for recovering metals from lithium-ion batteries, and specifically to methods and systems for recovering cobalt and nickel jointly in metallic form via electrowinning processes. The present disclosure further provides methods and systems for preparing lithium-ion battery materials for use in metal recovery processes.
Processing method for lithium ion battery scrap
A method for processing lithium ion battery scrap according to this invention includes a leaching step of leaching lithium ion battery scrap to obtain a leached solution; an aluminum removal step of neutralizing the leached solution to a pH range of from 4.0 to 6.0, then performing solid-liquid separation and removing aluminum in the leached solution to obtain a first separated solution; and an iron removal step of adding an oxidizing agent to the first separated solution and adjusting the pH in a range of from 3.0 to 5.0, then performing solid-liquid separation and removing iron in the first separated solution to obtain a second separated solution.
System and method for parallel solution extraction of one or more metal values from metal-bearing materials
A process and system is provided for recovery of one or more metal values using solution extraction techniques and for metal value recovery. In an exemplary embodiment, the solution extraction system comprises a first solution extraction circuit and a second solution extraction circuit. A first metal-bearing solution is provided to the first and second circuit, and a second metal-bearing solution is provided to the first circuit. The first circuit produces a first rich electrolyte solution, which can be forwarded to primary metal value recovery, and a low-grade raffinate, which is forwarded to secondary metal value recovery. The second circuit produces a second rich electrolyte solution, which is also forwarded to primary metal value recovery. The first and second solution extraction circuits have independent organic phases and each circuit can operate independently of the other circuit.
METHOD FOR RECOVERING VALUABLE METAL SULFIDES
Provided is a method for recovering a valuable metal sulfide, the method including: (a) adding limestone to a residual solution including a valuable metal to remove iron and aluminum; (b) adding sulfuric acid and a sulfide to the solution from which the iron and aluminum are removed to recover the valuable metal sulfide; and (c) adding air or sulfuric acid to the solution from which the valuable metal sulfide is recovered to remove sulfur.
METHOD FOR SEPARATING COPPER, NICKEL, AND COBALT
Provided is a method for separating copper, nickel, and cobalt, the method being capable of efficiently and selectively separating copper, nickel, and cobalt from alloys containing copper, nickel, and cobalt, such as highly corrosive alloys containing copper, nickel, and cobalt obtained by dry-processing used lithium ion batteries. The alloy containing copper, nickel, and cobalt is brought into contact with nitric acid in the co-presence of a sulfiding agent to obtain a solid containing copper and a leachate containing nickel and cobalt.
METHOD FOR SEPARATING COPPER FROM NICKEL AND COBALT
Provided is a method for separating copper from nickel and cobalt with which it is possible to selectively and efficiently separate copper, as well as nickel and cobalt, from an alloy including copper, nickel, and cobalt such as an alloy having high corrosion resistance that includes copper, nickel, and cobalt obtained by dry treatment of waste lithium ion cells. An alloy including copper, nickel, and cobalt is brought into contact with sulfuric acid in the joint presence of a sulfurizing agent, and a solid containing copper and a leachate containing nickel and cobalt are obtained.
Methods for controlling iron via magnetite formation in hydrometallurgical processes
A method of controlling iron in a hydrometallurgical process is disclosed. The method may comprise the steps of: leaching (14, 114) a feed slurry (2, 102); forming a pregnant leach solution (12a, 12b; 112a, 112b); removing a first leach residue (18, 118) from the pregnant leach solution (12a, 12b); and sending a portion (12b, 112b) of the pregnant leach solution (12a, 12b) and/or raffinate (22, 122) produced therefrom, to an iron removal process (34, 134). According to some preferred embodiments, the iron removal process (34, 134) may comprise the steps of: sequentially processing the pregnant leach solution (12a, 12b) and/or raffinate (22, 122) produced therefrom in a first reactor (R.sub.1) a second reactor (R.sub.2), and a third reactor (R.sub.3); maintaining a pH level of the first reactor (R.sub.1) above 4, by virtue of the addition of a first base; maintaining a pH level of the second (R.sub.2) and/or third (R.sub.3) reactors above 8.5, by virtue of a second base; and forming solids (46) comprising magnetite (68). The method may further comprise the steps of performing a solid liquid separation step (36) after the iron removal process (34, 134); and performing a magnetic separation step (64) to remove magnetite (68) from said solids comprising magnetite (68), without limitation. A system for performing the method is also disclosed.
Systems and methods for improved metal recovery using ammonia leaching
Systems and methods for basic leaching are provided. In various embodiments, a method is provided comprising leaching a slurry comprising a copper bearing material and an ammonia leach medium, adding copper powder to the slurry, separating the slurry into a pregnant leach solution and solids, and performing a solvent extraction on the pregnant leach solution to produce an loaded aqueous stream.
Method of ore processing using mixture including acidic leach solution and oxidizing agent
A method of selectively leaching a metal such as nickel from an ore or ore processing intermediate comprising the metal and cobalt. The ore or ore processing intermediate is contacted with an acidic leach solution comprising an amount of an oxidising agent sufficient to oxidise a major portion of the cobalt to thereby cause it to be stabilised in the solid phase while a major portion of the metal is dissolved for subsequent recovery.