C23C4/11

DOPED NICKEL OXIDE TARGET AND PREPARATION METHOD AND APPLICATION THEREOF
20230235448 · 2023-07-27 ·

A doped nickel oxide target includes a nickel oxide substrate and a dopant doped therein. The dopant includes at least one compound that contains one or more elements of Cu, Ca, Cr, Sn, Hg, Pb, Mg, Mn, Ag, Co, and Pr.

DOPED NICKEL OXIDE TARGET AND PREPARATION METHOD AND APPLICATION THEREOF
20230235448 · 2023-07-27 ·

A doped nickel oxide target includes a nickel oxide substrate and a dopant doped therein. The dopant includes at least one compound that contains one or more elements of Cu, Ca, Cr, Sn, Hg, Pb, Mg, Mn, Ag, Co, and Pr.

Calcium-magnesium-alumino-silicate resistant thermal barrier coatings

A method for forming a coating system on a component includes depositing a reactive layer with predetermined CMAS reaction kinetics on at least a portion of a thermal barrier coating. The method also includes activating the reactive layer with a scanning laser. A component, such as a gas turbine engine component, includes a substrate, a thermal barrier coating and a reactive layer. The thermal barrier coating is deposited on at least a portion of the substrate. The reactive layer is deposited on at least a portion of the thermal barrier coating. The reactive layer has predetermined CMAS reaction kinetics activated by laser scanning.

Calcium-magnesium-alumino-silicate resistant thermal barrier coatings

A method for forming a coating system on a component includes depositing a reactive layer with predetermined CMAS reaction kinetics on at least a portion of a thermal barrier coating. The method also includes activating the reactive layer with a scanning laser. A component, such as a gas turbine engine component, includes a substrate, a thermal barrier coating and a reactive layer. The thermal barrier coating is deposited on at least a portion of the substrate. The reactive layer is deposited on at least a portion of the thermal barrier coating. The reactive layer has predetermined CMAS reaction kinetics activated by laser scanning.

COATED PIPE RESISTANT TO CASING WEAR

A steel tubular pipe, which is threaded, sleeved, or integral, includes at least one first male threaded end, an inner surface, and a metal deposition layer on the inner surface and of thickness between 0.01 mm and 0.8 mm deposited on all or part of the inner surface of the pipe.

Creating 3D mark on protective coating on metal part using mask and metal part so formed

A method for creating a three-dimensional (3D) mark in a protective coating including at least one of a TBC and a bond coating over a metal part, is provided. The method may include positioning a mask over the protective coating, the mask including an opening pattern therein; and performing an abrasive waterjet process on the protective coating using the mask. The abrasive waterjet erodes a first portion of the protective coating exposed through the first opening pattern to create the 3D mark. The mask is removed, leaving the 3D mark in the protective coating. The 3D mark only partially penetrates through the protective coating. A metal part may include a metal body, a protective coating over the metal body, and the 3D mark in the protective coating, is also provided. The 3D mark in the protective coating may include an opening having a width of between 30 and 300 micrometers.

Connecting material for solid oxide fuel cell, manufacturing method thereof, and solid oxide fuel cell comprising same

The present specification relates to a connecting material for a solid oxide fuel cell, comprising a conductive substrate; and a ceramic protective film provided on one surface of the conductive substrate, in which the ceramic protective film comprises an oxide represented by Formula 1, a manufacturing method thereof, and a solid oxide fuel cell comprising the same.

Connecting material for solid oxide fuel cell, manufacturing method thereof, and solid oxide fuel cell comprising same

The present specification relates to a connecting material for a solid oxide fuel cell, comprising a conductive substrate; and a ceramic protective film provided on one surface of the conductive substrate, in which the ceramic protective film comprises an oxide represented by Formula 1, a manufacturing method thereof, and a solid oxide fuel cell comprising the same.

SLOTTED CERAMIC COATING WITH A REACTIVE PHASE COATING DISPOSED THEREON FOR IMPROVED CMAS RESISTANCE AND METHODS OF FORMING THE SAME

A coated component including a slotted ceramic coating with a reactive phase coating disposed thereon for improved resistance to environmental contaminant compositions, along with methods of its formation, is provided. The coated component may include a substrate defining a surface, a ceramic coating disposed on the surface of the substrate, and a reactive phase coating disposed on the layer of environmental contaminant compositions. The ceramic coating includes a plurality of slots disposed in the ceramic coating forming segments of ceramic coating material.

SLOTTED CERAMIC COATING WITH A REACTIVE PHASE COATING DISPOSED THEREON FOR IMPROVED CMAS RESISTANCE AND METHODS OF FORMING THE SAME

A coated component including a slotted ceramic coating with a reactive phase coating disposed thereon for improved resistance to environmental contaminant compositions, along with methods of its formation, is provided. The coated component may include a substrate defining a surface, a ceramic coating disposed on the surface of the substrate, and a reactive phase coating disposed on the layer of environmental contaminant compositions. The ceramic coating includes a plurality of slots disposed in the ceramic coating forming segments of ceramic coating material.