Patent classifications
C04B14/106
Use of a clay in the preparation of a geopolymer precursor
A method for the use of a clay including: less than 30% of kaolinite; and at least 20% of muscovite and/or illite; from 1% to 20% of smectite; the muscovite and/or illite/kaolinite weight ratio being greater than 1; for the preparation of a geopolymer precursor.
ARTICLE MADE OF CONGLOMERATE MATERIAL AND METHOD FOR MANUFACTURING SUCH ARTICLE
Article made of conglomerate material in the form of a slab comprising an aggregate which includes granules of expanded material having a selected particle size range and defining between them inter-granular cavities containing only air and no filling material. The aggregate also includes a binder present in a controlled minimum quantity sufficient for lining the granules of expanded material. The article also comprises a lining layer integral with the aggregate. The invention also relates to a method for the production of an article made of conglomerate material.
ARTICLE MADE OF CONGLOMERATE MATERIAL AND METHOD FOR MANUFACTURING SUCH ARTICLE
Article made of conglomerate material in the form of a slab comprising an aggregate which includes granules of expanded material having a selected particle size range and defining between them inter-granular cavities containing only air and no filling material. The aggregate also includes a binder present in a controlled minimum quantity sufficient for lining the granules of expanded material. The article also comprises a lining layer integral with the aggregate. The invention also relates to a method for the production of an article made of conglomerate material.
Compositions and methods for providing increased strength in ceiling, flooring, and building products
A composition for addition to a ceiling tile, flooring product, or other construction product may include microfibrillated cellulose and optionally an inorganic particulate material. The ceiling tile, flooring product, or other construction product may further include perlite, mineral wool, wood pulp, starch and other additives, where the wood pulp and other inorganic particulate materials are bonded to the microfibrillated cellulose. Methods of manufacturing the compound are also disclosed.
Compositions and methods for providing increased strength in ceiling, flooring, and building products
A composition for addition to a ceiling tile, flooring product, or other construction product may include microfibrillated cellulose and optionally an inorganic particulate material. The ceiling tile, flooring product, or other construction product may further include perlite, mineral wool, wood pulp, starch and other additives, where the wood pulp and other inorganic particulate materials are bonded to the microfibrillated cellulose. Methods of manufacturing the compound are also disclosed.
Preventing or reducing plant growth by biocementation
The present invention primarily relates to the use of a mixture capable of biocementation as a means of preventing or reducing plant growth, preferably weed growth. The invention also relates to a method for preventing or reducing plant growth, preferably weed growth, on/in a substrate.
Preventing or reducing plant growth by biocementation
The present invention primarily relates to the use of a mixture capable of biocementation as a means of preventing or reducing plant growth, preferably weed growth. The invention also relates to a method for preventing or reducing plant growth, preferably weed growth, on/in a substrate.
Geopolymer cement compositions and methods of use
Methods of cementing include providing a geopolymer cement composition that includes a monophase amorphous hydraulic binder material (MAHBM), a metal silicate, an alkaline activator, and a carrier fluid, introducing the geopolymer cement composition into a subterranean formation, and allowing the geopolymer cement composition to set in the subterranean formation. The MAHBM includes silica or alumina core particulates coated with an amorphous calcium silicate hydrate.
ADMIXTURE COMPOSITION FOR THE PRODUCTION OF LIGHTWEIGHT CONCRETE CONTAINING POLYSTYRENE BEADS, PROCESS FOR THE PREPARATION OF THE COMPOSITION AND ITS APPLICATION
The present invention relates to an admixture composition for the production of lightweight concretes containing polystyrene beads, which comprises a mixture of organic and inorganic substances which consists of the reaction products of polyurethane resin, tetraethyl orthosilicate, a glycol compound, an aromatic vinyl compound containing an unsaturated double bond, preferably styrene, and an inorganic silicate compound and preferably comprises the following components: glycol copolymer type compounds, in an amount of 15-10 w/w %, glycol polymer-silica type compounds, in an amount of 45-50 w/w %, polyurethane-based resin, in an amount of 13-22 w/w % polystyrene in an amount of 2-3% w/w %, and foam glass beads in an amount of 25-15 w/w %, and a) for the production of a liquid product, based on the total mass of the above composition, organic solvents in an amount of 15-20 w/w %, and water in an amount of 10-5 w/w %; or b) for the production of a solid preparation, based on the total mass of the above composition, polyvinyl acetate or polyvinyl alcohol in an amount of 10-5 w/w %; aluminium hydroxide in an amount of 2-5 w/w %, and calcined limestone powder in an amount of 8-10 w/w %. The invention also relates to the production and use of the above admixture composition.
ADMIXTURE COMPOSITION FOR THE PRODUCTION OF LIGHTWEIGHT CONCRETE CONTAINING POLYSTYRENE BEADS, PROCESS FOR THE PREPARATION OF THE COMPOSITION AND ITS APPLICATION
The present invention relates to an admixture composition for the production of lightweight concretes containing polystyrene beads, which comprises a mixture of organic and inorganic substances which consists of the reaction products of polyurethane resin, tetraethyl orthosilicate, a glycol compound, an aromatic vinyl compound containing an unsaturated double bond, preferably styrene, and an inorganic silicate compound and preferably comprises the following components: glycol copolymer type compounds, in an amount of 15-10 w/w %, glycol polymer-silica type compounds, in an amount of 45-50 w/w %, polyurethane-based resin, in an amount of 13-22 w/w % polystyrene in an amount of 2-3% w/w %, and foam glass beads in an amount of 25-15 w/w %, and a) for the production of a liquid product, based on the total mass of the above composition, organic solvents in an amount of 15-20 w/w %, and water in an amount of 10-5 w/w %; or b) for the production of a solid preparation, based on the total mass of the above composition, polyvinyl acetate or polyvinyl alcohol in an amount of 10-5 w/w %; aluminium hydroxide in an amount of 2-5 w/w %, and calcined limestone powder in an amount of 8-10 w/w %. The invention also relates to the production and use of the above admixture composition.