Patent classifications
C04B18/142
SOLID WASTE LARGE-MIXING-AMOUNT CONCRETE PREFABRICATED LAMINATED SLAB AND PREPARATION METHOD THEREOF
The present disclosure relates to the technical field of solid waste recycling and fabricated buildings, and provides a solid waste large-mixing-amount concrete prefabricated laminated slab and a preparation method thereof. The solid waste large-mixing-amount concrete prefabricated laminated slab provided by the present disclosure comprises a prefabricated layer and a laminated layer. Transverse grooves and longitudinal grooves are formed in the surface of the prefabricated layer. During application, the grooves can be used for erecting pipelines, the contact area of the prefabricated layer and the laminated layer can also be increased, the combined effect of new concrete and old concrete is improved, the integrity of a floor slab is enhanced, and the effect of improving the overall stress capacity of the floor slab is achieved.
SOLID WASTE LARGE-MIXING-AMOUNT CONCRETE PREFABRICATED LAMINATED SLAB AND PREPARATION METHOD THEREOF
The present disclosure relates to the technical field of solid waste recycling and fabricated buildings, and provides a solid waste large-mixing-amount concrete prefabricated laminated slab and a preparation method thereof. The solid waste large-mixing-amount concrete prefabricated laminated slab provided by the present disclosure comprises a prefabricated layer and a laminated layer. Transverse grooves and longitudinal grooves are formed in the surface of the prefabricated layer. During application, the grooves can be used for erecting pipelines, the contact area of the prefabricated layer and the laminated layer can also be increased, the combined effect of new concrete and old concrete is improved, the integrity of a floor slab is enhanced, and the effect of improving the overall stress capacity of the floor slab is achieved.
Soil stabilization material based on solid waste and bioenzyme, and preparation method thereof
A soil solidification material based on solid waste and bioenzyme, and a preparation method thereof are disclosed. The soil solidification material is composed of the following components in parts by weight: recycled aggregate 22-35 parts, steel slag 20-30 parts, high-calcium fly ash 16-24 parts, the bioenzyme 5-15 parts, an inorganic adsorbent 10-18 parts, an organic adsorbent 8-20 parts, industrial waste gypsum 25-35 parts, an activator 20-30 parts, sodium citrate 1-3 parts, and slaked lime 0.02-0.2 parts. The present disclosure adopts the recycled aggregate, the steel slag, the industrial waste gypsum and the high-calcium fly ash as the main components of the soil solidification material to reduce the cost. The soil solidification material of the present disclosure prepared by optimizing the proportion is capable of significantly improving the engineering properties of the soil or the mixed contaminated soil, and has significant economic and environmental benefits.
Soil stabilization material based on solid waste and bioenzyme, and preparation method thereof
A soil solidification material based on solid waste and bioenzyme, and a preparation method thereof are disclosed. The soil solidification material is composed of the following components in parts by weight: recycled aggregate 22-35 parts, steel slag 20-30 parts, high-calcium fly ash 16-24 parts, the bioenzyme 5-15 parts, an inorganic adsorbent 10-18 parts, an organic adsorbent 8-20 parts, industrial waste gypsum 25-35 parts, an activator 20-30 parts, sodium citrate 1-3 parts, and slaked lime 0.02-0.2 parts. The present disclosure adopts the recycled aggregate, the steel slag, the industrial waste gypsum and the high-calcium fly ash as the main components of the soil solidification material to reduce the cost. The soil solidification material of the present disclosure prepared by optimizing the proportion is capable of significantly improving the engineering properties of the soil or the mixed contaminated soil, and has significant economic and environmental benefits.
METHOD FOR MAKING CARBONATED PRECAST CONCRETE PRODUCTS WITH ENHANCED DURABILITY
A method for making a carbonated precast concrete product includes: obtaining a mixture including at least one binder material, an aggregate, and water; molding the mixture into a molded intermediate; demolding the molded intermediate to obtain a demolded intermediate, the demolded intermediate having a first water-to-binder ratio; conditioning the demolded intermediate to provide a conditioned article having a second water-to-binder ratio less than the first water-to-binder ratio of the demolded intermediate; moisturizing at least one surface of the conditioned article with an aqueous medium, thereby causing a weight gain of the conditioned article and providing a moisturized product, a first portion of the moisturized product having a third water-to-binder ratio greater than a fourth water-to-binder ratio of a remainder of the moisturized product; and curing the moisturized product with carbon dioxide to obtain the carbonated precast concrete product.
METHOD FOR MAKING CARBONATED PRECAST CONCRETE PRODUCTS WITH ENHANCED DURABILITY
A method for making a carbonated precast concrete product includes: obtaining a mixture including at least one binder material, an aggregate, and water; molding the mixture into a molded intermediate; demolding the molded intermediate to obtain a demolded intermediate, the demolded intermediate having a first water-to-binder ratio; conditioning the demolded intermediate to provide a conditioned article having a second water-to-binder ratio less than the first water-to-binder ratio of the demolded intermediate; moisturizing at least one surface of the conditioned article with an aqueous medium, thereby causing a weight gain of the conditioned article and providing a moisturized product, a first portion of the moisturized product having a third water-to-binder ratio greater than a fourth water-to-binder ratio of a remainder of the moisturized product; and curing the moisturized product with carbon dioxide to obtain the carbonated precast concrete product.
Ultra High Performance Concrete
A precast concrete structure formed of a cementitious mixture is provided, the cementitious mixture comprising a mixture of: (a) cement, (b) silica fume, (c) supplemental material (limestone and/or slag), (d) masonry sand, (e) water and ice (f) plasticizers and (g) workability admixtures. The result is an improved concrete for use in the formation of long span bridge elements that are simple and safe to manufacture and having improved properties. The instant abstract is neither intended to define the invention disclosed in this specification nor intended to limit the scope of the invention in any way.
Ultra High Performance Concrete
A precast concrete structure formed of a cementitious mixture is provided, the cementitious mixture comprising a mixture of: (a) cement, (b) silica fume, (c) supplemental material (limestone and/or slag), (d) masonry sand, (e) water and ice (f) plasticizers and (g) workability admixtures. The result is an improved concrete for use in the formation of long span bridge elements that are simple and safe to manufacture and having improved properties. The instant abstract is neither intended to define the invention disclosed in this specification nor intended to limit the scope of the invention in any way.
Anti-stripping agent for asphalt mixture including refined slowly-cooled slag, method for preparing the same, asphalt mixture including the same and method for preparing the same
The present technology relates to an anti-stripping agent for an asphalt mixture, which includes a refined slowly-cooled slag obtained by processing slag, generated in ironmaking and steelmaking processes, using a specific method, and to a method for preparing the same, an asphalt mixture including the same, and a method for preparing the asphalt mixture. The refined slowly-cooled slag may include 55 to 65 mass % of CaO, 5 to 10 mass % of SiO.sub.2, 1 to 5 mass % of Al.sub.2O.sub.3, and 1 to 5 mass % of MgO.
Anti-stripping agent for asphalt mixture including refined slowly-cooled slag, method for preparing the same, asphalt mixture including the same and method for preparing the same
The present technology relates to an anti-stripping agent for an asphalt mixture, which includes a refined slowly-cooled slag obtained by processing slag, generated in ironmaking and steelmaking processes, using a specific method, and to a method for preparing the same, an asphalt mixture including the same, and a method for preparing the asphalt mixture. The refined slowly-cooled slag may include 55 to 65 mass % of CaO, 5 to 10 mass % of SiO.sub.2, 1 to 5 mass % of Al.sub.2O.sub.3, and 1 to 5 mass % of MgO.