C04B22/147

Multi-component inorganic anchoring system based on fine aluminous cement

A multi-component inorganic anchoring system, for chemical fastening of anchors and post-installed reinforcing bars in mineral substrates, includes a curable powdery aluminous cement component A and an initiator component B in an aqueous phase for initiating a curing process. The powdery aluminous cement component A includes an aluminous cement component based on powdery calcium aluminate cement and component B includes an accelerator constituent and water. Furthermore, at least part of the calcium aluminate cement of component A has an average particle size in the range of from 0.5 to 15 μm. Methods of using the calcium aluminate cement in a multi-component inorganic anchoring system to increase load values and methods for chemical fastening of anchors in mineral substrates can be performed.

Multi-component inorganic anchoring system based on fine aluminous cement

A multi-component inorganic anchoring system, for chemical fastening of anchors and post-installed reinforcing bars in mineral substrates, includes a curable powdery aluminous cement component A and an initiator component B in an aqueous phase for initiating a curing process. The powdery aluminous cement component A includes an aluminous cement component based on powdery calcium aluminate cement and component B includes an accelerator constituent and water. Furthermore, at least part of the calcium aluminate cement of component A has an average particle size in the range of from 0.5 to 15 μm. Methods of using the calcium aluminate cement in a multi-component inorganic anchoring system to increase load values and methods for chemical fastening of anchors in mineral substrates can be performed.

Two-component inorganic injection mortar system based on fine aluminous cement having increased load values

A two-component inorganic injection mortar system includes a curable aqueous-phase aluminous cement component A and an initiator component B in aqueous-phase for initiating the curing process. Component A includes at least one blocking agent which is phosphoric acid, metaphosphoric acid, phosphorous acid or phosphonic acid, at least one plasticizer and water. Component B includes an initiator, at least one retarder, at least one mineral filler and water. The curable aqueous-phase aluminous cement component A includes calcium aluminate cement having an average particle size in the range of from 0.5 to 15 μm. A two-component system, which is ready-for-use, can be used for chemical fastening of anchors, such as metal elements, or in mineral substrates, such as structures made of brickwork, concrete, pervious concrete or natural stone.

Two-component inorganic injection mortar system based on fine aluminous cement having increased load values

A two-component inorganic injection mortar system includes a curable aqueous-phase aluminous cement component A and an initiator component B in aqueous-phase for initiating the curing process. Component A includes at least one blocking agent which is phosphoric acid, metaphosphoric acid, phosphorous acid or phosphonic acid, at least one plasticizer and water. Component B includes an initiator, at least one retarder, at least one mineral filler and water. The curable aqueous-phase aluminous cement component A includes calcium aluminate cement having an average particle size in the range of from 0.5 to 15 μm. A two-component system, which is ready-for-use, can be used for chemical fastening of anchors, such as metal elements, or in mineral substrates, such as structures made of brickwork, concrete, pervious concrete or natural stone.

DOUBLE-RESPONSE SELF-DEGRADABLE TEMPORARY PLUGGING AGENT AND PREPARATION METHOD THEREOF
20210380865 · 2021-12-09 ·

The present disclosure relates to a double-response self-degradable temporary plugging agent and a preparation method thereof. The double-response self-degradable temporary plugging agent is prepared by compounding a crosslinkable monomer with a temperature-sensitive degradablity and an inorganic material with an acid solubility with a first monomer, a dispersant, an initiator and water, and subjecting the resulting mixture to a polymerization.

Passivated cement accelerator

Cement compositions for primary cementing of well bores where a liquid mixture of pre-hydrated cementitious particles are combined with cement particles to form a cement composition. The pre-hydrated cementitious particles are encapsulated with the hydration product and are capable of being stored in a liquid for one day or longer

Passivated cement accelerator

Cement compositions for primary cementing of well bores where a liquid mixture of pre-hydrated cementitious particles are combined with cement particles to form a cement composition. The pre-hydrated cementitious particles are encapsulated with the hydration product and are capable of being stored in a liquid for one day or longer

POZZOLANIC MIXTURE AND CEMENTING COMPOSITION

The present invention is directed to a pozzolanic mixture used as a supplementary cementitious material (SCM) comprising an activated clay, a limestone and a setting regulator. Moreover, it is also directed to a cementitious composition comprising said pozzolanic mixture, a clinker and a setting regulator. Finally, the invention is also directed to a concrete comprising the cementitious composition described above, fine aggregate, coarse aggregate and water, optionally the concrete may have other additives.

POZZOLANIC MIXTURE AND CEMENTING COMPOSITION

The present invention is directed to a pozzolanic mixture used as a supplementary cementitious material (SCM) comprising an activated clay, a limestone and a setting regulator. Moreover, it is also directed to a cementitious composition comprising said pozzolanic mixture, a clinker and a setting regulator. Finally, the invention is also directed to a concrete comprising the cementitious composition described above, fine aggregate, coarse aggregate and water, optionally the concrete may have other additives.

Fire-resistant two-component mortar system based on aluminous cement for a fire-resistant chemical fastening of anchors and post-installed reinforcing bars and use thereof

A fire-resistant two-component mortar system contains a curable aqueous-phase aluminous cement component A and an initiator component B in aqueous-phase for initiating the curing process. Component A further contains at least one blocking agent selected from phosphoric acid, metaphosphoric acid, phosphorous acid and phosphonic acids, at least one plasticizer, and water. Component B contains an initiator, at least one retarder, at least one mineral filler, and water. A fire-resistant two-component system, which is ready-for-use, can be used for a fire-resistant chemical fastening of anchors and post-installed reinforcing bars in mineral surfaces, such as structures made of brickwork, concrete, pervious concrete or natural stone.