C04B24/223

DRY GROUT COMPOSITION AND CAPSULE FOR ANCHORING REINFORCING MEMBER, DOWEL OR ANCHOR ELEMENTS
20200317570 · 2020-10-08 ·

A dry grout composition including a calcium aluminosulfate based hydraulic cement, a mineral filler, a thixotropic agent, and a superplasticizer agent. Also, an anchoring capsule, containing the dry grout composition, for use in anchoring reinforcing member dowel, or anchor elements in a hole of a substrate, and a method of use.

Additive containing a superplasticizer and a copolymer

The present invention relates to admixtures, especially a dispersant for solid particles, in particular a dispersant for mineral binder compositions, comprising: a) a superplasticizer and b) a copolymer having a polymer backbone and side chains bonded thereto, comprising at least one ionizable monomer unit M1 and at least one side chain-bearing monomer unit M2, wherein the copolymer has a nonrandom distribution of the monomer units M1 and/or the monomer units M2 in a direction along the polymer backbone, and wherein the superplasticizer and the copolymer differ from a chemical and/or structural point of view.

Additive containing a superplasticizer and a copolymer

The present invention relates to admixtures, especially a dispersant for solid particles, in particular a dispersant for mineral binder compositions, comprising: a) a superplasticizer and b) a copolymer having a polymer backbone and side chains bonded thereto, comprising at least one ionizable monomer unit M1 and at least one side chain-bearing monomer unit M2, wherein the copolymer has a nonrandom distribution of the monomer units M1 and/or the monomer units M2 in a direction along the polymer backbone, and wherein the superplasticizer and the copolymer differ from a chemical and/or structural point of view.

Polymer dispersant for well cementing

The present disclosure concerns a cement dispersant for cement compositions wherein the cement dispersant is a polynaphthalene sulfonate salt having a weight average molecular weight of from 2500 g/mol to 3000 g/mol. The cement compositions are of from 10 weight percent to 70 weight percent of a cement precursor based on the total weight of the cement composition, from 5 weight percent to 70 weight percent water based on the total weight of the cement composition, and from 0.001 percent by weight of cement (BWOC) to 1.0 percent BWOC the cement dispersant. The cement dispersant provides improved rheological properties, allowing for good cement dispensing and increased presence of weighting agents.

Polymer dispersant for well cementing

The present disclosure concerns a cement dispersant for cement compositions wherein the cement dispersant is a polynaphthalene sulfonate salt having a weight average molecular weight of from 2500 g/mol to 3000 g/mol. The cement compositions are of from 10 weight percent to 70 weight percent of a cement precursor based on the total weight of the cement composition, from 5 weight percent to 70 weight percent water based on the total weight of the cement composition, and from 0.001 percent by weight of cement (BWOC) to 1.0 percent BWOC the cement dispersant. The cement dispersant provides improved rheological properties, allowing for good cement dispensing and increased presence of weighting agents.

ENGINEERED CONCRETE BINDER COMPOSITION
20190345059 · 2019-11-14 ·

A novel engineered concrete binder composition providing overall reduced clinker factor and improved binding properties. The said concrete binder composition includes a primary binder in a ratio of 10-60 weight percent and a secondary binder in a ratio of 40-90 weight percent. The said primary binder is selected from a primary material group having spontaneous hydration property. The said secondary binder is selected from a secondary material group having induced hydration property.

ENGINEERED CONCRETE BINDER COMPOSITION
20190345059 · 2019-11-14 ·

A novel engineered concrete binder composition providing overall reduced clinker factor and improved binding properties. The said concrete binder composition includes a primary binder in a ratio of 10-60 weight percent and a secondary binder in a ratio of 40-90 weight percent. The said primary binder is selected from a primary material group having spontaneous hydration property. The said secondary binder is selected from a secondary material group having induced hydration property.

PREPARATION OF WATER-REDUCING COMPOSITION, WATER-REDUCING COMPOSITION AND HYDRAULIC COMPOSITION
20190330109 · 2019-10-31 · ·

A water-reducing composition is obtained by a method for preparing the water-reducing composition, the method including stirring a water-reducing agent, a water-soluble cellulose ether, a gum and a defoamer by a high speed stirrer, in which the water-reducing agent has a solid component concentration of 10 to 25% by weight and an Na.sup.+ ion concentration of 8,500 ppm or higher, and in which a stirring element in the high speed stirrer has a peripheral speed of 8.50 m/s or higher, and the water-reducing composition has a sedimentation volume of 80% by volume or higher after being left standing for 72 hours from immediately after preparing the water-reducing composition, or being dispersion.

PREPARATION OF WATER-REDUCING COMPOSITION, WATER-REDUCING COMPOSITION AND HYDRAULIC COMPOSITION
20190330109 · 2019-10-31 · ·

A water-reducing composition is obtained by a method for preparing the water-reducing composition, the method including stirring a water-reducing agent, a water-soluble cellulose ether, a gum and a defoamer by a high speed stirrer, in which the water-reducing agent has a solid component concentration of 10 to 25% by weight and an Na.sup.+ ion concentration of 8,500 ppm or higher, and in which a stirring element in the high speed stirrer has a peripheral speed of 8.50 m/s or higher, and the water-reducing composition has a sedimentation volume of 80% by volume or higher after being left standing for 72 hours from immediately after preparing the water-reducing composition, or being dispersion.

Method for preparing hydraulic composition
10435332 · 2019-10-08 · ·

A hydraulic composition is prepared by mixing (A) an admixture aqueous solution containing a water-soluble salt which is a water-reducing agent or setting retarder, and a water-soluble cellulose ether with (B) a fresh concrete composition containing a hydraulic substance, an aggregate, and water at job site. The method is effective for preventing the admixture solution from thickening even though the water-soluble cellulose ether without glyoxal treatment is used.