C04B35/83
High temperature oxidation protection for composites
Systems and methods for forming an oxidation protection system on a composite structure are provided. In various embodiments, an oxidation protection system disposed on a substrate may comprise a boron-silicon-glass layer formed directly on the composite structure. The boron-silicon-glass layer may comprise a boron compound, a silicon compound, and a glass compound.
Barrier coating resin formulations, and related methods
A barrier coating resin formulation comprising at least one polycarbosilane preceramic polymer, at least one organically modified silicon dioxide preceramic polymer, at least one filler, and at least one solvent. A barrier coating comprising a reaction product of the at least one polycarbosilane preceramic polymer and the at least one organically modified silicon dioxide preceramic polymer and the at least one filler is also disclosed, as are articles comprising the barrier coating, rocket motors comprising the barrier coating, and methods of forming the articles.
Barrier coating resin formulations, and related methods
A barrier coating resin formulation comprising at least one polycarbosilane preceramic polymer, at least one organically modified silicon dioxide preceramic polymer, at least one filler, and at least one solvent. A barrier coating comprising a reaction product of the at least one polycarbosilane preceramic polymer and the at least one organically modified silicon dioxide preceramic polymer and the at least one filler is also disclosed, as are articles comprising the barrier coating, rocket motors comprising the barrier coating, and methods of forming the articles.
High temperature oxidation protection for composites
An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.
High temperature oxidation protection for composites
An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.
Graphite-containing refractory and method of producing graphite-containing refractory
A method of producing a graphite-containing refractory within which carbon fiber bundles are placed, the graphite constituting 1% to 80% by mass, the method including a bundling step of bundling carbon fibers to form the carbon fiber bundles; a mixing step of mixing a refractory raw material with graphite to prepare a graphite-containing refractory raw material; a pressing step of pressing the graphite-containing refractory raw material in which the carbon fiber bundles are placed to prepare a formed product; and a drying step of drying the pressed product, wherein the bundling step includes bundling 1000 to 300000 of the carbon fibers with a fiber diameter of 1 to 45 μm/fiber to form carbon fiber bundles 100 mm or more in length.
Graphite-containing refractory and method of producing graphite-containing refractory
A method of producing a graphite-containing refractory within which carbon fiber bundles are placed, the graphite constituting 1% to 80% by mass, the method including a bundling step of bundling carbon fibers to form the carbon fiber bundles; a mixing step of mixing a refractory raw material with graphite to prepare a graphite-containing refractory raw material; a pressing step of pressing the graphite-containing refractory raw material in which the carbon fiber bundles are placed to prepare a formed product; and a drying step of drying the pressed product, wherein the bundling step includes bundling 1000 to 300000 of the carbon fibers with a fiber diameter of 1 to 45 μm/fiber to form carbon fiber bundles 100 mm or more in length.
METHOD FOR DENSIFYING COMPOSITE MATERIALS
A method for densifying one or more porous substrates with pyrolytic carbon by chemical vapour infiltration, includes admitting, at the inlet of the densification furnace, a reactive gaseous phase including at least one pyrolytic carbon precursor; reacting at least a fraction of the reactive gaseous phase with the porous substrate or substrates; extracting, at the outlet of the densification furnace, gaseous effluents originating from the reactive gaseous phase; reintroducing, with the reactive gaseous phase admitted at the inlet of the densification furnace, at least a fraction of the gaseous effluents extracted at the outlet of the furnace, wherein the fraction of the gaseous effluents introduced with the reactive gaseous phase includes at least one polyaromatic hydrocarbon compound.
METHOD FOR DENSIFYING COMPOSITE MATERIALS
A method for densifying one or more porous substrates with pyrolytic carbon by chemical vapour infiltration, includes admitting, at the inlet of the densification furnace, a reactive gaseous phase including at least one pyrolytic carbon precursor; reacting at least a fraction of the reactive gaseous phase with the porous substrate or substrates; extracting, at the outlet of the densification furnace, gaseous effluents originating from the reactive gaseous phase; reintroducing, with the reactive gaseous phase admitted at the inlet of the densification furnace, at least a fraction of the gaseous effluents extracted at the outlet of the furnace, wherein the fraction of the gaseous effluents introduced with the reactive gaseous phase includes at least one polyaromatic hydrocarbon compound.
Method for injecting a loaded suspension into a fibrous texture and method for manufacturing a part made of composite material
A method for injecting a loaded suspension into a fibrous texture having a three-dimensional or multilayer weaving includes the injection of a suspension containing a powder of solid particles into the volume of the fibrous texture. The injection of the loaded suspension is carried out by at least one hollow needle in communication with a loaded suspension supply device, each needle being movable in at least one direction extending between a first face and a second opposite face of the fibrous texture so as to inject the loaded suspension at one or more determined depths in the fibrous texture.