C04B41/86

HIGH TEMPERATURE OXIDATION PROTECTION FOR CARBON-CARBON COMPOSITES
20230150884 · 2023-05-18 · ·

A method for forming an oxidation protection system on a composite structure may comprise: applying a ceramic layer slurry to the composite structure, wherein the ceramic layer slurry comprises aluminum and silicon in a solvent or carrier fluid; and heating the composite structure in an environment comprising nitrogen gas and oxygen gas to form a ceramic layer on the composite structure, wherein the ceramic layer comprises aluminum nitride and alumina.

HIGH TEMPERATURE OXIDATION PROTECTION FOR CARBON-CARBON COMPOSITES
20230150884 · 2023-05-18 · ·

A method for forming an oxidation protection system on a composite structure may comprise: applying a ceramic layer slurry to the composite structure, wherein the ceramic layer slurry comprises aluminum and silicon in a solvent or carrier fluid; and heating the composite structure in an environment comprising nitrogen gas and oxygen gas to form a ceramic layer on the composite structure, wherein the ceramic layer comprises aluminum nitride and alumina.

Cool side coating for ceramic or ceramic matrix composite article

An article may include a substrate including a ceramic or a ceramic matrix composite. The substrate defines a hot side surface configured to face a heated gas environment and a cool side surface opposite the hot side surface. The article also includes a cool side coating on the cool side surface. The cool side coating comprises at least one material having a flow temperature equal to or slightly less than a temperature of the heated gas environment.

Cool side coating for ceramic or ceramic matrix composite article

An article may include a substrate including a ceramic or a ceramic matrix composite. The substrate defines a hot side surface configured to face a heated gas environment and a cool side surface opposite the hot side surface. The article also includes a cool side coating on the cool side surface. The cool side coating comprises at least one material having a flow temperature equal to or slightly less than a temperature of the heated gas environment.

HIGH-WEAR-RESISTANCE FAR-INFRARED CERAMIC POLISHED GLAZED TILE AND PREPARATION METHOD THEREFOR

The present application provides a high-wear-resistance far-infrared ceramic polished glazed tile and preparation method therefor. The preparation method includes application of far-infrared overglaze, ink-jet printing, application of transparent far-infrared polished glaze and application of abrasion-resistant far-infrared polished glaze in sequence on a body, firing, and polishing. By adopting the far-infrared overglaze, the transparent far-infrared polished glaze and the abrasion-resistant far-infrared polished glaze in combination, the polished glaze tile can have a far-infrared function, high transparency, and high abrasion resistance.

HIGH-WEAR-RESISTANCE FAR-INFRARED CERAMIC POLISHED GLAZED TILE AND PREPARATION METHOD THEREFOR

The present application provides a high-wear-resistance far-infrared ceramic polished glazed tile and preparation method therefor. The preparation method includes application of far-infrared overglaze, ink-jet printing, application of transparent far-infrared polished glaze and application of abrasion-resistant far-infrared polished glaze in sequence on a body, firing, and polishing. By adopting the far-infrared overglaze, the transparent far-infrared polished glaze and the abrasion-resistant far-infrared polished glaze in combination, the polished glaze tile can have a far-infrared function, high transparency, and high abrasion resistance.

NANOCOMPOSITE COATINGS FOR OXIDATION PROTECTION OF COMPOSITES
20170349825 · 2017-12-07 · ·

The present disclosure provides a method for coating a composite structure comprising the steps of applying a first slurry of a first phosphate glass composition on an outer surface of the composite structure. The first slurry comprises a first additive including at least one of molybdenum disulfide or tungsten disulfide. The method may further include heating the composite structure to a temperature sufficient to form a base layer adhered to the composite structure.

METHOD TO FABRICATE HIGH TEMPERATURE COMPOSITE WITH INTEGRATED BARRIER COATING

A method of fabricating a ceramic component includes hot pressing a composite component with a glass powder / filler cover mixture to form a consolidated glass-based coating on the composite component.

METHOD TO FABRICATE HIGH TEMPERATURE COMPOSITE WITH INTEGRATED BARRIER COATING

A method of fabricating a ceramic component includes hot pressing a composite component with a glass powder / filler cover mixture to form a consolidated glass-based coating on the composite component.

Red paint for ceramic decoration

The present invention provides a red paint for ceramic decoration, including a glass matrix, and a red colorant and a protective material that are intermingled in the glass matrix. The red colorant contains gold nanoparticles and silver nanoparticles. The protective material contains silica nanoparticles.