C04B2235/3852

Ceramic article and method therefor using particle infiltration and preceramic polymer infiltration

A method of fabricating a ceramic article includes providing a porous body that includes a plurality of fiber bundles that has an intra-bundle porosity and an inter-bundle porosity, infiltrating the intra-bundle porosity and the inter-bundle porosity with a mixture of particles in a liquid carrier, the particles having an average size selected with respect to at least the intra-bundle porosity, removing the liquid carrier from the porous body to deposit the particles in the intra-bundle porosity and in the inter-bundle porosity, infiltrating a preceramic polymer into a remaining intra-bundle porosity and a remaining inter-bundle porosity, and thermally converting the preceramic polymer to a ceramic material.

MATERIALS FOR AMMONIA SYNTHESIS
20200224323 · 2020-07-16 ·

Disclosed herein are doped perovskite oxides. The doped perovskite oxides may be used as a cathode material in an electrochemical cell to electrochemically generate ammonia from N.sub.2. The doped perovskite oxides may be combined with nitride compounds, for instance iron nitride, to further increase the efficiency of the ammonia production.

BORON NITRIDE NANOTUBE (BNNT)-NANOPARTICLE COMPOSITES, METHODS FOR THE PREPARATION THEREOF AND THEIR MACROSCOPIC ASSEMBLIES

The present application relates to boron nitride nanotube (BNNT)-nanoparticle composites, to methods of preparing such composites and their use, for example, in metal/ceramic matrix composites and/or macroscopic assemblies. For example, the methods comprise subjecting a source of hydrogen, a source of boron, a source of nitrogen and a nanoparticle precursor to a stable induction thermal plasma and cooling the reaction mixture to obtain the composite.

Sintered material and cutting tool including same

A sintered material includes cubic boron nitride grains and a binder, a grain size D50 of the cubic boron nitride grains when a cumulative value of the cubic boron nitride grains is 50% in an area-based grain size distribution being more than 0.5 m and less than or equal to 5 m, more than or equal to 70 volume % and less than or equal to 98 volume % of the cubic boron nitride grains being included in the sintered material, the binder being composed of A.sub.1-xCr.sub.xN, where 0x1, and a remainder, the remainder being composed of at least one of a first element and a compound including the first element and a second element, the first element being one or more elements selected from a group consisting of W, Co, Ni, Mo, Al, and Cr, the second element being one or more elements selected from a group consisting of nitrogen, carbon, oxygen, and boron.

METHOD FOR PRODUCING CERAMIC SINTERED BODY, CERAMIC SINTERED BODY, AND LIGHT EMITTING DEVICE
20200172804 · 2020-06-04 · ·

Provided are a method for producing a ceramic sintered body having improved light emission intensity, a ceramic sintered body, and a light emitting device. The method for producing a ceramic sintered body comprises preparing a molded body that contains a nitride fluorescent material having a composition containing: at least one alkaline earth metal element M.sup.1 selected from the group consisting of Ba, Sr, Ca, and Mg; at least one metal element M.sup.2 selected from the group consisting of Eu, Ce, Tb, and Mn; Si; and N, wherein a total molar ratio of the alkaline earth metal element M.sup.1 and the metal element M.sup.2 in 1 mol of the composition is 2, a molar ratio of the metal element M.sup.2 is a product of 2 and a parameter y and wherein y is in a range of 0.001 or more and less than 0.5, a molar ratio of Si is 5, and a molar ratio of N is 8, and wherein the nitride fluorescent material has a crystallite size, as calculated by X-ray diffraction measurement using the Halder-Wagner method, of 550 or less, and calcining the molded body at a temperature in a range of 1,600 C. or more and 2,200 C. or less to obtain a sintered body.

Polycrystalline diamond with iron-containing binder

This disclosure relates to a polycrystalline diamond (PCD) body comprising a PCD material formed of intergrown diamond grains forming a diamond network, and an iron-containing binder.

Semiconductor Substrate
20200144154 · 2020-05-07 ·

A semiconductor substrate includes a dielectric insulation layer and a first metallization layer attached to the dielectric insulation layer. The dielectric insulation layer includes a first material having a thermal conductivity of between 25 and 180 W/mK, and an insulation strength of between 15 and 50 kV/mm, and an electrically conducting or semiconducting second material evenly distributed within the first material.

Surface Modified Particulate In Sintered Products
20200115289 · 2020-04-16 ·

Disclosed are coated inorganic particulate and polymer composite material for use in molding/sintering processes. The composite material is uniquely adapted for forming powdered materials into solid objects and associated processes. Improved products are provided under process conditions through surface interfacially modified powders.

Refractory ceramic product

The invention relates to a refractory ceramic product.

SILICON CARBIDE CERAMIC
20200071236 · 2020-03-05 ·

An object of the present invention is to provide an SiC ceramics having an excellent environmentally resistant coating.

An SiC ceramics comprising a metal oxide, the SiC ceramics comprising a surface modification layer containing a silicate, the surface modification layer being derived from a raw material forming the SiC ceramics, which is a matrix.