C04B2235/405

Member for plasma processing apparatus and plasma processing apparatus with the same

Provided is a member for a plasma processing apparatus consisting of a tungsten carbide phase. The member includes at least one type of atom selected from the group consisting of a Fe atom, a Co atom, and a Ni atom, in which the total content of the atoms is in a range of 30 to 3300 atomic ppm.

PRECIPITATE-STRENGTHENED HARD METAL-DIAMOND COMPOSITE
20220397005 · 2022-12-15 ·

A cutting table for a cutting element, including: a diamond phase; a tungsten carbide phase; a cobalt-tungsten metallic phase; and an intermetallic phase comprising Co.sub.3WC.sub.x, where 0≤x≤1. Also disclosed is a method of manufacturing a cutting element, the method including: sintering diamond and tungsten carbide particles in the presence of Co and W to about 1520° C. or greater under pressure of about 57 kbar or greater to form a hard metal-diamond composite compact and solubilize carbon and tungsten within the compact; cooling the cutting element at about 1° C./sec or greater; and subsequent to cooling the cutting element, heat-treating the cutting element to precipitate carbon and tungsten in the compact as an intermetallic phase.

THROUGH THICKNESS REINFORCEMENT
20220388912 · 2022-12-08 ·

A method for making a ceramic matrix composite component includes densifying a fibrous preform of the component with a ceramic matrix to form an intermediate component; infiltrating a hole in the intermediate component with an infiltrate material comprising a solid and a metallic alloy whose reaction forms a carbide, silicide, boride or combination thereof, heating the infiltrate material to a temperature in excess of a melting point of the metallic alloy; and sequentially cooling regions of the hole starting from an interior end of the hole to the outer surface of the intermediate component to form a solidified through-thickness reinforcement element. The hole extends in a through-thickness direction and is open to an exterior surface of the intermediate component.

SUPERHARD CONSTRUCTIONS AND METHODS OF MAKING SAME

A polycrystalline super hard construction is disclosed having a first region comprising a body of thermally stable polycrystalline super hard material having an exposed surface forming a working surface, and a peripheral side edge, the polycrystalline super hard material comprising a plurality of grains of super hard material; a second region forming a substrate to the first region; and a third region interposed between the first and second regions. The third region extends across a surface of the second region along an interface, the interface comprising a portion having an uneven topology and a substantially planar portion, the third region comprising a composite material including a first phase comprising a plurality of non-intergrown diamond grains, and a matrix material.

Superhard constructions and methods of making same

A polycrystalline super hard construction comprises a body of polycrystalline super hard material and a substrate bonded to the body along an interface. The substrate a first end surface forming the interface, the first end surface comprising a projection extending from the body of the substrate into the body of super hard material towards the cutting face, the body of polycrystalline material extending around the projection. The body of polycrystalline material comprises a first region more thermally stable than a second region, the first region comprising an annular portion located around the projection, the second region extending between and bonding the first region to the substrate. The first region has a thickness from the cutting face along the peripheral side edge to the interface of at least around 3 mm and a portion of the projection has a thickness measured in a plane extending along the longitudinal axis of at least around 3 mm.

SiC powder and method for manufacturing same, electrically heated honeycomb structure and method for manufacturing same

A SiC powder containing 70% by mass or more of a β-SiC, wherein in a volume-based cumulative particle size distribution measured by a laser diffraction method, a D50 is 8 to 35 μm and a D10 is 5 μm or more.

SUPPORTING SUBSTRATES FOR CUTTING ELEMENTS, AND RELATED METHODS
20230091691 · 2023-03-23 ·

A cutting element comprises a supporting substrate, and a cutting table attached to an end of the supporting substrate. The cutting table comprises inter-bonded diamond particles, and a thermally stable material within interstitial spaces between the inter-bonded diamond particles. The thermally stable material comprises a carbide precipitate having the general chemical formula, A.sub.3XZ.sub.n-1, where A comprises one or more of Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, Hf, Ta, W, Re, Os, Ir, Pt, Au, Hg, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Ac, Th, Pa, and U; X comprises one or more of Al, Ga, Sn, Be, Bi, Te, Sb, Se, As, Ge, Si, B, and P; Z comprises C; and n is greater than or equal to 0 and less than or equal to 0.75. A method of forming a cutting element, an earth-boring tool, a supporting substrate, and a method of forming a supporting substrate are also described.

Method for manufacturing sintered body, structure, and composite structure
11607728 · 2023-03-21 · ·

A method for manufacturing a sintered body, the method including heating a mixture that contains a plurality of particles of a metal oxide having a spinel-type structure, and a metal acetylacetonate under pressure at a temperature of from a melting point or higher of the metal acetylacetonate to 600° C. or lower, to form a sintered body that contains the metal oxide having the spinel-type structure.

SILICON NITRIDE SINTERED BODY, WEAR-RESISTANT MEMBER USING THE SAME, AND MANUFACTURING METHOD FOR SILICON NITRIDE SINTERED BODY
20230080570 · 2023-03-16 ·

A silicon nitride sintered body includes at least one black portion with a major axis of 10 μm or more in a field of view with a unit area of 5 mm×5 mm, when observing an arbitrary cross-section of the silicon nitride sintered body using a metallurgical microscope. A major axis of the black portion is Preferably 500 μm or less. The number of the black portion within the field of view with a unit area of 5 mm×5 mm is preferably 2 or more and 10 or less. A segregation portion of Fe is preferably included in the black portion.

Magnetizable abrasive particle and method of making the same

Magnetizable abrasive particles are described comprising ceramic particles having outer surfaces comprising a coating of unsintered polyion and magnetic particles bonded to the polyion. In favored embodiments, the magnetic particles have a magnetic saturation of at least 10, 15, 20, 25, 30, 35, 40, 45 or 50 emu/gram. In another embodiment, an abrasive article is described comprising a plurality of magnetizable abrasive particles as described herein retained in a binder material. Also described are method of making magnetizable abrasive particles and methods of making an abrasive article comprising magnetizable abrasive particles.