C04B2235/428

METHOD OF FORMING CERAMIC MATRIX COMPOSITE AND CERAMIC MATRIX COMPOSITE

A method of forming a ceramic matrix composite with being impregnated with molten metal includes: stacking a plurality of fiber layers that are layers of reinforced fibers impregnated with base resin to form a laminate in which a matrix layer containing fibers extending in a direction of impregnation with the molten metal is disposed between the fiber layers; forming an impregnation path in the matrix layer entirely in an in-plane direction perpendicular to a direction of the stacking in the laminate by carbonizing the formed laminate; and impregnating, with the molten metal, the laminate in which the impregnation path has been formed.

Negative electrode active material for lithium secondary battery, preparation method therefor, and lithium secondary battery comprising same

The present invention relates to a negative active material for a lithium secondary battery, a preparation method therefor, and a lithium secondary battery including the same. The negative electrode active material is a negative electrode material for a secondary battery, the negative electrode active material comprising a silicon-carbon composite comprising: a core comprising crystalline carbon and silicon particles; and an amorphous carbon-containing coating layer disposed on a surface of the core, wherein the negative electrode active material comprises: silicon oxide formed on a surface of the silicon particles; and an oxide of crystalline carbon, formed on a surface of the crystalline carbon, the average particle diameter (D50) of the silicon particles having a nanometer size, the proportion of O relative to Si in the silicon oxide is 30%-50%, and the proportion of O relative to C in the oxide of the crystalline carbon is 4%-10%.

Ceramic component

A ceramic component, wherein the component contains 20 to 60 wt. % SiC, 5 to 40 wt. % free silicon and 10 to 65 wt. % free carbon. The disclosure also relates to the use of the component. The method for producing the ceramic component includes the following steps: a) providing a green body based on carbon, which has been produced by means of a 3D-printing method, b) impregnating the green body with a solution selected from the group consisting of a sugar solution, a starch solution or a cellulose solution, or a resin system including a mixture containing at least one resin, at least one solvent and at least one curing agent, wherein the at least one resin and the at least one solvent are different, c) drying or curing the impregnated green body.

NOVEL MATERIALS WITH EXTREMELY DURABLE INTERCALATION OF LITHIUM AND MANUFACTURING METHODS THEREOF

Composites of silicon and various porous scaffold materials, such as carbon material comprising micro-, meso- and/or macropores, and methods for manufacturing the same are provided. The compositions find utility in various applications, including electrical energy storage electrodes and devices comprising the same.

Silicon carbide body with localized diamond reinforcement

A reaction-bonded silicon carbide (SiC) body is produced by: providing a preform including ceramic elements and carbon, and one or more surface features; providing a powder which includes diamond particles and carbon; locating the powder in the surface feature(s); and infiltrating the preform and the powder with molten silicon (Si) to form reaction-bonded SiC in the preform, and to form reaction-bonded SiC coatings on the diamond particles. The present disclosure also relates to a device/component which includes: a main body portion and discrete elements located at least partially within the main body portion. The main body portion may include reaction-bonded SiC and Si, but not diamond, while the discrete elements include diamond particles, reaction-bonded SiC coatings surrounding the diamond particles, and Si. According to the present disclosure, diamond may be advantageously located only where it is needed.

Method and apparatus for pyrolyzing an electrode

An electrode heat treatment device and associated method for fabricating an electrode are described, and include forming a workpiece, including coating a current collector with a slurry. The workpiece is placed on a first spool, and the first spool including the workpiece is placed in a sealable chamber, wherein the sealable chamber includes the first spool, a heat exchange work space, and a second spool. An inert environment is created in the sealable chamber. The workpiece is subjected to a multi-step continuous heat treatment operation in the inert environment, wherein the multi-step continuous heat treatment operation includes continuously transferring the workpiece through the heat exchange work space between the first spool and the second spool and controlling the heat exchange work space to an elevated temperature.

ARMOR PLATING MADE OF FINE-GRAIN BORON CARBIDE AND SILICON CARBIDE
20230034822 · 2023-02-02 ·

An antiballistic armor-plating component, includes a ceramic body made of a material comprising, as percentages by volume, between 35% and 55% of silicon carbide, between 20% and 50% of boron carbide, between 15% and 35% of a metallic silicon phase or of a metallic phase including silicon.

SiC powder and method for manufacturing same, electrically heated honeycomb structure and method for manufacturing same

A SiC powder containing 70% by mass or more of a β-SiC, wherein in a volume-based cumulative particle size distribution measured by a laser diffraction method, a D50 is 8 to 35 μm and a D10 is 5 μm or more.

CVD FUNCTIONALIZED PARTICLES FOR CMC APPLICATIONS
20230036697 · 2023-02-02 ·

A method of manufacturing ceramic matrix composites includes producing chemical vapor deposition functionalized ceramic particles before injecting the functionalized ceramic particles into the CMC fabric. The functionalized ceramic particles are mixed with a binder solution and then dispensed into voids present between adjacent tows of the CMC fabric. Injecting the particles in the center of the voids reduces the size and volume fraction of the voids/defects, improving the homogeneity of surface texture, homogeneity of microstructure, and part model shape conformity.

SUPPORTING SUBSTRATES FOR CUTTING ELEMENTS, AND RELATED METHODS
20230091691 · 2023-03-23 ·

A cutting element comprises a supporting substrate, and a cutting table attached to an end of the supporting substrate. The cutting table comprises inter-bonded diamond particles, and a thermally stable material within interstitial spaces between the inter-bonded diamond particles. The thermally stable material comprises a carbide precipitate having the general chemical formula, A.sub.3XZ.sub.n-1, where A comprises one or more of Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, Hf, Ta, W, Re, Os, Ir, Pt, Au, Hg, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Ac, Th, Pa, and U; X comprises one or more of Al, Ga, Sn, Be, Bi, Te, Sb, Se, As, Ge, Si, B, and P; Z comprises C; and n is greater than or equal to 0 and less than or equal to 0.75. A method of forming a cutting element, an earth-boring tool, a supporting substrate, and a method of forming a supporting substrate are also described.