Patent classifications
C04B2235/785
ELECTROLYTE SHEET FOR SOLID OXIDE FUEL BATTERY, PRODUCTION METHOD OF ELECTROLYTE SHEET FOR SOLID OXIDE FUEL BATTERY, AND SINGLE CELL FOR SOLID OXIDE FUEL BATTERY
An electrolyte sheet for solid oxide fuel cells includes a ceramic plate body containing a cubic zirconia sintered material, wherein, with the ceramic plate body being defined to have nine portions including an outer peripheral portion and a central portion, ceramic grains in each of the nine portions have a median size D.sub.50 of 1.0 μm to 4.0 μm, and a maximum median size D.sub.50 of the ceramic grains among the nine portions is 1.0 to 1.3 times a minimum median size D.sub.50 of the ceramic grains among the nine portions.
METHOD OF MANUFACTURING MULTILAYER CERAMIC CAPACITOR
A method of manufacturing a multilayer ceramic capacitor includes printing an internal electrode pattern on a dielectric layer, forming a dielectric pattern in a region other than a region in which the internal electrode pattern is printed, laminating dielectric layers to form a multilayer body, exposing the internal electrode pattern and the dielectric pattern from a side surface of the multilayer body, removing at least a portion of the exposed dielectric pattern, and forming a dielectric gap layer on the side surface.
Lithium composite oxide sintered body plate and lithium secondary battery
Disclosed is a lithium complex oxide sintered plate including a plurality of primary grains having a layered rock-salt structure, the primary grains being bonded. The lithium complex oxide has a composition represented by the formula: Li.sub.x(Co.sub.1-yM.sub.y)O.sub.2±δ (wherein, 1.0≤x≤1.1, 0<y≤0.1, 0≤δ<1, and M is at least one selected from the group consisting of Mg, Ni, Al, and Mn), and the primary grains have a mean tilt angle of more than 0° to 30° or less, the mean tilt angle being a mean value of the angles defined by the (003) planes of the primary grains and the plate face of the lithium complex oxide sintered plate.
Dielectric ceramic composition and multi-layer ceramic electronic component using the same
A dielectric ceramic composition and a multilayer ceramic electronic component are provided, the dielectric ceramic composition includes a barium titanate base material main component and a subcomponent, a microstructure after sintering includes a first crystal grain including 3 or less domain boundaries and a second crystal grain including 4 or more domain boundaries, and an area ratio of the second crystal grain to the total crystal grains is 20% or less.
Process for Producing a Colored Dental Zirconia Article
The invention relates to a process of producing a dental zirconia article, the process comprising the step of sintering a porous dental zirconia article, the sintering comprising a heat-treatment segment A characterized by a heating rate of at least 3 K/sec up to a temperature of at least 1,200° C., the porous dental zirconia article being composed of a zirconia material containing 6.0 to 8.0 wt. % yttria, 0.05 to 0.12 wt. % alumina and comprising a coloring component containing Tb, the porous dental zirconia article being essentially free of Fe components. The invention also relates to a process comprising the additional step of applying a glazing composition to the outer surface of the porous zirconia article before the heat-treatment or sintering is conducted.
DIELECTRIC COMPOSITION AND MULTILAYER CAPACITOR INCLUDING THE SAME
There are provided a dielectric composition and a multilayer capacitor including the same. The dielectric composition contains: barium titanate (BaTiO.sub.3); and 0.6 to 0.9 mol of calcium (Ca) and 0.5 to 2.0 mol of magnesium (Mg) based on 100 mol of barium titanate.
Composite sintered material and tool using same
A composite sintered material includes: cubic boron nitride grains; and hexagonal boron nitride grains or the hexagonal boron nitride grains and wurtzite type boron nitride grains, wherein a dislocation density of the cubic boron nitride grains is more than or equal to 1×10.sup.15/m.sup.2 and less than or equal to 1×10.sup.17/m.sup.2, a median diameter d50 of equivalent circle diameters of the cubic boron nitride grains is more than or equal to 10 nm and less than or equal to 500 nm, and a relationship of the following expression 1 is satisfied:
0.015≤(Vh+Vw)/(Vc+Vh+Vw)≤0.5, Expression 1:
where Vc represents a volume-based content ratio of the cubic boron nitride grains, Vh represents a volume-based content ratio of the hexagonal boron nitride grains, and Vw represents a volume-based content ratio of the wurtzite type boron nitride grains.
INSERT AND CUTTING TOOL
An insert includes a cBN sintered compact including cBN particles and a binder phase binding the cBN particles. The cBN particles occupy 60% or more of the cross-sectional area of the cBN sintered compact. The binder phase contains Al compound particles containing at least one of AN or Al.sub.2O.sub.3. A particle distribution of the Al compound particles in a cumulative distribution based on the number of the Al compound particles in a cross section of the cBN sintered compact is as follows. The proportion of the Al compound particles with the particle diameter of 0.3 μm or larger is 5% or more, and the proportion of the Al compound particles with the particle diameter of 0.5 μm or larger is less than 5%.
Method of manufacturing multilayer ceramic capacitor
A method of manufacturing a multilayer ceramic capacitor includes printing an internal electrode pattern on a dielectric layer, forming a dielectric pattern in a region other than a region in which the internal electrode pattern is printed, laminating dielectric layers to form a multilayer body, exposing the internal electrode pattern and the dielectric pattern from a side surface of the multilayer body, removing at least a portion of the exposed dielectric pattern, and forming a dielectric gap layer on the side surface.
Hard sintered body
The present invention provides a sintered body containing W and WC, having excellent hardness, strength, compactness, and corrosion resistance, without containing W.sub.2C, and capable of being used for the purpose of a cutting tool or a glass molding die, or a seal ring. There is provided a sintered body containing 4 to 50 vol % of tungsten metal as binder phases, 50 to 95 vol % of tungsten carbide (WC), and 0.5 to 5.0 vol % of tungsten oxide (WO.sub.2), in which the tungsten oxide (WO.sub.2) has an average grain size of 5 nm to 150 nm and is present in a sintered body structure at an average density of 5 to 20 particles/μm.sup.2.