C04B2237/127
ELECTRIC CIRCUIT BOARD AND POWER MODULE
An electric circuit board includes an insulating substrate, a metal plate, and a brazing material with which the insulating substrate and the metal plate are joined together. The metal plate has a side surface over which recessed portions are scattered. The side surface of the metal plate has lines in regions around the recessed portions. The metal plate is made of copper or a copper alloy. The brazing material has a side surface that is continuous with the side surface of the metal plate. The brazing material is a silver-copper brazing alloy. A ratio of copper on the side surface of the brazing material is higher than a copper component ratio of the silver-copper brazing alloy.
Process for Producing a Metal-Ceramic Substrate, and a Metal-Ceramic Substrate Produced Using Such Method
The invention relates to a process for producing a metal-ceramic substrate (1), comprising: providing a ceramic element (10) and a metal layer, providing a gas-tight container (25) that encloses the ceramic element (10), the container (25) preferably being formed from the metal layer or comprising the metal layer, forming the metal-ceramic substrate (1) by connecting the metal layer to the ceramic element (10) by means of hot isostatic pressing, wherein, for the purpose of forming the metal-ceramic substrate (1), an active metal layer (15) or a contact layer comprising an active metal is arranged at least in some sections between the metal layer and the ceramic element (10) for supporting the connection of the metal layer to the ceramic element (10).
High optical power light conversion device using a phosphor element with solder attachment
A light generator comprises a light conversion device and a light source arranged to apply a light beam to the light conversion element. The light conversion device includes an optoceramic or other solid phosphor element comprising one or more phosphors embedded in a ceramic, glass, or other host, a metal heat sink, and a solder bond attaching the optoceramic phosphor element to the metal heat sink. The optoceramic phosphor element does not undergo cracking in response to the light source applying a light beam of beam energy effective to heat the optoceramic phosphor element to the phosphor quenching point.
SINTERED BODY, SUBSTRATE, CIRCUIT BOARD, AND MANUFACTURING METHOD OF SINTERED BOY
A sintered body includes a crystal grain containing silicon nitride, and a grain boundary phase. If dielectric losses of the sintered body are measured while applying an alternating voltage to the sintered body and continuously changing a frequency of the alternating voltage from 50 Hz to 1 MHz, an average value ε.sub.A of dielectric losses of the sintered body in a frequency band from 800 kHz to 1 MHz and an average value ε.sub.B of dielectric losses of the sintered body in a frequency band from 100 Hz to 200 Hz satisfy an expression |ε.sub.A−ε.sub.B|≤0.1.
Semiconductor processing equipment with high temperature resistant nickel alloy joints and methods for making same
A method for the joining of ceramic pieces with a hermetically sealed joint comprising brazing a layer of joining material between the two pieces. The ceramic pieces may be aluminum nitride or other ceramics, and the pieces may be brazed with Nickel and an alloying element, under controlled atmosphere. The completed joint will be fully or substantially Nickel with another element in solution. The joint material is adapted to later withstand both the environments within a process chamber during substrate processing, and the oxygenated atmosphere which may be seen within the interior of a heater or electrostatic chuck. Semiconductor processing equipment comprising ceramic and joined with a nickel alloy and adapted to withstand processing chemistries, such as fluorine chemistries, as well as high temperatures.
Bonded Assembly, And Ceramic Circuit Substrate And Semiconductor Device Using The Same
A bonded assembly according to the present embodiment, includes a metal plate and a ceramic substrate bonded to each other through a bonding layer containing Ag. In the bonded assembly, in a measurement region that is formed in a cross section formed by a thickness direction of the bonding layer and an orthogonal direction thereto, and that has a size of a length in the thickness direction of the bonding layer×a length of 200 μm in the orthogonal direction, a Ag-rich region having a Ag concentration of 60 at % or more has an area ratio of 70% or less to a Ag-poor region having a Ag concentration of 50 at % or less.
NUCLEAR REACTOR FUEL ROD AND FUEL ASSEMBLY HAVING BUNDLED SAME
A nuclear reactor fuel rod is a fuel rod for a light-water reactor. The nuclear reactor fuel rod includes a fuel cladding tube and an end plug, both of which are formed of a silicon carbide material. A bonding portion between the fuel cladding tube and the end plug is formed by brazing with a predetermined metal bonding material interposed, and/or by diffusion bonding. The predetermined metal bonding material has a solidus temperature of 1200° C. or higher. An outer surface of the bonding portion, and a portion of an outer surface of the fuel cladding tube and the end plug, which is adjacent to the outer surface of the bonding portion are covered by bonding-portion coating formed of a predetermined coating metal. The predetermined metal bonding material and the predetermined coating metal have an average linear expansion coefficient which is less than 10 ppm/K.
Support Substrate and Method for Producing a Support Substrate
A support substrate (1), in particular a metal-ceramic substrate, as a support for electric components, comprising: —at least one metal layer (10) and—an insulating element (30), in particular a ceramic element, a glass element, a glass ceramic element, and/or a high temperature-resistant plastic element. The at least one metal layer (10) and the insulating element (30) extend along a main extension plane (HSE) and are arranged one over the other in a stacking direction (S) running perpendicularly to the main extension plane (HSE), wherein in a completed support substrate (1), a binding layer (12) is formed between the at least one metal layer (10) and the insulating element (30), and an adhesive layer (13) of the binding layer (12) has a surface resistance which is greater than 5 Ohm/sq.
Substrate for power modules, substrate with heat sink for power modules, and power module
The present invention provides a power module substrate including an insulating substrate, a circuit layer which is formed on one surface of the insulating substrate, and a metal layer which is formed on the other surface of the insulating substrate, in which the circuit layer has a first aluminum layer made of aluminum or an aluminum alloy which is bonded to the insulating substrate and a first copper layer made of copper or a copper alloy which is bonded to the first aluminum layer by solid-phase diffusion, the metal layer has a second aluminum layer made of aluminum or an aluminum alloy, and a relationship between a thickness t.sub.1 of the circuit layer and a thickness t.sub.2 of the second aluminum layer of the metal layer satisfy t.sub.1<t.sub.2.
Method for producing a connection between two ceramic parts - in particular, of parts of a pressure sensor
A method according to the invention for producing a connection between two surfaces or surface sections of two ceramic parts comprises: provision of a first ceramic part and of a second ceramic part; provision of an active brazing solder material on at least one surface section of at least one of the ceramic parts; and heating the active brazing solder in a vacuum brazing process. The whole active brazing solder material is provided for connecting the first and the second ceramic part by a sputtering method, wherein at least one surface section of at least one of the ceramic parts, preferably of the two ceramic parts, is layered with a layer sequence of individual components of the active brazing solder material, wherein the average strength of the layers of an individual component of the active brazing solder is no more than 0.5%, in particular not more than 0.2%, preferably not more than 0.1% and especially preferably not more than 0.05% of the strength of the joining region.